Comparing the corrosion behavior of nanograined and coarse-grained interstitial free steels

被引:7
作者
Dehghani, Kamran [1 ]
Hosseini, Maryam [1 ]
Nekahi, Atiye [1 ]
机构
[1] Amirkabir Uni Tech, Dept Min Metall Eng, Tehran, Iran
关键词
Corrosion; Interstitial free steel; Wire brushing; Nanostructure; Severe plastic deformation; AUSTENITIC STAINLESS-STEEL; SEVERE PLASTIC-DEFORMATION; FE-CR ALLOYS; ELECTROCHEMICAL-BEHAVIOR; NANOCRYSTALLINE SURFACE; STRUCTURAL RELAXATION; SULFURIC-ACID; CHLORIDE-IONS; RESISTANCE; 304-STAINLESS-STEEL;
D O I
10.3139/146.110956
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The corrosion behavior of nanograined (NG) IF-steel was compared with its coarse-grained (CG) counterpart. The corrosion tests were carried out using different solutions of NaCl and H2SO4. The results show that the nanostructured IF steel exhibited higher corrosion resistance (E-corr) and lower corrosion rate (i(corr)). According to the corroded microstructures, extensive cracking was observed in the case of CG subjected to both chloride and acidic media, as well as localized corrosion with signs of severe pitting. The results also show that NaCl can act as an inhibitor when added to H2SO4-containg solution leading to a decrease in the detrimental effect of H2SO4.
引用
收藏
页码:999 / 1006
页数:8
相关论文
共 33 条
[1]  
Albrimi YA, 2011, INT J ELECTROCHEM SC, V6, P4614
[2]  
[Anonymous], MET HDB A
[3]  
Bahafi A., 2009, WORLD APPL SCI J, V7, P22
[4]   Corrosion resistance of ultra fine-grained Ti [J].
Balyanov, A ;
Kutnyakova, J ;
Amirkhanova, NA ;
Stolyarov, VV ;
Valiev, RZ ;
Liao, XZ ;
Zhao, YH ;
Jiang, YB ;
Xu, HF ;
Lowe, TC ;
Zhu, YT .
SCRIPTA MATERIALIA, 2004, 51 (03) :225-229
[5]   Formation of nanograin in IF steels by friction stir processing [J].
Chabok, A. ;
Dehghani, K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 528 (01) :309-313
[6]  
Davies G., 2003, Mater. Automob. Bodies, P189
[7]   Corrosion resistance of nanostructured titanium [J].
Garbacz, H. ;
Pisarek, M. ;
Kurzydlowski, K. J. .
BIOMOLECULAR ENGINEERING, 2007, 24 (05) :559-563
[8]   Beneficial role of chloride ions during pickling of steel in sulfuric acid [J].
Gaur, B ;
Singh, TB ;
Singh, DDN .
CORROSION, 1996, 52 (02) :154-159
[9]   Microstructure and corrosion properties of ultrafine-grained interstitial free steel [J].
Hadzima, Branislav ;
Janecek, Milos ;
Estrin, Yuri ;
Kim, Hyoung Seop .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 462 (1-2) :243-247
[10]   Electrochemical corrosion behaviour of a novel submicron-grained austenitic stainless steel in an acidic NaCl solution [J].
Hamada, A. S. ;
Karjalainen, L. P. ;
Somani, M. C. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 431 (1-2) :211-217