Oxidation of 4H-SiC covered with a SmSix surface alloy

被引:8
|
作者
Kildemo, M [1 ]
Grossner, U
Juel, M
Svensson, BG
Raaen, S
机构
[1] Norwegian Univ Sci & Technol, Dept Phys, N-7491 Trondheim, Norway
[2] Univ Oslo, Dept Phys, N-0371 Oslo, Norway
[3] Univ Oslo, Ctr Mat Sci & Nanotechnol, N-0371 Oslo, Norway
关键词
soft X-ray photoelectron spectroscopy; catalysis; surface electronic phenomena; silicon; carbon; samarium; rare earth oxide; alloys; semiconductor-insulator interfaces;
D O I
10.1016/j.susc.2006.01.030
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Oxidation of Sm/4H-SiC is studied by X-ray photoemission spectroscopy (XPS) and low energy electron diffraction (LEED). In particular, we report kinetic information from the oxidation of a SmSix (1 x 1) surface alloy formed on (0001) 4H-SiC. During the initial oxidation of the SmSix alloy, a (2 x 2)-LEED pattern is observed. Furthermore, the Sm 2+ valency observed from the clean SmSix surface alloy, which is related to surface samarium, atoms, disappear at 15 L oxygen exposure. The oxygen atom is consequently deduced to be located at bridge or hollow sites involving one Sm atom. The initial oxidation result in an oxygen deficit SmSiOx interface oxide, probably as a consequence of the high oxidation temperatures in this work (900-1050 degrees C). We report that in a prolonged oxidation (longer than 10 U) a SiO2 layer forms on top of the samarium silicon oxide interface layer. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:1300 / 1307
页数:8
相关论文
共 50 条
  • [21] Two-dimensional Roughness Growth at Surface and Interface of SiO2 Films during Thermal Oxidation of 4H-SiC(0001)
    Hasunuma, R.
    Fukasawa, T.
    Kosugi, R.
    Ishida, Y.
    Yamabe, K.
    SILICON CARBIDE AND RELATED MATERIALS 2011, PTS 1 AND 2, 2012, 717-720 : 785 - +
  • [22] Study on nanohardness of helium-implanted 4H-SiC
    Zhang Yong
    Zhang Chong-Hong
    Zhou Li-Hong
    Li Bing-Sheng
    Yang Yi-Tao
    ACTA PHYSICA SINICA, 2010, 59 (06) : 4130 - 4135
  • [23] Carrier Generation Lifetimes in 4H-SiC MOS Capacitors
    Marinella, Matthew J.
    Schroder, Dieter K.
    Chung, Gilyong
    Loboda, Mark J.
    Isaacs-Smith, Tamara
    Williams, John R.
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 2010, 57 (08) : 1910 - 1923
  • [24] Exciton line temperature evolution in 4H-SiC crystals
    Zimbone, M.
    Litrico, G.
    Chibbaro, C.
    Reitano, R.
    PHYSICA SCRIPTA, 2010, 81 (04)
  • [25] Vapor phase surface preparation (etching) of 4H-SiC substrates using tetrafluorosilane (SiF4) in a hydrogen ambient for SiC epitaxy
    Rana, T.
    Chandrashekhar, M. V. S.
    Sudarshan, Tangali S.
    JOURNAL OF CRYSTAL GROWTH, 2013, 380 : 61 - 67
  • [26] Defect induced ferromagnetism in 4H-SiC single crystals
    Li, Lin
    Hua, Wei
    Prucnal, Slawomir
    Yao, Shu-De
    Shao, Lin
    Potzger, Kay
    Zhou, Shengqiang
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2012, 275 : 33 - 36
  • [27] Epitaxial graphene on 4H-SiC by pulsed electron irradiation
    Huang, Qingsong
    Chen, Xiaolong
    Liu, Jun
    Wang, Wenjun
    Wang, Gang
    Wang, Wanyan
    Yang, Rong
    Liu, Yu
    Guo, Liwei
    CHEMICAL COMMUNICATIONS, 2010, 46 (27) : 4917 - 4919
  • [28] Determination of Band Structure at GaAs/4H-SiC Heterojunctions
    Liang, J. B.
    Shimizu, S.
    Arai, M.
    Shigekawa, N.
    SEMICONDUCTOR WAFER BONDING: SCIENCE, TECHNOLOGY AND APPLICATIONS 14, 2016, 75 (09): : 221 - 227
  • [29] Characterization of the carrot defect in 4H-SiC epitaxial layers
    Hassan, J.
    Henry, A.
    McNally, P. J.
    Bergman, J. P.
    JOURNAL OF CRYSTAL GROWTH, 2010, 312 (11) : 1828 - 1837
  • [30] Excimer laser ablation of single crystal 4H-SiC and 6H-SiC wafers
    Gupta, Saurabh
    Pecholt, Ben
    Molian, Pal
    JOURNAL OF MATERIALS SCIENCE, 2011, 46 (01) : 196 - 206