Influence of brazing time on microstructure of high temperature brazing diamond with Ni-Cr alloy

被引:3
|
作者
Sun Bin [1 ]
Meng Pu [1 ]
Lu Jinbin [1 ]
Zhao Bin [1 ]
Liu Jian Jun [2 ]
机构
[1] Zhongyuan Univ Technol, Zhengzhou 450007, Peoples R China
[2] Zhengzhou Yutong Ground Co Ltd, Zhengzhou 450016, Peoples R China
关键词
brazing time; diamond; Ni-Cr alloy; microstructure; BRAZED DIAMOND; PARAMETERS; INTERFACE; GRITS; METAL;
D O I
10.4028/www.scientific.net/AMR.452-453.628
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Samples of high temperature brazing diamond with Ni-Cr alloy are prepared in protective atmosphere furnace for brazing time is 1 minute, 2 minutes, and 5 minutes. The microstructures were analyzed with Scanning electron microscope, energy dispersive spectroscopy and X-ray diffraction. The results show that there are two layers of carbides on the surface of diamond, lamellar carbide Cr3C2 and columnar carbide Cr7C3, the growth direction of Cr3C2 has a certain orientation relationship with the crystallographic plane of diamond, and Cr7C3 nucleates on the surface of Cr3C2. With the increase of brazing time, the morphology of carbide Cr3C2 turns from linear to lamellar and carbide Cr7C3 turns from granule to columnar. After brazing, chemical metallurgical combination is achieved between diamonds and brazing alloy and carbides are the primary reason for the strong bond strength.
引用
收藏
页码:628 / +
页数:2
相关论文
共 50 条
  • [21] Effects of brazing atmospheres on interfacial microstructure between diamond grits and brazing alloy
    Jiangsu Key Laboratory of Precision and Micro-Manufacturing Technology, NUAA, 29 Yudao Street, Nanjing 210016, China
    Trans. Nanjing Univ. Aero. Astro., 2008, 4 (248-253):
  • [22] Effects of brazing temperature and holding time on wettability of brazing diamond and brazing interface analysis
    Chen, Jigang
    Wang, Xiaokang
    Li, Xiangrui
    Li, Na
    Yang, Qingxiang
    WELDING IN THE WORLD, 2020, 64 (10) : 1763 - 1770
  • [23] Effects of brazing temperature and holding time on wettability of brazing diamond and brazing interface analysis
    Jigang Chen
    Xiaokang Wang
    Xiangrui Li
    Na Li
    Qingxiang Yang
    Welding in the World, 2020, 64 : 1763 - 1770
  • [24] Research on brazing behaviour between diamond grinding wheel and Ni - Cr alloy
    Yao, Z.
    Xu, H.
    Xiao, B.
    Wu, Z.
    Nongye Jixie Xuebao/Transactions of the Chinese Society of Agricultural Machinery, 2001, 32 (04): : 96 - 98
  • [25] Residual stress distribution in synthetic diamond grains brazed with Ni-Cr brazing filler metal
    Meng, Pu
    MATERIA-RIO DE JANEIRO, 2023, 28 (03):
  • [26] Thermodynamic studies on interfacial reactions between diamond and Ni-Cr filler metal in vacuum brazing
    Lu, Jin-Bin
    Xu, Jiu-Hua
    Xu, Hong-Jun
    Fu, Yu-Can
    Jiang, Cheng-Yu
    Hanjie Xuebao/Transactions of the China Welding Institution, 2004, 25 (01): : 21 - 24
  • [27] REDUCTION IN THE STRENGTH OF A DISPERSION-HARDENING ALLOY OF THE NI-CR SYSTEM UNDER THE EFFECT OF THE BRAZING ALLOY
    PRIVEZENTSEV, VV
    SEMENOV, VN
    WELDING PRODUCTION, 1980, 27 (10): : 39 - 41
  • [28] High temperature brazing of diamond tools
    姚正军
    苏宏华
    傅玉灿
    徐鸿钧
    TransactionsofNonferrousMetalsSocietyofChina, 2005, (06) : 1297 - 1302
  • [29] High temperature brazing of diamond tools
    Yao, Zheng-Jun
    Su, Hong-Hua
    Fu, Yu-Can
    Xu, Hong-Jun
    Transactions of Nonferrous Metals Society of China (English Edition), 2005, 15 (06): : 1297 - 1302
  • [30] High temperature brazing of diamond tools
    Yao, ZJ
    Su, HH
    Fu, YC
    Xu, HJ
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2005, 15 (06) : 1297 - 1302