Crack-healing behavior and strength recovery of hot-pressed TZ3Y20A-MoSi2 ceramics

被引:13
作者
Zhang, Xiu-Ping [1 ]
Ouyang, Jia-Hu [1 ]
Liu, Zhan-Guo [1 ]
Wang, Yu-Jin [1 ]
Wang, Ya-Ming [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2015年 / 648卷
基金
中国国家自然科学基金;
关键词
Crack-healing; MoSi2; Heat treatment; Oxidation reaction; Ceramics; HIGH-TEMPERATURE STRENGTH; SI3N4/SIC CERAMICS; FATIGUE-STRENGTH; COMPOSITE; STRESS; SIOX;
D O I
10.1016/j.msea.2015.09.041
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Crack-healing behavior and strength recovery of ZrO2(Y2O3)-Al2O3-MoSi2 (TZ3Y20A-MoSi2) ceramics have been investigated. Heat treatment in air enhances distinctly the flexural strength of TZ3Y20A-MoSi2 ceramics. Si-O oxide and ZrSiO4 are found after heat treatment, in which the former heals the cracks and recovers the strength, however, the latter is one kind of brittle materials that reduces mechanical performance of ceramics. The TZ3Y20A-10 vol% MoSi2 ceramic has a complete crack-healing effect and strength recovery by suitable heat treatment at 1373 K for 3 h in air, however, the strength does not recover completely under other heat treatment conditions. With further increasing the MoSi2 contents to 20 vol%, the flexural strength of as heat-treated TZ3Y20A-MoSi2 ceramics is higher than that of pre-cracked specimens, but remains lower than that of smooth specimens. Crack closure and rebonding of the crack walls are due to the formation of Si-O glassy phase by oxidation reaction. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:299 / 304
页数:6
相关论文
共 26 条
[1]   Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics [J].
Ando, K ;
Chu, MC ;
Tsuji, K ;
Hirasawa, T ;
Kobayashi, Y ;
Sato, S .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) :1313-1319
[2]   Crack-healing behavior of Si3N4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature [J].
Ando, K ;
Takahashi, K ;
Nakayama, S ;
Saito, S .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (09) :2268-2272
[3]  
[Anonymous], 2009, Self-healing materials: fundamentals, design strategies, and applications
[4]  
Byung-Soo Kim, 2003, Journal of the Society of Materials Science, Japan, V52, P667, DOI 10.2472/jsms.52.667
[5]  
Chen H, 2012, INT J ELECTROCHEM SC, V7, P12680
[6]   Crack healing in silicon carbide [J].
Chu, MC ;
Cho, SJ ;
Lee, YC ;
Park, HM ;
Yoon, DY .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (03) :490-492
[7]   Effects of random particle dispersion and size on the indentation behavior of SiC particle reinforced metal matrix composites [J].
Ekici, Recep ;
Apalak, M. Kemal ;
Yildirim, Mustafa ;
Nair, Fehmi .
MATERIALS & DESIGN, 2010, 31 (06) :2818-2833
[8]   Ion beam effects in SiOx (x < 2) subjected to low energy Ar+, He+ and N+ bombardment [J].
Holgado, JP ;
Barranco, A ;
Yubero, F ;
Espinos, JP ;
González-Elipe, AR .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2002, 187 (04) :465-474
[9]  
Hu J.H, 2002, HDB PRACTICAL INORGA
[10]   Indentation crack healing in low glass-content mullite [J].
Hvizdos, P ;
Kasiarová, M .
FRACTOGRAPHY OF ADVANCED CERAMICS, 2002, 223 :257-260