The effect of margin thickness, degree of convergence and bonding interlayer on the marginal failure of glass-simulated all-ceramic crowns

被引:14
作者
Sornsuwan, Tanapon [1 ,2 ]
Swain, Michael V. [1 ]
机构
[1] Univ Sydney, Discipline Biomat, Fac Dent, Sydney, NSW 2010, Australia
[2] Naresuan Univ, Fac Dent, Restorat Dept, Phitsanulok, Thailand
关键词
All-ceramic crown; Fracture strength; Degree of convergence; Margin thickness; Resin adhesive; FRACTURE-MECHANICS ANALYSIS; FINITE-ELEMENT-ANALYSIS; THIN COATINGS; DENTAL CROWNS; STRENGTH; RESISTANCE; DESIGN; RESTORATIONS; TEETH; INDENTATION;
D O I
10.1016/j.actbio.2012.08.006
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The objectives objectives of this study were to identify the effect of design parameters, namely marginal thickness, degree of convergence and the different interfacial conditions, on the initial failure load that induces cracking from the margin in glass-simulated dental crowns. Crown-like glass cylinders were prepared to simulate posterior all-ceramic crowns with two different marginal thicknesses (0.8 or 1.2 mm) and degrees of convergence (6 degrees or 12 degrees). A three-step bonding system was used complementarily with a silane coupling agent to adhesively bond the specimens to resin dies. The crowns were subjected to an axial applied load to generate hoop tensile stress at the crown margin. The entire loading and fracture processes were recorded by video camera. The loading data were compared with the other two interfacial treatments (Vaseline grease and directly poured uncured resin on glass). The Weibull distribution was used to statistically analyze the characteristic failure load and the mean values. The fracture surfaces were fractographically analyzed along with the load-displacement curves, and the degrees of crack stability for each parameter were also identified. It was found that there is no difference in the initial failure load between the different marginal thicknesses in all interfacial conditions. The bonded crowns present more resistance to crack propagation. The higher convergence crown preparation can reduce the initial failure load at the crowns' margin, which can be resisted by a strongly bonded interface. Clear interactions between margin design parameters and their effects on the stress development and crack propagation are necessary to develop an appropriate design of all-ceramic crowns. (c) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:4426 / 4437
页数:12
相关论文
共 57 条
  • [51] Effect of convergence angle and luting agent on the fracture strength of In ceram crowns
    Correr Sobrinho L.
    Consani S.
    Knowles J.C.
    [J]. Journal of Materials Science: Materials in Medicine, 1999, 10 (8) : 493 - 496
  • [52] Thompson Van P., 2004, J. Appl. Oral Sci., V12, P26
  • [53] A comparison of the porcelain fracture resistance of screw-retained and cement-retained implant-supported metal-ceramic crowns
    Torrado, E
    Ercoli, C
    Al Mardini, M
    Graser, GN
    Tallents, RH
    Cordaro, L
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2004, 91 (06) : 532 - 537
  • [54] Minimizing Stress Concentrations in the Femoral Heads of Hip Joint Prostheses: Effect of Borehole Shapes
    Uddin, Mohammad Sharif
    Zhang, L. C.
    [J]. ADVANCES IN MATERIALS PROCESSING IX, 2010, 443 : 736 - 741
  • [55] The role of skirt geometry of dental crowns on the mechanics of failure: Experimental and numerical study
    Whitton, Anne
    Qasirn, Tarek
    Ford, Chris
    Hu, Xiao Zhi
    Bush, Mark
    [J]. MEDICAL ENGINEERING & PHYSICS, 2008, 30 (05) : 661 - 668
  • [56] Effect of occlusal contact size on interfacial stresses and failure of a bonded ceramic: FEA and monotonic loading analyses
    Yi, Yang-Jin
    Kelly, J. Robert
    [J]. DENTAL MATERIALS, 2008, 24 (03) : 403 - 409
  • [57] Contact fracture of full-ceramic crowns subjected to occlusal loads
    Zhang, Dongsheng
    Lu, Chenglin
    Zhang, Xiuyin
    Mao, Shuangshuang
    Arola, Dwayne
    [J]. JOURNAL OF BIOMECHANICS, 2008, 41 (14) : 2995 - 3001