Effect of scratching frequency on the tribocorrosion resistance of Al-Mn amorphous thin films

被引:19
作者
Chen, Jia [1 ,2 ]
Cai, Wenjun [2 ]
机构
[1] Univ S Florida, Dept Mech Engn, Tampa, FL 33620 USA
[2] Virginia Polytech Inst & State Univ, Dept Mat Sci & Engn, Blacksburg, VA 24060 USA
基金
美国国家科学基金会;
关键词
Amorphous thin film; Wear; Corrosion; Tribocorrosion; Coefficient of friction; Oxide film; HIGH DUCTILITY COMBINATION; ELECTROCHEMICAL CHARACTERISTICS; INTERMETALLIC PHASES; HIGH-STRENGTH; CORROSION; STEEL; ALLOYS; WEAR; ALUMINUM; DEGRADATION;
D O I
10.1016/j.wear.2018.12.055
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Amorphous metallic thin films show great promise for applications where mechanical and chemical attack co-exist due to their excellent wear, corrosion, and tribocorrosion resistance. In this research, the effect of scratching frequency on amorphous Al-Mn thin film were studied in simulated seawater by varying the scratching frequency from 0.05 to 1 Hz in reciprocal motion. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were applied to characterize the microstructure before and after tribocorrosion testing. Post-tribocorrosion topography measurement was performed using non-contact optical 3D profilometer. It was found that the total tribocorrosion rate, including both mechanical and chemical wear, increased with increasing scratching frequency. Mechanical wear increased with scratching frequency, mostly related to an increment of coefficient of friction and real contact area. On the other hand, chemical wear tend to increase with scratching frequency, most likely due to faster repassivation kinetics at lower frequency. Cross-sectional TEM analysis shows that the disordered surface layer primarily consists of aluminum oxide where manganese is completely absent.
引用
收藏
页码:1457 / 1465
页数:9
相关论文
共 42 条
[1]   Processing of ultrafine-grained titanium with high strength and good ductility by a combination of multiple forging and rolling [J].
Bezi, Z. ;
Krallics, G. ;
El-Tahawy, M. ;
Pekker, P. ;
Gubicza, J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 688 :210-217
[2]   Electrochemical characteristics of intermetallic phases in aluminum alloys - An experimental survey and discussion [J].
Birbilis, N ;
Buchheit, RG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (04) :B140-B151
[3]   Tuning nanoscale grain size distribution in multilayered Al-Mn alloys [J].
Cai, Wenjun ;
Schuh, Christopher A. .
SCRIPTA MATERIALIA, 2012, 66 (3-4) :194-197
[4]   Heavy carbon alloyed FCC-structured high entropy alloy with excellent combination of strength and ductility [J].
Chen, L. B. ;
Wei, R. ;
Tang, K. ;
Zhang, J. ;
Jiang, F. ;
He, L. ;
Sun, J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 716 :150-156
[5]   MOLECULAR-ORIGINS OF FRICTION - THE FORCE ON ADSORBED LAYERS [J].
CIEPLAK, M ;
SMITH, ED ;
ROBBINS, MO .
SCIENCE, 1994, 265 (5176) :1209-1212
[6]   A crystal chemical approach to the formulation of self-lubricating nanocomposite coatings [J].
Erdemir, A .
SURFACE & COATINGS TECHNOLOGY, 2005, 200 (5-6) :1792-1796
[7]   CO2 erosion-corrosion of pipeline steel (API X65) in oil and gas conditions-A systematic approach [J].
Hu, Xinming ;
Neville, Anne .
WEAR, 2009, 267 (11) :2027-2032
[8]   Electrochemical and materials aspects of tribocorrosion systems [J].
Landolt, D. .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2006, 39 (15) :3121-3127
[9]   Electrochemical methods in tribocorrosion: a critical appraisal [J].
Landolt, D ;
Mischler, S ;
Stemp, M .
ELECTROCHIMICA ACTA, 2001, 46 (24-25) :3913-3929
[10]   Depassivation-repassivation Behavior of a CoCrMo Alloy under Tribological Contact in Simulated Body Fluids [J].
Li, Xinyi ;
Yan, Yu ;
Zhang, Haijun ;
Su, Yanjing ;
Qiao, Lijie .
INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (03) :2495-2505