Reinforcement effect of polyethylene fibre in root-filled teeth: comparison of two restoration techniques

被引:83
作者
Belli, S
Erdemir, A [1 ]
Yildirim, C
机构
[1] Kirikkale Univ, Fac Dent, Dept Endodont, TR-71200 Kirikkale, Turkey
[2] Selcuk Univ, Fac Dent, Dept Endodont, Konya, Turkey
关键词
endodontically treated teeth; fracture resistance; polyethylene ribbon fibre;
D O I
10.1111/j.1365-2591.2006.01057.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
To compare in vitro two different fibre placement techniques on reinforcement of root-filled molar teeth with mesio-occluso-distal (MOD) cavities. Fifty sound extracted human mandibular molars were used (n = 10). Group 1 served as control. From group 2-5, endodontic access and standard MOD cavities were prepared. Following root canal treatment, group 2 was kept unrestored. In groups 3 and 4, the teeth were restored with composite resin (AP-X; Kuraray, Japan). A groove was prepared on occlusal surface of the finished restorations in group 4 from buccal to lingual direction. Polyethylene woven fibre (Ribbond; Seattle, WA, USA) was inserted in the groove in combination with flowable resin that was cured for 20 s and covered with composite resin. Cavity surfaces were covered with flowable resin in group 5, and polyethylene fibre was placed into the bed of resin in a buccal to lingual direction before the composite restoration was placed. All specimens were stored in 100% humidity at 37 degrees C for 24 h. Compressive loading of the teeth was performed by a universal testing machine at a crosshead speed of 0.5 mm min(-1) until failure. The data were recorded in Newton and submitted to ANOVA and Tukey post hoc test. The mean load necessary to fracture the samples in each group was: G1: 1671.57 +/- 131.54(a); G2: 375.21 +/- 34.30(b); G3: 749.47 +/- 124.54(c); G4: 1224.36 +/- 132.17(d); G5: 926.88 +/- 118.28(e). Different superscript letters demonstrate significant difference between groups. Polyethylene fibre use over or under MOD composite restorations significantly increased fracture strength. However, when the fibre was placed on the occlusal surface of the restoration in buccal to lingual direction, significantly higher fracture resistance was observed.
引用
收藏
页码:136 / 142
页数:7
相关论文
共 30 条
[1]   Risk indicators for posterior tooth fracture [J].
Bader, JD ;
Shugars, DA ;
Martin, JA .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 2004, 135 (07) :883-892
[2]   The effect of fibre insertion on fracture resistance of root filled molar teeth with MOD preparations restored with composite [J].
Belli, S ;
Erdemir, A ;
Ozcopur, M ;
Eskitascioglu, G .
INTERNATIONAL ENDODONTIC JOURNAL, 2005, 38 (02) :73-80
[3]  
BLASER PK, 1983, OPER DENT, V8, P6
[4]   PUNCH SHEAR TESTING OF EXTRACTED VITAL AND ENDODONTICALLY TREATED TEETH [J].
CARTER, JM ;
SORENSEN, SE ;
JOHNSON, RR ;
TEITELBAUM, RL ;
LEVINE, MS .
JOURNAL OF BIOMECHANICS, 1983, 16 (10) :841-+
[5]  
ELSHERIF MH, 1988, OPER DENT, V13, P50
[6]   Use of polyethylene ribbon to create a provisional fixed partial denture after immediate implant placement: A clinical report [J].
Eskitascioglu, G ;
Eskitascioglu, A ;
Belli, S .
JOURNAL OF PROSTHETIC DENTISTRY, 2004, 91 (01) :11-14
[7]   Evaluation of two post core systems using two different methods (fracture strength test and a finite elemental stress analysis) [J].
Eskitascioglu, G ;
Belli, S ;
Kalkan, M .
JOURNAL OF ENDODONTICS, 2002, 28 (09) :629-633
[8]   RESISTANCE TO CUSP FRACTURE IN CLASS II PREPARED AND RESTORED PREMOLARS [J].
GELB, MN ;
BAROUCH, E ;
SIMONSEN, RJ .
JOURNAL OF PROSTHETIC DENTISTRY, 1986, 55 (02) :184-185
[9]  
GUSY GE, 1979, J PROSTHET DENT, V42, P39
[10]   RESISTANCE TO FRACTURE OF ENDODONTICALLY TREATED PREMOLARS RESTORED WITH NEW-GENERATION DENTIN BONDING SYSTEMS [J].
HERNANDEZ, R ;
BADER, S ;
BOSTON, D ;
TROPE, M .
INTERNATIONAL ENDODONTIC JOURNAL, 1994, 27 (06) :281-284