Nano-deposition on 3-D open-cell aluminum foam materials for improved energy absorption capacity

被引:27
作者
Wang, Wei [1 ]
Burgueno, Rigoberto [2 ]
Hong, Jung-Wuk [2 ,3 ]
Lee, Ilsoon [1 ]
机构
[1] Michigan State Univ, Dept Chem Engn & Mat Sci, E Lansing, MI 48824 USA
[2] Michigan State Univ, Dept Civil & Environm Engn, E Lansing, MI 48824 USA
[3] Korea Adv Inst Sci & Technol, Dept Civil & Environm Engn, Taejon 305701, South Korea
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2013年 / 572卷
基金
美国国家科学基金会;
关键词
Open-cell foam; Energy absorption capacity; 3-D electro-deposition; Nano-crystalline; RECEPTOR GROUP DENSITY; METALLIC FOAMS; MECHANICAL-PROPERTIES; POLYMER; ELECTRODEPOSITION; BEHAVIOR; COPPER; FILMS;
D O I
10.1016/j.msea.2013.02.032
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Open cell aluminum (Al) foams have been used as energy absorbers for decades. Their energy absorption capacity can be enhanced by thickening the foam struts, or increasing the foam's relative density. However, the enhancement is compromised by the inherent characteristics of its stress-strain property relationship, whereby upon homogeneous strut thickening, an increase in the plateau stress without a reduction in densification strain cannot be achieved. In this work, to overcome this inherent barrier, nano-crystalline copper (Cu) was deposited onto the Al foam and novel 3-D Cu/Al, heterogeneously thickened, composite foam structured materials were fabricated and tested for the first time. A non-cyanide nano-crystalline copper electro-deposition system was setup for the coating of open-cell Al foam, and, the energy absorption capacity as a function of foam pore size and Cu coating thickness was investigated. A variety of characterization methods confirmed the nano-crystalline structure of the Cu deposition (38 nm). The energy absorption capacity of Al foams (with average strut thickness of 192 mu m) reinforced with a 60 mu m Cu coating was 3 times greater than that of plain foams. The compressive stress-strain response of the composite samples showed no significant reduction of the densification strain compared to the uncoated foams due to the small change in the foam strut thickness and pore size. A comparison between thin Cu-coated and uncoated Al foam samples with the same overall strut thickness (i.e., same effective volume density and porosity) showed that the nano-reinforced foams had superior energy absorption capacity over plain foams with the same overall thickness, (similar to 2 times greater). (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:75 / 82
页数:8
相关论文
共 46 条
[1]   Control of specular and diffuse reflection of light using particle self-assembly at the polymer and metal interface [J].
Ahn, Jin Soo ;
Hendricks, Troy R. ;
Lee, Ilsoon .
ADVANCED FUNCTIONAL MATERIALS, 2007, 17 (17) :3619-3625
[2]  
Akiyama S., 1987, U.S. Patent, Patent No. [4713277, 4,713,277]
[3]  
[Anonymous], 2005, B25387 ASTM, pB253
[4]  
[Anonymous], 1953, STAND XRAY DIFFR POW
[5]   The properties of foams and lattices [J].
Ashby, MF .
PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 2006, 364 (1838) :15-30
[6]   THE MECHANICAL-PROPERTIES OF CELLULAR SOLIDS [J].
ASHBY, MF .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (09) :1755-1769
[7]  
Avallone E.A., 2006, MARKS STANDARD HDB M, V11th
[8]   Manufacture, characterisation and application of cellular metals and metal foams [J].
Banhart, J .
PROGRESS IN MATERIALS SCIENCE, 2001, 46 (06) :559-U3
[9]   Aluminium foams for transport industry [J].
Baumeister, J ;
Banhart, J ;
Weber, M .
MATERIALS & DESIGN, 1997, 18 (4-6) :217-220
[10]  
Bicelli LP, 2008, INT J ELECTROCHEM SC, V3, P356