Oxidation of 4H-SiC covered with a SmSix surface alloy

被引:8
|
作者
Kildemo, M [1 ]
Grossner, U
Juel, M
Svensson, BG
Raaen, S
机构
[1] Norwegian Univ Sci & Technol, Dept Phys, N-7491 Trondheim, Norway
[2] Univ Oslo, Dept Phys, N-0371 Oslo, Norway
[3] Univ Oslo, Ctr Mat Sci & Nanotechnol, N-0371 Oslo, Norway
关键词
soft X-ray photoelectron spectroscopy; catalysis; surface electronic phenomena; silicon; carbon; samarium; rare earth oxide; alloys; semiconductor-insulator interfaces;
D O I
10.1016/j.susc.2006.01.030
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Oxidation of Sm/4H-SiC is studied by X-ray photoemission spectroscopy (XPS) and low energy electron diffraction (LEED). In particular, we report kinetic information from the oxidation of a SmSix (1 x 1) surface alloy formed on (0001) 4H-SiC. During the initial oxidation of the SmSix alloy, a (2 x 2)-LEED pattern is observed. Furthermore, the Sm 2+ valency observed from the clean SmSix surface alloy, which is related to surface samarium, atoms, disappear at 15 L oxygen exposure. The oxygen atom is consequently deduced to be located at bridge or hollow sites involving one Sm atom. The initial oxidation result in an oxygen deficit SmSiOx interface oxide, probably as a consequence of the high oxidation temperatures in this work (900-1050 degrees C). We report that in a prolonged oxidation (longer than 10 U) a SiO2 layer forms on top of the samarium silicon oxide interface layer. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:1300 / 1307
页数:8
相关论文
共 50 条
  • [1] Improvements in graphene growth on 4H-SiC(0001) using plasma induced surface oxidation
    Minami, Ouki
    Ito, Ryota
    Hosoo, Kohei
    Ochi, Makoto
    Sano, Yasuhisa
    Kawai, Kentaro
    Yamamura, Kazuya
    Arima, Kenta
    JOURNAL OF APPLIED PHYSICS, 2019, 126 (06)
  • [2] Interfacial investigation of in situ oxidation of 4H-SiC
    Virojanadara, C
    Johansson, LI
    SURFACE SCIENCE, 2001, 472 (1-2) : L145 - L149
  • [3] Insight into the initial oxidation of 4H-SiC from first-principles thermodynamics
    Li, Wenbo
    Zhao, Jijun
    Zhu, Qiaozhi
    Wang, Dejun
    PHYSICAL REVIEW B, 2013, 87 (08)
  • [4] Surface defects in 4H-SiC: properties, characterizations and passivation schemes
    Mao, Weiwei
    Cui, Can
    Xiong, Huifan
    Zhang, Naifu
    Liu, Shuai
    Dou, Maofeng
    Song, Lihui
    Yang, Deren
    Pi, Xiaodong
    SEMICONDUCTOR SCIENCE AND TECHNOLOGY, 2023, 38 (07)
  • [5] Preparation and oxidation characteristics of Si layers grown on 4H-SiC substrates
    Li, Yunkai
    Zhao, Siqi
    Wei, Moyu
    Jiao, Jingyi
    Yan, Guoguo
    Liu, Xingfang
    VACUUM, 2024, 227
  • [6] Photoluminescence study of oxidation-induced faults in 4H-SiC epilayers
    Miyano, Yutaro
    Asafuji, Ryosuke
    Yagi, Shuhei
    Hijikata, Yasuto
    Yaguchi, Hiroyuki
    AIP ADVANCES, 2015, 5 (12):
  • [7] Oxidation temperature influence on the properties of oxide layers thermally grown on 4H-SiC by wet oxidation
    Dartora, G. H. S.
    Radtke, C.
    Stedile, F. C.
    PHYSICA SCRIPTA, 2025, 100 (01)
  • [8] 4H-SiC Surface Modified by a Green Femtosecond Laser at Low Fluence
    Liu, Yi-Hsien
    Cheng, Chung-Wei
    JOURNAL OF LASER MICRO NANOENGINEERING, 2023, 18 (03): : 157 - 160
  • [9] Effect of Direct Nitridation of 4H-SiC Surface on MOS Interface States
    Sakai, Takashi
    Hemmi, Mitsunori
    Murata, Yusuke
    Yamakami, Tomohiko
    Hayashibe, Rinpei
    Onuma, Yoshinaru
    Kamimura, Kiichi
    SILICON CARBIDE AND RELATED MATERIALS 2011, PTS 1 AND 2, 2012, 717-720 : 725 - 728
  • [10] Origin of hydrogen passivation in 4H-SiC
    Cai, Xuefen
    Yang, Yang
    Deng, Hui-Xiong
    Wei, Su-Huai
    PHYSICAL REVIEW MATERIALS, 2021, 5 (06)