The effects of aging treatment and strain rates on damage evolution in AA 6061 aluminum alloy in compression

被引:45
作者
Adesola, A. O. [1 ]
Odeshi, A. G. [1 ]
Lanke, U. D.
机构
[1] Univ Saskatchewan, Dept Mech Engn, Saskatoon, SK S7N 5A9, Canada
基金
加拿大自然科学与工程研究理事会; 加拿大健康研究院;
关键词
Aluminum alloy; Precipitation hardening; High strain rates; Microstructure; Adiabatic shear bands; ADIABATIC SHEAR BANDS; MG-SI ALLOYS; DYNAMIC DEFORMATION; MICROSTRUCTURAL EVOLUTION; PRECIPITATION; LOCALIZATION; FRACTURE; RECRYSTALLIZATION; BEHAVIOR;
D O I
10.1016/j.matdes.2012.08.021
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
AA 6061 aluminum alloy in T4, T6 and T8 temper were subjected to quasi-static compressive loading at a strain-rate of 3.2 x 10(-3) s(-1) and dynamic compressive loading at strain-rates between 7.0 x 10(3) and 8.5 x 10(3) s(-1). The effects of strain rates and temper condition on the deformation behavior of the alloy are discussed. Under the quasi-static loading, deformation was relatively homogeneous and controlled by strain hardening, which is more pronounced in the naturally aged than the artificially aged alloys. Thermal softening played a dominant role under impact loading leading to strain localization along narrow bands called adiabatic shear bands (ASBs). Both deformed bands consisting of aligned second phase particles and transformed bands consisting of fine recrystallized grains were observed. The average size of the recrystallized grains in the transformed bands is about 600 nm and varies slightly depending on the temper condition. The fine grains are suggested to form by dynamic recrystallization. The T4 alloy showed the highest propensity for thermal softening, strain localization and cracking under impact loading while the T8 alloy showed the least tendency. The degree of recrystallization in the transformed band is influenced by temper condition with T8 alloy having the highest fraction of unrecrystallized grains inside the transformed bands. This is related to the temperature rise in the transformed bands that was estimated to be highest in the T4 alloy and lowest in the T8 alloy. The combined effects of high temperature and severe strain inside the transformed bands caused dissolution of second phase particles and induced microstructural changes that resulted in less silicon inside the transformed bands than in the adjacent region. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:212 / 221
页数:10
相关论文
共 43 条
  • [41] Shear localization and recrystallization in dynamic deformation of 8090 Al-Li alloy
    Xu, YB
    Zhong, WL
    Chen, YJ
    Shen, LT
    Liu, Q
    Bai, YL
    Meyers, MA
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 299 (1-2): : 287 - 295
  • [42] Shear localization in dynamic deformation: Microstructural evolution
    Xu, Yongbo
    Zhang, Jinghua
    Bai, Yilong
    Meyers, Marc Andre
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (04): : 811 - 843
  • [43] Damage and fracture mechanism of aluminium alloy thick-walled cylinder under external explosive loading
    Yang, Y.
    Zeng, Y.
    Li, D. H.
    Li, M.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 490 (1-2): : 378 - 384