Effect of Y content on interface reaction and wettability between a nickel-base single crystal superalloy melt and ceramic mould

被引:29
作者
Zi, Yun [1 ,2 ]
Meng, Jie [1 ]
Zhang, Chaowei [1 ]
Yang, Yanhong [1 ]
Zhou, Yizhou [1 ]
Ding, Yutian [3 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
[2] Univ Sci & Technol China, Dept Mat Sci & Engn, Hefei 230026, Anhui, Peoples R China
[3] Lanzhou Univ Technol, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou 730050, Gansu, Peoples R China
基金
国家重点研发计划; 中国国家自然科学基金;
关键词
Nickel-base single crystal superalloy melt; Ceramic mould; Interface reaction; Wettability; Y content; THERMAL-CONDUCTIVITY; NI; MICROSTRUCTURE; EVOLUTION; REMOVAL; ALLOYS; HF;
D O I
10.1016/j.jallcom.2019.03.037
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, the effect of Y content on interface reaction and wettability between a nickel-base single crystal supperalloy melt and ceramic mould were studied by means of sessile drop tests. The microstructural characterization of the alloy-ceramic interface and the elemental compositions of reaction products were performed by scanning electron microscope (SEM) and electron probe micro-analyzer (EPMA), the phases of reaction products were identified by X-ray diffraction (XRD), and the surface analysis of reaction products was carried out by X-ray photoelectron spectroscopy (XPS). The results showed that Al and Hf in the alloy reacted with SiO2 in the ceramic mould when Y content was lower than 0.011 wt%, and the reaction products were Al2O3 and HfO2, with little change in the wetting angle. However, when Y content was higher than 0.017 wt%, Y and Al in the alloy reacted with SiO2 in the ceramic mould, and the wetting angle decreased significantly. 0.017 wt% was the critical concentration of Y content that would cause interface reactions. The reaction products of 0.017 and 0.025 wt% Y alloys were Y3Al2(AlO4)(3), the reaction products of 0.1 wt% Y alloy were Y3Al5O12 and Y4Al2O9, and the reaction products of 0.5 and 1.0 wt% Y alloys were double reaction layer composed of Y2O3 and Y3Al5O12. Si generated by the interface reactions could react with O-2 in the atmosphere to form SiOx during the cooling of the alloy-ceramic couples. (C) 2019 Published by Elsevier B.V.
引用
收藏
页码:472 / 484
页数:13
相关论文
共 45 条
[1]   WETTING UNDER CHEMICAL-EQUILIBRIUM AND NONEQUILIBRIUM CONDITIONS [J].
AKSAY, IA ;
HOGE, CE ;
PASK, JA .
JOURNAL OF PHYSICAL CHEMISTRY, 1974, 78 (12) :1178-1183
[2]  
[Anonymous], 1995, CRITERIA METHODS EVA
[3]  
[Anonymous], J MAT ENG
[4]  
[Anonymous], THESIS
[5]  
[Anonymous], THESIS
[6]   Effect of Trace O Element on High-temperature Wettability Between Ni3Al Melt and Y2O3 Ceramic [J].
Bai, Peng ;
Zhang, Hua-Rui ;
Wan, Bei-Bei ;
Ran, Chao ;
Zhang, Hu .
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2018, 31 (05) :552-560
[7]  
Barin I., 1989, Thermochemical Data of Pure Substances, V3rd
[8]  
Chen Jian, 2001, Journal of Shanghai Jiaotong University, V35, P364
[9]  
CHEN MING-HAI, 2002, CEMENTED CARBIDE, V19, P199
[10]   熔模铸造高温合金与陶瓷材料界面反应研究进展 [J].
陈晓燕 ;
肖旅 ;
余建波 ;
孙宝德 ;
李飞 .
特种铸造及有色合金, 2016, 36 (08) :844-848