Tensile Strength Evolution and Damage Mechanisms of Al-Si Piston Alloy at Different Temperatures

被引:14
作者
Wang, Meng [1 ,2 ]
Pang, Jianchao [1 ]
Qiu, Yu [1 ]
Liu, Haiquan [1 ,2 ]
Li, Shouxin [1 ]
Zhang, Zhefeng [1 ,2 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, 72 Wenhua Rd, Shenyang 110016, Liaoning, Peoples R China
[2] Univ Sci & Technol China, Sch Mat Sci & Engn, Hefei 230026, Anhui, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Si piston alloy; Damage mechanism; High temperature; In situ tensile; Strength; CYCLE FATIGUE BEHAVIOR; ALUMINUM-ALLOY; MICROSTRUCTURE EVOLUTION; DEFORMATION-BEHAVIOR; STRESS STATES; PARTICLES; MG; FRACTURE; SILICON; ADDITIONS;
D O I
10.1002/adem.201700610
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The Al-Si piston alloys always bear different temperatures because of its peculiar component structure and service condition. Therefore, the tensile strength, elongation to fracture, and corresponding damage mechanisms of Al12SiCuNiMg piston alloys (ASPA) have been investigated with in situ technique at different temperatures. The tensile properties show two-stage tendencies: the former stage (25-280 degrees C) is determined by easily broken phases with inherent brittleness (such as primary Si), and the fracture behavior presents rapid brittle fracture after reaching the critical stress (about 430MPa, based on in situ technique and the elastic stress field model). The later one (280-425 degrees C) is dominated by particles debonding and phase coarsening. The plastic deformation behavior, dynamic recovery, and flow process become more significant on account of thermal activation. The Considere criterion h=K indicates that the transition of damage behaviors from insufficient local strength to insufficient matrix strength and the corresponding failure model shifts from brittle to ductile fracture. Based on the damage mechanisms, the elastic field model and thermal activation relation model have been established to characterize the strength of the ASPA at different temperature ranges.
引用
收藏
页数:9
相关论文
共 37 条
  • [31] Eutectic Al-Si-Cu-Fe-Mn alloys with enhanced mechanical properties at room and elevated temperature
    Wang, E. R.
    Hui, X. D.
    Chen, G. L.
    [J]. MATERIALS & DESIGN, 2011, 32 (8-9) : 4333 - 4340
  • [32] Wang Q. G., 2003, METALL MATER TRANS A, V34, P2002
  • [33] On the use of Considere's criterion in tensile testing of materials which accumulate internal damage
    Weber, L
    Kouzeli, M
    San Marchi, C
    Mortensen, A
    [J]. SCRIPTA MATERIALIA, 1999, 41 (05) : 549 - 551
  • [34] Weir J. R., 1964, TECH INF TECH REP, V26, P3357
  • [35] The cracking mechanism of silicon particles in an A357 aluminum alloy
    Yeh, JW
    Liu, WP
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (11): : 3558 - 3568
  • [36] Tensile Properties and Deformation Behaviors of a New Aluminum Alloy for High Pressure Die Casting
    Zhang, Peng
    Li, Zhenming
    Liu, Baoliang
    Ding, Wenjiang
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (04) : 367 - 378
  • [37] High-temperature low-cycle fatigue behaviour of a cast Al-12Si-CuNiMg alloy
    Zhang, Qing
    Zuo, Zhengxing
    Liu, Jinxiang
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2013, 36 (07) : 623 - 630