A Simple Method to Produce Fiber Metal Laminates with Enhanced Mechanical Properties Using an Ethylene Vinyl Acetate (EVA)-based Adhesive Film

被引:2
作者
Kim, Jinku [1 ]
机构
[1] Hongik Univ, Dept Bio & Chem Engn, 2639 Sejong Ro, Sejong 30016, South Korea
基金
新加坡国家研究基金会;
关键词
fiber metal laminates (FMLs); mechanical strength; glass fiber reinforced plastic; adhesive film; SURFACE PRETREATMENT; VOID CONTENT; ALUMINUM; GLARE; PERFORMANCE; MORPHOLOGY; FATIGUE; JOINTS; WATER;
D O I
10.7317/pk.2019.43.2.295
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Fiber metal laminates (FMLs) have lower density and greater mechanical strength, compared with metal alloys, however it is known that their mechanical properties highly depend on interfacial strength between metal and composite. We introduce a simple method for producing FMLs with enhanced mechanical strength by incorporation of ethylene vinyl acetate-based film without any pre-treatment steps. In addition, to reduce the curing time, an in-house hot press was used to fabricate the FMLs, instead of using conventional autoclave method. Hybrid composites were prepared to place an adhesive layer between prepreg layer and aluminum layer and an in-house hot press and an autoclave (as a control) was also used to fabricate FMLs. Tensile strength, flexural strength, and peel adhesion strength of the FMLs were measured and compared. The results revealed that interfacial void formation was minimized by insertion of the adhesive film and, as a result, mechanical strength of the FMLs with adhesive film was greater than those without the film. This simple method may be useful to produce a FML with improved mechanical strength.
引用
收藏
页码:295 / 301
页数:7
相关论文
共 23 条
  • [1] Fatigue and damage tolerance issues of Glare in aircraft structures
    Alderliesten, R. C.
    Homan, J. J.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (10) : 1116 - 1123
  • [2] Long term behaviour of Glare
    Borgonje, B
    Ypma, MS
    [J]. APPLIED COMPOSITE MATERIALS, 2003, 10 (4-5) : 243 - 255
  • [3] Evaluation of adhesion of continuous fiber-epoxy composite/aluminum laminates
    Botelho, EC
    Silva, RA
    Pardini, LC
    Rezende, MC
    [J]. JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2004, 18 (15-16) : 1799 - 1813
  • [4] Botelho Edson Cocchieri, 2006, Mat. Res., V9, P247
  • [5] Strategies for the replacement of chromic acid anodising for the structural bonding of aluminium alloys
    Critchlow, GW
    Yendall, KA
    Bahrani, D
    Quinn, A
    Andrews, F
    [J]. INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2006, 26 (06) : 419 - 453
  • [6] Silane solution stability and film morphology of water-based bis-1,2-(triethoxysilyl)ethane for thin-film deposition on aluminium
    De Graeve, I.
    Tourwe, E.
    Biesemans, M.
    Willem, R.
    Terryn, H.
    [J]. PROGRESS IN ORGANIC COATINGS, 2008, 63 (01) : 38 - 42
  • [7] Failure of carbon composite-to-aluminum joints with combined mechanical fastening and adhesive bonding
    Kweon, Jin-Hwe
    Jung, Jae-Woo
    Kim, Tae-Hwan
    Choi, Jin-Ho
    Kim, Dong-Hyun
    [J]. COMPOSITE STRUCTURES, 2006, 75 (1-4) : 192 - 198
  • [8] The effect of surface treatments on interfacial fatigue crack initiation in aluminum/epoxy bonds
    Lefebvre, DR
    Ahn, BK
    Dillard, DA
    Dillard, JG
    [J]. INTERNATIONAL JOURNAL OF FRACTURE, 2002, 114 (02) : 191 - 202
  • [9] Effect of surface morphology on crack growth at a sol-gel reinforced epoxy/aluminum interface
    Liu, J
    Chaudhury, MK
    Berry, DH
    Seebergh, JE
    Osborne, JH
    Blohowiak, KY
    [J]. JOURNAL OF ADHESION, 2006, 82 (05) : 487 - 516
  • [10] Effects of cure cycles on void content and mechanical properties of composite laminates
    Liu, L
    Zhang, BM
    Wang, DF
    Wu, ZJ
    [J]. COMPOSITE STRUCTURES, 2006, 73 (03) : 303 - 309