Corrosion of Aluminized Steel in Aggressive Natural Water

被引:2
|
作者
Akhoondan, M. [1 ]
Saguees, A. A. [1 ]
机构
[1] Univ S Florida, Dept Civil & Environm Engn, Tampa, FL 33620 USA
来源
CORROSION (GENERAL) - 221ST ECS MEETING | 2013年 / 45卷 / 19期
关键词
D O I
10.1149/04519.0025ecst
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Aluminized steel Type 2 (AST2) has a similar to 50 mu m thick coating with outer and inner layers of mostly Al and Fe-Al intermetallic respectively. AST2 is used for culvert and drainage pipes that are required to have long service life. The use of calcium carbonate-rich backfill (limestone) found to be a key contributing factor to the observed early deterioration. Limestone contributed to form a high pH environment sufficient to cause passivity breakdown of the passive film on aluminum. AST2 specimens were exposed in limestone-water cells with water being continuously replenished at a slow rate. A high steady state pH developed that was aggressive to aluminum passive film. Electrochemical measurements and direct inspection indicated onset of severe early corrosion with consequent fast wastage of the outer film. Corrosion rate decreased later as a thick corrosion product layer covered the surface and formed a transport limitation barrier.
引用
收藏
页码:25 / 35
页数:11
相关论文
共 50 条
  • [21] CORROSION-RESISTANCE AND CORROSION BEHAVIOR OF ALUMINIZED STEEL SHEET UNDER SALT CORROSIVE ENVIRONMENT
    HIGUCHI, S
    ASAKAWA, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1991, 77 (02): : 258 - 265
  • [22] Galvanic corrosion of carbon and steel in aggressive environments
    Tavakkolizadeh, M
    Saadatmanesh, H
    JOURNAL OF COMPOSITES FOR CONSTRUCTION, 2001, 5 (03) : 200 - 210
  • [23] Inhibitive and bactericidal effects of natural naphthenates on steel corrosion in sea water
    Samedov, A. M.
    Alieva, L. I.
    Abbasov, V. M.
    PROTECTION OF METALS, 2008, 44 (04): : 397 - 401
  • [24] Inhibitive and bactericidal effects of natural naphthenates on steel corrosion in sea water
    A. M. Samedov
    L. I. Alieva
    V. M. Abbasov
    Protection of Metals, 2008, 44 : 397 - 401
  • [25] AN ANALYSIS OF THE SIGNIFICANCE OF COATING THICKNESS ON THE CORROSION BEHAVIOR OF HOT DIP ALUMINIZED STEEL
    AGARWAL, SB
    LEGAULT, RA
    MATERIALS PERFORMANCE, 1983, 22 (10) : 19 - 23
  • [26] Microstructural and Corrosion Properties of PEO Coated Zinc-Aluminized (ZA) Steel
    Pezzato, Luca
    Settimi, Alessio Giorgio
    Cerchier, Pietrogiovanni
    Gennari, Claudio
    Dabala, Manuele
    Brunelli, Katya
    COATINGS, 2020, 10 (05)
  • [27] CORROSION RESISTANCE OF STAINLESS STEEL TP347H WITH ALUMINIZED LAYER
    Luo Hong
    Yu Lan-ying
    Li Xin-yue
    Zeng Xian-guang
    METAL SCIENCE AND HEAT TREATMENT, 2010, 52 (1-2) : 32 - 35
  • [28] Corrosion resistance of stainless steel TP347H with aluminized layer
    Luo Hong
    Yu Lan-ying
    Li Xin-yue
    Zeng Xian-guang
    Metal Science and Heat Treatment, 2010, 52 : 32 - 35
  • [29] Nanocrystallization of aluminized surface of carbon steel for enhanced resistances to corrosion and corrosive wear
    Chen, C.
    Li, D. Y.
    Shang, C. J.
    ELECTROCHIMICA ACTA, 2009, 55 (01) : 118 - 124
  • [30] DEVELOPMENT OF HOT DIP ALUMINIZED STEEL SHEET WITH EXCELLENT CHARACTERISTICS .5. CORROSION BEHAVIOR OF ALUMINIZED STEEL SHEET IN DEICING SALT USAGE ENVIRONMENT
    OHMORI, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (05): : S437 - S437