Tribological performance and behaviour of CVD TiC/TiCN/TiN multilayer coating at elevated temperature

被引:10
作者
Wang, Shao-Long [1 ]
Jiang, Nan [1 ]
机构
[1] Chinese Acad Sci, Key Lab Marine New Mat & Related Technol, Zhejiang Key Lab Marine Mat & Protect Technol, Ningbo Inst Mat Technol & Engn, Ningbo 315201, Peoples R China
关键词
Coating; abrasive; adhesive; wear; high temperature; WEAR BEHAVIOR; TICN; TIN; IMPROVEMENT; COMPOSITES; DEPOSITION; RESISTANCE; STEEL; TIALN; TIO2;
D O I
10.1080/02670844.2020.1807813
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
TiC/TiCN/TiN multilayer coating was prepared on a high-speed tool steel W6Mo5Cr4V2 by chemical vapour deposition. The tribological performance and behaviour of the coating were investigated at an elevated temperature of 400-600 degrees C. Results show that the friction coefficient of the coating first decreases from 0.39 to 0.08 and then increases from 0.08 to 0.23 with the increase in temperature, while the average wear rate increases continuously from 0.97 x 10(-13)to 2.11 x 10(-13) m(3)N(-1)m(-1). The tribochemical product of Fe(2)O(3)in the tribo-oxidative layer (TiO2 + Fe2O3) could reduce the coating friction coefficient but enlarge the wear rate. As the Fe(2)O(3)component increases, the consumption of the tribo-oxidative layer accelerates gradually and the coating wear mechanism transforms from the mild oxidative-abrasive-adhesive wear to severe oxidative-adhesive wear.
引用
收藏
页码:1 / 11
页数:11
相关论文
共 30 条
  • [1] Tribological behavior at elevated temperature of multilayer TiCN/TiC/TiN hard coatings produced by chemical vapor deposition
    Bao, Mingdong
    Xu, Xuebo
    Zhang, Haijun
    Liu, Xiaoping
    Tian, Linhai
    Zeng, Zhaoxin
    Song, Yubin
    [J]. THIN SOLID FILMS, 2011, 520 (02) : 833 - 836
  • [2] Synthesis of Hard Carbon-TiN/TiC Composites by Reacting Cellulose with TiCl4 Followed by Carbothermal Nitridation/Reduction
    Cheng, Hang
    Garcia-Araez, Nuria
    Hector, Andrew L.
    Soule, Samantha
    [J]. INORGANIC CHEMISTRY, 2019, 58 (09) : 5776 - 5786
  • [3] The effect of calcination temperatures on wear properties of TiO2 coated CP-Ti
    Comakli, O.
    Yetim, T.
    Celik, A.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2014, 246 : 34 - 39
  • [4] Assessment of the Cr doping and size effects on the Raman-active modes of rutile TiO2 by UV/Visible polarized Raman spectroscopy
    Cristian Vasquez, G.
    Maestre, David
    Cremades, Ana
    Piqueras, Javier
    [J]. JOURNAL OF RAMAN SPECTROSCOPY, 2017, 48 (06) : 847 - 854
  • [5] deFaria DLA, 1997, J RAMAN SPECTROSC, V28, P873, DOI 10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO
  • [6] 2-B
  • [7] Wear Behavior and Mechanical Properties of TiO2 Coating Deposited Electrophoretically on 316 L Stainless Steel
    Dhiflaoui, Hafedh
    Kaouther, Khlifi
    Larbi, Ahmed Ben Cheikh
    [J]. JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2018, 140 (03):
  • [8] Deposition of CVD-TiCN and TiAlN coatings guided with thermodynamic calculations
    Du, Liye
    Wang, Shaoqing
    Du, Yong
    Qiu, Lianchang
    Chen, Zhuo
    Chen, Xiangming
    Liu, Zi-kui
    Zhang, Cong
    [J]. INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2018, 109 (04) : 277 - 283
  • [9] In situ synthesis of TiC-TiN-reinforced Fe-base plasma cladding coatings
    Feng, Zaiqiang
    Tang, Mingqi
    Liu, Yuqiang
    Yan, Zhenwei
    Li, Gang
    Zhang, Ruizhu
    [J]. SURFACE ENGINEERING, 2018, 34 (04) : 309 - 315
  • [10] Machining GX2CrNiMoN26-7-4 DSS Alloy: Wear Analysis of TiAlN and TiCN/Al2O3/TiN Coated Carbide Tools Behavior in Rough End Milling Operations
    Gomes Silva, Francisco Jose
    Martinho, Rui Pedro
    Martins, Carlos
    Lopes, Hernani
    Gouveia, Ronny Miguel
    [J]. COATINGS, 2019, 9 (06)