Study on the sequence length distribution of polypropylene by the successive self-nucleation and annealing (SSA) calorimetric technique

被引:33
作者
Chang, Hefei [1 ]
Zhang, Yu [2 ]
Ren, Shitong [1 ]
Dang, Xiaofei [2 ]
Zhang, Liaoyun [1 ]
Li, Huayi [2 ]
Hu, Youliang [2 ]
机构
[1] Chinese Acad Sci, Grad Univ, Beijing 100049, Peoples R China
[2] Chinese Acad Sci, Inst Chem, CAS Key Lab Engn Plast, Beijing Natl Lab Mol Sci, Beijing 100190, Peoples R China
基金
美国国家科学基金会;
关键词
ZIEGLER-NATTA CATALYSTS; DIFFERENTIAL SCANNING CALORIMETRY; MADE ISOTACTIC POLYPROPYLENE; RISING ELUTION FRACTIONATION; PROPYLENE-BUTENE COPOLYMERS; ACTIVE-SITES; CRYSTALLIZATION BEHAVIOR; THERMAL FRACTIONATION; METALLOCENE CATALYSTS; PROPENE POLYMERIZATION;
D O I
10.1039/c2py20452e
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The effect of successive self-nucleation and annealing (SSA) parameters including the annealing time t(s), annealing temperature interval and heating and cooling rates on the crystallization properties of polypropylene were researched in detail. Based on those results, the crystallization behavior and the sequence length distribution of polypropylene with different isotacticity and propylene/1-butene copolymer with different 1-butene comonomer content prepared by Ziegler-Natta catalyst were studied through SSA. With the increase of the isotacticity of polypropylene, the sequence length of the polypropylene gradually increases. The polypropylene prepared by propylene bulk polymerization has stronger crystallization ability and longer sequence length than that prepared by propylene sully polymerization. For the propylene/1-butene copolymer, the crystallization ability gradually reduces and the sequence length of each chain segment gradually decreases with the increase of 1-butene content in copolymer. In addition, the polypropylene samples with similar isotactic index prepared by Ziegler-Natta catalyst and metallocene catalyst under similar polymerization condition were also characterized through the SSA technique. The results show that the sequence length of polypropylene prepared by Ziegler-Natta catalyst is far longer than that prepared by metallocene catalyst. The interesting phenomenon that polypropylene prepared by metallocene catalyst has multiple melting peaks after SSA treatment, which is similar to the polypropylene prepared by Ziegler-Natta catalyst, was first reported.
引用
收藏
页码:2909 / 2919
页数:11
相关论文
共 63 条
[1]   Structural and kinetic factors governing the formation of the γ polymorph of isotactic polypropylene [J].
Alamo, RG ;
Kim, MH ;
Galante, MJ ;
Isasi, JR ;
Mandelkern, L .
MACROMOLECULES, 1999, 32 (12) :4050-4064
[2]  
[Anonymous], 1989, POLYM HDB
[3]  
Arnal M. L., 1998, ANN TECH C ANTEC C P, V2, P2007
[4]   Applications of successive self-nucleation and annealing (SSA) to polymer characterization [J].
Arnal, ML ;
Balsamo, V ;
Ronca, G ;
Sánchez, A ;
Müller, AJ ;
Cañizales, E ;
de Navarro, CU .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2000, 59 (1-2) :451-470
[5]  
ARNAL ML, 1999, ANTEC 99, V2, P2329
[6]   Crystallization of metallocene-made isotactic polypropylene:: Disordered modifications intermediate between the α and γ forms [J].
Auriemma, F ;
De Rosa, C .
MACROMOLECULES, 2002, 35 (24) :9057-9068
[7]  
Barino L, 1998, MACROMOL THEOR SIMUL, V7, P407, DOI 10.1002/mats.1998.040070404
[8]  
Bond EB, 1999, J POLYM SCI POL PHYS, V37, P3050, DOI 10.1002/(SICI)1099-0488(19991101)37:21<3050::AID-POLB14>3.0.CO
[9]  
2-L
[10]  
BUSICO V, 1986, MAKROMOL CHEM, V187, P1115