Role of Boundary Strengthening on Prevention of Type IV Failure in High Cr Ferritic Heat-Resistant Steels

被引:30
作者
Liu, Yuan [1 ]
Tsukamoto, Susumu [1 ]
Sawada, Kota [2 ]
Abe, Fujio [2 ]
机构
[1] Natl Inst Mat Sci, Struct Mat Unit, Tsukuba, Ibaraki 3050047, Japan
[2] Natl Inst Mat Sci, Mat Reliabil Unit, Tsukuba, Ibaraki 3050047, Japan
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2014年 / 45A卷 / 03期
关键词
CREEP STRENGTH; REVERSE TRANSFORMATION; WELDED-JOINTS; 9CR STEEL; MICROSTRUCTURE; SUPPRESSION; AUSTENITE; MECHANISM; BEHAVIOR; FRACTURE;
D O I
10.1007/s11661-013-2072-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructure evolution of newly developed 9Cr-3W-3Co-V, Nb steel with boron addition (B steel) has been analyzed during HAZ thermal cycle at the peak temperature of around A(c3) (A(c3) HAZ) and post-weld heat treatment (PWHT) to elucidate the prevention mechanism of type IV failure by boron addition. It was found that enhancement of the boundary strengthening by precipitates is the main reason for prevention of type IV failure by boron addition. In B steel HAZ, original austenite is reconstituted through martensitic alpha to gamma reverse transformation during the heating and original martensite is reconstituted through martensitic transformation during cooling of the A(c3) HAZ thermal cycle. This process allows M23C6 carbides to precipitate at the prior austenite grain (PAG) and block boundaries during PWHT even if the chemical segregation of carbide forming elements exists. The effect of boundary strengthening on the creep property has also been investigated. Microstructure evolution during creep was compared among Gr.92 with different A(c3) HAZ microstructures prepared by three kinds of heat treatments and B steel. The results revealed that both the boundary length and kernel average misorientation value decreased in all samples during creep. However, this process occurred very rapidly in A(c3) HAZ simulated Gr.92, whereas it was significantly retarded in the other samples with sufficient boundary strengthening by precipitates. This result confirms that the precipitates formed at PAG and block boundaries play the most important role to stabilize the microstructure of A(c3) HAZ simulated samples during creep and prolong the creep life.
引用
收藏
页码:1306 / 1314
页数:9
相关论文
共 25 条
[1]   Stabilization of martensitic microstructure in advanced 9Cr steel during creep at high temperature [J].
Abe, F ;
Horiuchi, T ;
Taneike, M ;
Sawada, K .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 378 (1-2) :299-303
[2]   Microstructure and creep strength of welds in advanced ferritic power plant steels [J].
Abe, F ;
Tabuchi, M .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2004, 9 (01) :22-30
[3]   Microstructure evolution in HAZ and suppression of Type IV fracture in advanced ferritic power plant steels [J].
Abe, F. ;
Tabuchi, M. ;
Tsukamoto, S. ;
Shirane, T. .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2010, 87 (11) :598-604
[4]   Suppression of Type IV fracture and improvement of creep strength of 9Cr steel welded joints by boron addition [J].
Abe, Fujio ;
Tabuchi, Masaaki ;
Kondo, Masayuki ;
Tsukamoto, Susumu .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2007, 84 (1-2) :44-52
[5]   Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants [J].
Abe, Fujio .
SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2008, 9 (01)
[6]   Improving the creep properties of 9Cr-3W-3Co-NbV steels and their weld joints by the addition of boron [J].
Albert, SK ;
Kondo, M ;
Tabuchi, M ;
Yin, FX ;
Sawada, K ;
Abe, F .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (02) :333-343
[7]   Type IV cracking in ferritic power plant steels [J].
Francis, J. A. ;
Mazur, W. ;
Bhadeshia, H. K. D. H. .
MATERIALS SCIENCE AND TECHNOLOGY, 2006, 22 (12) :1387-1395
[8]   HARDNESS OF TEMPERED MARTENSITE IN CARBON AND LOW-ALLOY STEELS [J].
GRANGE, RA ;
HRIBAL, CR ;
PORTER, LF .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1977, 8 (11) :1775-1785
[9]   Type IV Creep Damage Behavior in Gr.91 Steel Welded Joints [J].
Hongo, Hiromichi ;
Tabuchi, Masaaki ;
Watanabe, Takashi .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2012, 43A (04) :1163-1173
[10]  
Horiuchi Toshiaki., 2002, ISIJ International, V42, pS67, DOI DOI 10.2355/ISIJINTERNATIONAL.42.SUPPL_S67