Effect of long-term aging on the fracture toughness of primary coolant piping material Z3CN20.09M

被引:11
作者
Yu, Weiwei [1 ,2 ]
Fan, Minyu [2 ]
Gao, Hongbo [2 ]
Yu, Dunji [1 ]
Xue, Fei [2 ]
Chen, Xu [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Suzhou Nucl Power Res Inst, Suzhou 215004, Peoples R China
基金
中国国家自然科学基金;
关键词
Long-term aging; Primary coolant piping; Spinodal decomposition; Fracture toughness; SZW; Critical crack size; STRETCH-ZONE; DUCTILE FRACTURE; STAINLESS-STEELS; BEHAVIOR; RESISTANCE; WELDS;
D O I
10.1016/j.nucengdes.2017.12.022
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In this study, a series of accelerated thermal aging tests were performed on primary coolant piping materials (Z3CN20.09M) at 400 degrees C for 0, 2000, 5000 and 18,000 h to investigate the resulting microstructure change and fracture toughness. To further assess their fracture toughness, 0.2 mm offset line method and stretch zone width method were both employed to determine the fracture toughness. The results indicated that after long-term thermal aging, round shaped particles and characteristic morphology of spinodal decomposition were found in ferrite, thus resulting in the thermal aging embrittlement of Z3CN20.09M. Subsequently, the J-R curves and J-T curves all decreased significantly with the increasing thermal aging time. Furthermore, the fracture toughness parameters J(50), J(SZW(2D)), J(SZW(3D)) and dJ/d Delta a were first decreased rapidly and then slow saturated. In addition, the J(SZW(2D)) and J(SZW(3D)) values were significantly lower than J(Q) while the reduction of the critical crack size based on J(SZW(2D)) and J(SZW(3D)) parameters was about 30% compared with J(Q), and thus J(SZW) was relatively close to the onset of crack initiation.
引用
收藏
页码:150 / 160
页数:11
相关论文
共 33 条
[1]  
[Anonymous], 2015, 182015A ASTM
[2]  
[Anonymous], 2002, UNIFIED METHOD TEST
[3]  
[Anonymous], 1994, 6142 NUREGCR
[4]   Stretched zone width and blunting line equation for determination of initiation fracture toughness in low carbon highly ductile steels [J].
Bansal, Sandeep ;
Nath, S. K. ;
Ghosh, P. K. ;
Ray, S. .
INTERNATIONAL JOURNAL OF FRACTURE, 2009, 159 (01) :43-50
[5]   Thermal Aging Phenomena in Cast Duplex Stainless Steels [J].
Byun, T. S. ;
Yang, Y. ;
Overman, N. R. ;
Busby, J. T. .
JOM, 2016, 68 (02) :507-516
[6]   Low temperature thermal aging of austenitic stainless steel welds: Kinetics and effects on mechanical properties [J].
Chandra, K. ;
Kain, Vivekanand ;
Bhutani, Vikas ;
Raja, V. S. ;
Tewari, R. ;
Dey, G. K. ;
Chakravartty, J. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 534 :163-175
[7]   Fracture mechanics assessment of thermal aged nuclear piping based on the Leak-Before-Break concept [J].
Chen, Mingya ;
Yu, Weiwei ;
Qian, Guian ;
Wang, Rongshan ;
Lu, Feng ;
Zhang, Guodong ;
Xue, Fei ;
Chen, Zhilin .
NUCLEAR ENGINEERING AND DESIGN, 2016, 301 :333-340
[8]   Effect of thermal aging on the low cycle fatigue behavior of Z3CN20.09M cast duplex stainless steel [J].
Chen, Weifeng ;
Xue, Fei ;
Tian, Yang ;
Yu, Dunji ;
Yu, Weiwei ;
Chen, Xu .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 646 :263-271
[9]   INFLUENCE OF MICROSTRUCTURE ON THE FRACTURE-TOUGHNESS AND FRACTURE TOPOGRAPHY OF A DUPLEX STAINLESS-STEEL [J].
ERAUZKIN, E ;
IRISARRI, AM .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1992, 15 (02) :129-137
[10]   Residual stresses in austenitic stainless steel primary coolant pipes and welds of pressurized water reactors [J].
Faure, F ;
Leggatt, RH .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 1996, 65 (03) :265-275