Ultrasonic and Mechanical Measurements for the Detection of Crosslink Density of SBR and NBR Based on Various Curing Systems

被引:8
作者
Lawandy, S. N. [1 ]
Halim, S. F. [1 ]
Afifi, H. A. [2 ]
机构
[1] NIS, Lab Metrol & Technol Polymer, Giza, Egypt
[2] NIS, Lab Ultrason Metrol, Giza, Egypt
关键词
curing of polymers; crosslinking; compression; vulcanization; network; RUBBER; PARAMETERS; BLENDS;
D O I
10.1002/app.29285
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The stress-strain measurements of styrenebutadiene rubber (SBR) samples based on various Curing systems were used to access the crosslink density of various rubber mixes. Same materials were subjected to various uniaxial compression strains, The thicknesses before compression and after recovery were recorded. After recovery, pulse echo method was used to measure the ultrasonic velocity for the dilatational wave and that of shear wave at a frequency of 2 MHz and at room temperature. Both of the ultrasonic velocities were used to determine the elastic moduli of the samples. The relation between the elastic moduli and the corresponding recover values were used to determine the crosslink density of samples. The crosslink density values obtained from the two techniques were compared. Butadiene-acrylonitrile (NBR) rubber mix was used to show that the ultrasonic technique is applicable for other rubber Compounds. (c) 2008 Wiley Periodicals, Inc. J Appl Polym Sci 112: 366-371, 2009
引用
收藏
页码:366 / 371
页数:6
相关论文
共 23 条