Characterization on the coatings of Ni-base alloy with nano- and micron-size Sm2O3 addition prepared by laser deposition

被引:14
作者
Zhang, Shi Hong [1 ,2 ]
Li, Ming Xi [2 ]
Yoon, Jae Hong [1 ]
Cho, Tong Yul [1 ]
机构
[1] Changwon Natl Univ, Sch Nano & Adv Mat Engn, Chang Won 641773, Gyeongnam, South Korea
[2] Anhui Univ Technol, Sch Mat Sci & Engn, Maanshan City 243002, Anhui, Peoples R China
关键词
Composite materials; Coatings; Microstructure; Wear; Corrosion;
D O I
10.1016/j.matchemphys.2008.06.024
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The coating materials are the powder mixture Of micron-size Ni-base alloy powders with both 1.5 wt.% micron-size and nano-size Sm2O3 powders, which are prepared on Q235 steel plate by 2.0 kW CO2 laser deposition. The results indicate that with rare earth oxide Sm2O3 addition, the width of planar crystallization is smaller than that of the Ni-base alloy coatings. Micron- and nano-Sm2O3/Ni-base alloy coatings have similar microstructure showing the primary phase of gamma-Ni dendrite and eutectic containing gamma-Ni and Cr23C6 phases. However, compared to micron-Sm2O3/Ni-base alloy. preferred orientation of gamma-Ni dendrite of nano-Sm2O3/Ni-base alloy is weakened. Planar crystal of several-mu m thickness is first grown and then dendrite growth is observed at 1.5% micron-Sm2O3/Ni-base alloy coating whereas equiaxed dendrite is grown at 1.5% nano-Sm2O3/Ni-base alloy coating. Hardness and wear resistance of the coating improves with decreasing Sm2O3 size from micron to nano. The improvement on tribological property of nano-Sm2O3/Ni-base alloy over micron-Sm2O3/Ni-base alloy coatings can be attributed to the better resistance of equiaxed dendrite to adhesion interactions during the wear process. In 6 M HNO3 solution, the corrosion resistance is greatly improved with nano-Sm2O3 addition since the decrease of corrosion ratio along grain-boundary in nano-Sm2O3/Ni-base alloy coating contributes to harmonization of corrosion potential. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:668 / 674
页数:7
相关论文
共 21 条
[1]  
[Anonymous], MAT RES B
[2]   Microstructural characterization and microscopy analysis of laser cladding Stellite 12 and tungsten carbide [J].
Chiang, K. A. ;
Chen, Y. C. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 182 (1-3) :297-302
[3]   Synthesis of hard nano-structured metal matrix composite boride coatings using combined laser and sol-gel technology [J].
Choudhury, A. Roy ;
Ezz, Tamer ;
Li, n Li .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 445 :193-202
[4]   Advanced nano-particles anti-corrosion ceria based sol gel coatings for aluminum alloys [J].
Hamdy, Abdel Salam .
MATERIALS LETTERS, 2006, 60 (21-22) :2633-2637
[5]  
LI G, 2000, RARE EARTHS SOC, V18, P341
[6]   Microstructure of Al2O3 nanocrystalline/cobalt-based alloy composite coatings by laser deposition [J].
Li, Mingxi ;
He, Yizhu ;
Yuan, Xiaomin ;
Zhang, Shillong .
MATERIALS & DESIGN, 2006, 27 (10) :1114-1119
[7]   Effect of nano-Y2O3 on microstructure of laser cladding cobalt-based alloy coatings [J].
Li, MX ;
He, YZ ;
Yuan, XM .
APPLIED SURFACE SCIENCE, 2006, 252 (08) :2882-2887
[8]   Microstructure and dry sliding wear behavior of laser clad Ni-based alloy coating with the addition of SiC [J].
Li, Q ;
Song, GM ;
Zhang, YZ ;
Lei, TC ;
Chen, WZ .
WEAR, 2003, 254 (3-4) :222-229
[9]   Effects of La2O3 on microstructure and wear properties of laser clad γ/Cr7C3/TiC composite coatings on TiAl intermatallic alloy [J].
Liu, Xiu-Bo ;
Yu, Rong-Li .
MATERIALS CHEMISTRY AND PHYSICS, 2007, 101 (2-3) :448-454
[10]  
Pang H, 2000, J RARE EARTH, V18, P293