Freeze-Thaw Durability of Air-Entrained Concrete

被引:65
作者
Shang, Huai-Shuai [1 ,2 ]
Yi, Ting-Hua [3 ]
机构
[1] Qingdao Technol Univ, Sch Civil Engn, Qingdao 266033, Peoples R China
[2] Dalian Univ Technol, State Key Lab Struct Anal Ind Equipment, Dalian 116024, Peoples R China
[3] Dalian Univ Technol, Sch Civil Engn, Dalian 116024, Peoples R China
基金
中国国家自然科学基金;
关键词
FROST-RESISTANCE; DAMAGE;
D O I
10.1155/2013/650791
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
One of the most damaging actions affecting concrete is the abrupt temperature change (freeze-thaw cycles). The types of deterioration of concrete structures by cyclic freeze-thaw can be largely classified into surface scaling (characterized by the weight loss) and internal crack growth (characterized by the loss of dynamic modulus of elasticity). The present study explored the durability of concrete made with air-entraining agent subjected to 0, 100, 200, 300, and 400 cycles of freeze-thaw. The experimental study of C20, C25, C30, C40, and C50 air-entrained concrete specimens was completed according to "the test method of long-term and durability on ordinary concrete" GB/T 50082-2009. The dynamic modulus of elasticity and weight loss of specimens were measured after different cycles of freeze-thaw. The influence of freeze-thaw cycles on the relative dynamic modulus of elasticity and weight loss was analyzed. The findings showed that the dynamic modulus of elasticity and weight decreased as the freeze-thaw cycles were repeated. They revealed that the C30, C40, and C50 air-entrained concrete was still durable after 300 cycles of freeze-thaw according to the experimental results.
引用
收藏
页数:6
相关论文
共 17 条
[1]  
[Anonymous], 2003, THESIS DALIAN U TECH
[2]  
Atkins C., 2010, CONCRETE DURABILITY
[3]  
Cheng H.Q., 2003, HENAN SCI, V21, P214
[4]  
COHEN MD, 1992, ACI MATER J, V89, P406
[5]   Concrete durability [J].
Mather, B .
CEMENT & CONCRETE COMPOSITES, 2004, 26 (01) :3-4
[6]   Freeze-thaw durability of recycled concrete containing ceramic aggregate [J].
Medina, Cesar ;
Sanchez de Rojas, Maria Isabel ;
Frias, Moises .
JOURNAL OF CLEANER PRODUCTION, 2013, 40 :151-160
[7]   Evaluation of freeze-thaw damage in concrete by ultrasonic imaging [J].
Molero, M. ;
Aparicio, S. ;
Al-Assadi, G. ;
Casati, M. J. ;
Hernandez, M. G. ;
Anaya, J. J. .
NDT & E INTERNATIONAL, 2012, 52 :86-94
[8]  
National Standard of the People's Republic of China, 1999, GB17599 NAT STAND PE
[9]  
National Standard of the People's Republic of China, 2009, GBT500822009 NAT STA
[10]  
National Standard of the People's Republic of China, 1999, 27098 JTJ NAT STAND