Effects of H2O and H2O2 on thermal desorption of tritium from stainless steel

被引:8
作者
Quinlan, M. J. [1 ]
Shmayda, W. T.
Lim, S.
Salnikov, S.
Chambers, Z.
Pollock, E.
Schroeder, W. U.
机构
[1] Univ Rochester, Laser Energet Lab, Rochester, NY 14627 USA
关键词
D O I
10.13182/FST54-519
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Tritiated stainless steel was subjected to thermal desorption at various temperatures, different temperature profiles, and in the presence of different helium carrier gas additives. In all cases the identities of the desorbing tritiated species were characterized as either water soluble or insoluble. The samples were found to contain 1.1 mCi +/- 0.4 mCi. Approximately ninety-five percent of this activity was released in molecular water-soluble form. Additives of H(2)O or H(2)O(2) to dry helium carrier gas increase the desorption rate and lower the maximum temperature to which the sample must be heated, in order to remove the bulk of the tritium. The measurements validate a method of decontamination of tritiated steel and suggest a technique that can be used to further explore the mechanisms of desorption from tritiated metals.
引用
收藏
页码:519 / 522
页数:4
相关论文
共 8 条
[1]   CHEMICAL DECONTAMINATION OF THE TRITIUM-SORBING SURFACE OF TYPE-316 STAINLESS-STEEL [J].
HIRABAYASHI, T ;
SAEKI, M ;
TACHIKAWA, E .
JOURNAL OF NUCLEAR MATERIALS, 1985, 136 (2-3) :179-185
[2]   TRITIUM MASS BALANCE IN THE PIPING SYSTEM OF A FUSION-REACTOR [J].
NISHIKAWA, M ;
TAKEISHI, T ;
KAWAMURA, Y ;
TAKAGI, Y ;
MATSUMOTO, Y .
FUSION TECHNOLOGY, 1992, 21 (02) :878-882
[3]   Adsorption and desorption behavior of tritiated water on the piping materials [J].
Shiraishi, T ;
Odoi, S ;
Nishikawa, M .
JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 1997, 34 (07) :687-694
[4]  
SHMAYDA WT, 1996, FUSION TECHNOL, P1245
[5]  
SHMAYDA WT, 1992, 9251K ONT HYDR
[6]   Migration and release behavior of tritium in SS316 at ambient temperature [J].
Torikai, Y. ;
Murata, D. ;
Penzhorn, R.-D. ;
Akaishi, K. ;
Watanabe, K. ;
Matsuyama, M. .
JOURNAL OF NUCLEAR MATERIALS, 2007, 363 (1-3) :462-466
[7]   Chronic release of tritium from SS316 at ambient temperature: Correlation between depth profile and tritium liberation [J].
Torikai, Y ;
Penzhorn, RD ;
Matsuyama, M ;
Watanabe, K .
FUSION SCIENCE AND TECHNOLOGY, 2005, 48 (01) :177-181
[8]  
WISE H, 1990, MAT CONCEPTS SURFACE, P64