High cycling stability of zinc-anode/conducting polymer rechargeable battery with non-aqueous electrolyte

被引:98
作者
Guerfi, A. [1 ]
Trottier, J. [1 ]
Boyano, I. [2 ]
De Meatza, I. [2 ]
Blazquez, J. A. [2 ]
Brewer, S. [3 ]
Ryder, K. S. [4 ]
Vijh, A. [1 ]
Zaghib, K. [1 ]
机构
[1] Inst Rech Hydro Quebec, Varennes, PQ J3X 1S1, Canada
[2] IK4 CIDETEC, Donostia San Sebastian 20009, Gipuzkoa, Spain
[3] C Tech Innovat Ltd, Chester CH1 6EH, Cheshire, England
[4] Univ Leicester, Dept Chem, Leicester LE1 7RH, Leics, England
关键词
Energy storage; Zinc-polymer rechargeable battery; Zinc deposition/dissolution; Conducting polymer; LITHIUM BATTERIES; ELECTROCHEMICAL DEPOSITION; POLYANILINE; PERFORMANCE; CATHODE; HF;
D O I
10.1016/j.jpowsour.2013.09.082
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A non-aqueous zinc polyaniline secondary battery was fabricated with polyaniline Emeraldine base as cathode and zinc metal as anode in an electrolyte consisting of 0.3 M zinc-bis(trifluoromethyl-sulfonyl) imide Zn(TFSI)(2) dissolved in propylene carbonate. We observed that the formation of the battery required a prerequisite condition to stabilize the interfaces in order to maintain a stable capacity. The battery suffered from Zn dissolution which induces a competition between concurrent Zn dissolution and plating when the battery is in charge mode, and thus inefficient cycles are obtained. The capacity and coulombic efficiency of the battery depends on the charge discharge rates. We propose cycling protocols at different rates to determine the steady-state rates of competing reactions. When the cell is cycled at >= 1 C rate, the coulombic efficiency improves. The maximum capacity and energy densities of the battery are 148 mAhg(-1) and 127 mWhg(-1), respectively for discharge at C/2. The battery was successively charged/ discharged at constant current densities (1C rate), and high cycling stability was obtained for more than 1700 cycles at 99.8% efficiency. Zinc dissolution and self discharge of the battery were investigated after 24 h of standby. The investigation showed that the battery experiences a severe self-discharge of 48% per day. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:1099 / 1104
页数:6
相关论文
共 25 条
[1]   Will advanced lithium-alloy anodes have a chance in lithium-ion batteries? [J].
Besenhard, JO ;
Yang, J ;
Winter, M .
JOURNAL OF POWER SOURCES, 1997, 68 (01) :87-90
[2]   Addition of a thin-film inorganic solid electrolyte (Lipon) as a protective film in lithium batteries with a liquid electrolyte [J].
Dudney, NJ .
JOURNAL OF POWER SOURCES, 2000, 89 (02) :176-179
[3]   CYCLIC VOLTAMMETRIC INVESTIGATION OF THE FORMATION OF INTERMETALLIC PHASES AT A LIAL ELECTRODE IN METHYL ACETATE [J].
FUNG, YS ;
LAI, HC .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 1992, 22 (03) :255-261
[4]  
GAUTHIER M, 1989, POLYM ELECTROLYTE RE, V2, P285
[5]   New advances on bipolar rechargeable alkaline manganese dioxide-zinc batteries [J].
Ghaemi, M ;
Amrollahi, R ;
Ataherian, F ;
Kassaee, MZ .
JOURNAL OF POWER SOURCES, 2003, 117 (1-2) :233-241
[6]   Preparation of polyaniline nanofibers and their use as a cathode of aqueous rechargeable batteries [J].
Ghanbari, Kh. ;
Mousavi, M. F. ;
Shamsipur, M. .
ELECTROCHIMICA ACTA, 2006, 52 (04) :1514-1522
[7]  
Hooper A., 1988, ELECTROCHEMICAL SCI, V2
[8]   Comparative studies of chloride and chloride/citrate based electrolytes for zinc-polyaniline batteries [J].
Jugovic, B. Z. ;
Trisovic, T. Lj. ;
Stevanovic, J. S. ;
Maksimovic, M. D. ;
Grgur, B. N. .
ELECTROCHIMICA ACTA, 2006, 51 (28) :6268-6274
[9]   Electrochemical deposition of very smooth lithium using nonaqueous electrolytes containing HF [J].
Kanamura, K ;
Shiraishi, S ;
Takehara, Z .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (07) :2187-2197
[10]   ELECTROCHEMICAL DEPOSITION OF UNIFORM LITHIUM ON AN NI SUBSTRATE IN A NONAQUEOUS ELECTROLYTE [J].
KANAMURA, K ;
SHIRAISHI, S ;
TAKEHARA, Z .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1994, 141 (09) :L108-L110