Microstructure and ablation property of C/C-ZrC-SiC composites fabricated by chemical liquid-vapor deposition combined with precursor infiltration and pyrolysis

被引:27
作者
He, Qinchuan [1 ]
Li, Hejun [1 ]
Wang, Changcong [1 ]
Zhou, Huashan [1 ]
Lu, Jinhua [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Carbon Carbon Composites Res Ctr, Xian 710072, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
C/C-ZrC-SiC composites; Joint processes; Microstructure; Ablation resistance; THERMAL RETARDANT ABILITY; MECHANICAL-PROPERTIES; OXYACETYLENE TORCH; CARBON/CARBON COMPOSITES; C/C-SIC-ZRB2; COMPOSITES; OXIDATION PROTECTION; BEHAVIOR; RESISTANCE; TEMPERATURE; NANOWIRES;
D O I
10.1016/j.ceramint.2018.11.045
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
C/C-ZrC-SiC composites were produced by the joint processes of chemical liquid-vapor deposition (CLVD) and precursor infiltration and pyrolysis (PIP), and the effects of deposition period in CLVD process on the preparation, microstructure and anti-ablation property were studied. The results displayed the non-woven layers of the composites was preferred to be densified in CLVD method, but the subsequent PIP process could fill the pores of the fiber webs. Thus the joint technologies reduced the porosity of the composites and improved the content of ceramics. Meanwhile, the insufficient deposition in CLVD process led to large amounts of defects, which were not densified fully in the following PIP. However, the excessive deposition of CLVD filled the pores remarkably, so the channels for precursor infiltration in the subsequent PIP were reduced. When the deposition period was 8 h, the sample C8P9 had a low porosity, high ceramics content and uniform distribution, which was responsible for its outstanding ablation resistance. After ablation for 60 s, sample C8P9 was damaged slightly, and its mass and linear ablation rate was 1.22 x 10(-3) g/s and 1.07 x 10(-3) mm/s. The ablation surface was divided into four regions, and the different oxide coatings were generated on these regions. These coatings could provide effective protection for the composites, which made a significant contribution to improve the ablation resistance.
引用
收藏
页码:3767 / 3781
页数:15
相关论文
共 46 条
[1]  
[Anonymous], 1996, GIB323A96 NAT STAND
[2]   Microstructure and ablation behaviors of a novel gradient C/C-ZrC-SiC composite fabricated by an improved reactive melt infiltration [J].
Chang, Yabin ;
Sun, Wei ;
Xiong, Xiang ;
Chen, Zhaoke ;
Wang, Yalei ;
Hao, Zhenhua ;
Xu, Yonglong .
CERAMICS INTERNATIONAL, 2016, 42 (15) :16906-16915
[3]   Oxidation protection of carbon/carbon composites by a novel SiC nanoribbon-reinforced SiC-Si ceramic coating [J].
Chu, Yanhui ;
Li, Hejun ;
Luo, Huijuan ;
Li, Lu ;
Qi, Lehua .
CORROSION SCIENCE, 2015, 92 :272-279
[4]   Oxidation protection and behavior of C/C composites with an in situ SiC nanowire-SiC-Si/SiC-Si coating [J].
Chu, Yanhui ;
Li, Hejun ;
Fu, Qiangang ;
Qi, Lehua ;
Li, Lu ;
Liu, Yangtong .
CORROSION SCIENCE, 2013, 70 :285-289
[5]   Oxidation-protective and mechanical properties of SiC nanowire-toughened Si-Mo-Cr composite coating for C/C composites [J].
Chu Yanhui ;
Li Hejun ;
Fu Qiangang ;
Shi Xiaohong ;
Qi Lehua ;
Wei Bingbo .
CORROSION SCIENCE, 2012, 58 :315-320
[6]   Oxidation protection of C/C composites with a multilayer coating of SiC and Si plus SiC plus SiC nanowires [J].
Chu Yanhui ;
Li Hejun ;
Fu Qiangang ;
Wang Haipeng ;
Hou Xianghui ;
Zou Xu ;
Shang Gunan .
CARBON, 2012, 50 (03) :1280-1288
[7]   Oxidation protection of SiC-coated C/C composites by SiC nanowire-toughened CrSi2-SiC-Si coating [J].
Chu Yanhui ;
Li Hejun ;
Fu Qiangang ;
Qi Lehua ;
Wei Bingbo .
CORROSION SCIENCE, 2012, 55 :394-400
[8]   Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C [J].
Chu, Yanhui ;
Fu, Qiangang ;
Li, Hejun ;
Li, Kezhi ;
Zou, Xu ;
Gu, Caige .
CORROSION SCIENCE, 2011, 53 (09) :3048-3053
[9]   Chemical vapor infiltration of C/C composites:: Fast densification processes and matrix characterizations [J].
Delhaès, P ;
Trinquecoste, M ;
Lines, JF ;
Cosculluela, A ;
Goyhénèche, JM ;
Couzi, M .
CARBON, 2005, 43 (04) :681-691
[10]   Nanowire-toughened transition layer to improve the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites [J].
Fu, Qian-Gang ;
Jing, Jun-Yi ;
Tan, Bi-Yi ;
Yuan, Rui-Mei ;
Zhuang, Lei ;
Li, Lu .
CORROSION SCIENCE, 2016, 111 :259-266