Bond strength and durability of universal adhesive agents with lithium disilicate ceramics: A shear bond strength study

被引:6
|
作者
AlRabiah, Mohammed [1 ,2 ]
Labban, Nawaf [1 ]
Levon, John A. [2 ]
Brown, David T. [3 ]
Chu, Tien-Min [4 ]
Bottino, Marco C. [4 ]
Platt, Jeffery A. [4 ]
机构
[1] King Saud Univ, Coll Dent, Dept Prosthet Dent Sci, Riyadh, Saudi Arabia
[2] Indiana Univ, Sch Dent, Dept Prosthodont, Indianapolis, IN USA
[3] Indiana Univ, Sch Dent, Dept Comprehens Care & Gen Dent, Indianapolis, IN USA
[4] Indiana Univ, Sch Dent, Dept Biomed & Appl Sci, Indianapolis, IN USA
关键词
Universal adhesive agent; Silane; ageing; shear bond strength; durability; FIXED PARTIAL DENTURES; DENTAL CERAMICS; RESIN; MICROSTRUCTURE; SILANE; COMPOSITE; ZIRCONIA; PRIMERS;
D O I
10.1080/01694243.2017.1372932
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The aim was to assess the shear bond strength (SBS) of lithium disilicate (LD) ceramic to resin composite with different universal adhesives, duration of ageing and silane. One hundred and twenty LD ceramic discs were processed, fired and etched (HF acid 5%) for 20 s (sec). All specimens were divided into 12 groups (n = 10), based on different combinations of, 3 different universal adhesives [Scotchbond (SB) Universal Adhesive, All-Bond (AB) Universal, and Futurabond U (FU)], silane and different duration of ageing [24 h and 3 months]. Composite resin cylinders (Tetric ceram) (3 mm x 2 mm) were formed using bonding jig on ceramic and were light-cured. The specimens in groups 1-6 and 7-12 were stored in distilled water (37 degrees C) for 24 h and 3 months (thermocycling -5000 cycles 5-55 degrees C/30 s dwell time) before being subjected to bond strength testing respectively. Using universal testing machine shear bond test was performed at a crosshead speed of 1 mm/min. Failure modes and fracture patterns were assessed using stereomicroscope and scanning electron microscope. Analysis of variance was performed to analyze data. SBS was significantly higher with silane than without silane (p < 0.01), regardless of the type of adhesive or storage duration. Specimens tested at 24 h storage showed significantly higher (p < 0.01) SBS than specimens tested after 3-months. A comparison among different universal adhesives showed significantly distinct bond strength (p < 0.01). Optimal bonds to LD were achieved by application of silane. While ageing through storage had a negative impact on the SBS, it varied among different adhesives.
引用
收藏
页码:580 / 589
页数:10
相关论文
共 50 条
  • [31] THE SHEAR BOND STRENGTH OF SELF- ADHESIVE RESIN CEMENTS TO DENTAL CERAMICS
    Pirvu, Daniela Aurelia
    Galbinasu, Bogdan Mihai
    Patrascu, Ion
    Pirvu, Cristina Florentina
    Nitoi, Dan
    REVISTA ROMANA DE MATERIALE-ROMANIAN JOURNAL OF MATERIALS, 2012, 42 (02): : 193 - 203
  • [32] Effect of grape seed extract on the bond strength and adhesion durability of universal adhesive to dentin
    Abd El-Aal, Nermin H.
    Abed El-Haliem, Huda
    Zaghloul, Nadia M.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2022, 113
  • [33] Shear bond strength vs. μ-tensile bond strength of three adhesive systems.
    Nunes, MF
    Perdigao, J
    de Castro, PS
    Cardoso, PEC
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 361 - 361
  • [34] Effects of Lithium and Phosphorus on the Efficacy of a Liner for Increasing the Shear Bond Strength Between Lithium Disilicate and Zirconia
    Lee, Young-Hoon
    Park, Chan-Jin
    Cho, Lee-Ra
    Ko, Kyung-Ho
    Huh, Yoon-Hyuk
    JOURNAL OF ADHESIVE DENTISTRY, 2018, 20 (06): : 535 - 540
  • [35] Influence of Surface Treatment of Lithium Disilicate on Roughness and Bond Strength
    Sudre, Joao Paulo
    Salvio, Luciana Andrea
    Baroudi, Kusai
    Sotto-Maior, Bruno Salles
    Melo-Silva, Claudio Luis
    Souza Picorelli Assis, Neuza Maria
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2020, 33 (02) : 212 - 216
  • [36] Effect of universal adhesive pretreatments on the bond strength durability of conventional and adhesive resin cements to zirconia ceramic
    Kwon, Tae-Yub
    Han, Seung-Hee
    Lee, Du-Hyeong
    Park, Jin-Woo
    Kim, Young Kyung
    JOURNAL OF ADVANCED PROSTHODONTICS, 2024, 16 (02): : 105 - 114
  • [37] Influence of surface treatment of contaminated lithium disilicate and leucite glass ceramics on surface free energy and bond strength of universal adhesives
    Yoshida, Fumi
    Tsujimoto, Akimasa
    Ishii, Ryo
    Nojiri, Kie
    Takamizawa, Toshiki
    Miyazaki, Masashi
    Latta, Mark A.
    DENTAL MATERIALS JOURNAL, 2015, 34 (06) : 855 - 862
  • [38] The effect of hemostatic agents and dentin cleansing protocols on shear bond strength of resin composite using universal adhesive: an in vitro study
    Abu-Nawareg, Manar M.
    Hajjaj, Maher S.
    AbuHaimed, Tariq S.
    Ajaj, Reem A.
    Abuljadayel, Roaa
    AlNowailaty, Yousef
    Alnoury, Arwa
    Khouja, Naseeba
    Naguib, Ghada H.
    Alzahrani, Saeed J.
    Abuelenain, Dalia A.
    BMC ORAL HEALTH, 2024, 24 (01):
  • [39] Shear bond strengths of different substrates bonded to lithium disilicate ceramics
    Bitter, Kerstin
    Paris, Sebastian
    Hartwig, Christian
    Neumann, Konrad
    Kielbassa, Andrej M.
    DENTAL MATERIALS JOURNAL, 2006, 25 (03) : 493 - 502
  • [40] Bond strength of universal adhesive systems to enamel.
    Manhart, J
    Li, D
    Eldiwany, M
    Powers, JM
    Hickel, R
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 167 - 167