Adhesive wood joints under quasi-static and cyclic fatigue fracture Mode II loads

被引:25
作者
Clerc, Gaspard [1 ]
Brunner, Andreas J. [2 ]
Josset, Sebastien [3 ]
Niemz, Peter [1 ]
Pichelin, Frederic [1 ]
Van de Kuilen, Jan Willem G. [4 ]
机构
[1] Bern Univ Appl Sci Architecture Wood & Civil Engn, Solothurnstr 102, CH-2500 Biel, Switzerland
[2] Empa, Mech Syst Engn, Swiss Fed Labs Mat Sci & Technol, Uberlandstr 129, CH-8600 Dubendorf, Switzerland
[3] Henkel & Cie AG, Ind Str 17a, CH-6203 Sempach, Switzerland
[4] Tech Univ Munich, Wood Res Munich HFM, Winzerstr 45, DE-80797 Munich, Germany
关键词
Wood; Adhesive joints; Fatigue crack growth; 4-ENF; Mode II; GROWTH; RATIO;
D O I
10.1016/j.ijfatigue.2019.02.008
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper investigates the energy release rate (ERR) in Mode II in-plane shear during delamination propagation under quasi-static and cyclic fatigue fracture loading with the 4-point end notched flexure (4-ENF) fracture test specimen. Wood joints bonded with three different adhesives, one rather brittle phenol resorcinol formaldehyde (PRF) and two different one component polyurethane (1C-PUR) adhesives with relatively low modulus of elasticity were tested in order to investigate the influence of the adhesive properties on the damage propagation under quasi-static and cyclic fatigue loading. A simple reduction method based on the specimens' compliance was used to calculate the crack growth and the energy release rate during the test. Additionally, an automated analysis method was developed estimating the energy of crack initiation from quasi-static test results. This shall avoid introducing additional scatter due to operator-dependent, manual analysis. It was shown that the three tested adhesives are displaying similar ERR values under quasi-static loading. Under cyclic fatigue fracture loading, the more brittle PRF samples are showing a slower crack growth rate for similar energy release rate in comparison with the 1C-PUR adhesives. The proposed testing method, applied to adhesively bonded wood joints, has been shown to give satisfactory results. This can be used for the development of new adhesives with increased performance regarding fatigue delamination growth. The automated data analysis has potential for application on other materials under cyclic Mode II fatigue fracture loads.
引用
收藏
页码:40 / 52
页数:13
相关论文
共 27 条
[21]   Mode I delamination propagation and R-ratio effects in woven composite DCB specimens for a multi-directional layup [J].
Simon, Ido ;
Banks-Sills, Leslie ;
Fourman, Victor .
INTERNATIONAL JOURNAL OF FATIGUE, 2017, 96 :237-251
[22]   Mode I delamination fatigue crack growth in unidirectional fiber reinforced composites: Development of a standardized test procedure [J].
Stelzer, S. ;
Brunner, A. J. ;
Argueelles, A. ;
Murphy, N. ;
Pinter, G. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2012, 72 (10) :1102-1107
[23]   Experimental and numerical investigations on adhesively bonded hardwood joints [J].
Tannert, T. ;
Vallee, T. ;
Hehl, S. .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2012, 37 :65-69
[24]   Adhesively bonded connections in the context of timber engineering - A Review [J].
Vallee, Till ;
Tannert, Thomas ;
Fecht, Simon .
JOURNAL OF ADHESION, 2017, 93 (04) :257-287
[25]  
Watson P, 2013, WOOD RES-SLOVAKIA, V58, P43
[26]   Measurement of mode II fracture toughness of wood by the end-notched flexure test [J].
Yoshihara, H ;
Ohta, M .
JOURNAL OF WOOD SCIENCE, 2000, 46 (04) :273-278
[27]   Mode II R-curve of wood measured by 4-ENF test [J].
Yoshihara, H .
ENGINEERING FRACTURE MECHANICS, 2004, 71 (13-14) :2065-2077