The repair bond strength to resin matrix in cured resin composites after water aging

被引:17
作者
Alqarni, Dhaifallah [1 ]
Nakajima, Masatoshi [1 ]
Hosaka, Keiichi [1 ]
Ide, Kurumi [1 ]
Nagano, Daiki [1 ]
Wada, Takehiro [2 ]
Ikeda, Masaomi [3 ]
Mamanee, Teerapong [4 ]
Thanatvarakorn, Ornnicha [5 ]
Prasansuttiporn, Taweesak [4 ,6 ]
Foxton, Richard [7 ]
Tagami, Junji [1 ]
机构
[1] Tokyo Med & Dent Univ, Dept Cariol & Operat Dent, Dept Oral Hlth Sci, Grad Sch Med & Dent Sci,Bunkyo Ku, 1-5-45 Yushima, Tokyo 1138549, Japan
[2] Tokyo Med & Dent Univ, Dept Adv Biomat, Oral Hlth Sci, Grad Sch Med & Dent Sci,Bunkyo Ku, 1-5-45 Yushima, Tokyo 1138549, Japan
[3] Tokyo Med & Dent Univ, Dept Oral Prosthet Engn, Grad Sch, Bunkyo Ku, 1-5-45 Yushima, Tokyo 1138549, Japan
[4] Chiang Mai Univ, Fac Dent, Dept Restorat Dent & Periodontol, Chiang Mai 50200, Thailand
[5] Bangkokthonburi Univ, Fac Dent, 16-10 Leabklongtaweewatana Rd, Bangkok 10170, Thailand
[6] Chiang Mai Univ, Ctr Excellence Mat Sci & Technol, Chiang Mai 50200, Thailand
[7] Kings Coll London, Kings Coll London Dent Inst, Restorat Dent, Floor 25, London SE1 9RT, England
关键词
Repair bond strength; Water aging; Resin matrix; Adhesive application; Degree of conversion; SURFACE TREATMENTS; SORPTION; SYSTEMS;
D O I
10.4012/dmj.2018-044
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The repair microshear bond strengths (SBSs) to resin matrices in 4 different cured-composites after water storage (0, 60 s, 1 week, 1 month) were evaluated. Three different adhesive application methods to the cured-composites were performed; (1) none, (2) one-step self-etch adhesive application, and (3) one-step self-etch adhesive application with a silane coupling agent. Degree of conversion (DC) of the composite discs was determined using ATR/FT-IR with a time-based spectrum analysis. Initially, the amount of unreacted resin monomers in the repaired cured-composite contributed to the bonding performance of newly-filled uncured-composite to resin matrix of the cured-composite. Adhesive application could not improve their repair SBS. After 1-month of water-storage, the repair SBS was dependent on material, which either reduced or did not and was not influenced by their amount of un-reacted resin monomers. When repairing aged composite resin, the appropriate adhesive application procedures were different among resin composites.
引用
收藏
页码:233 / 240
页数:8
相关论文
共 25 条
  • [1] Brendeke J, 2007, J ADHES DENT, V9, P399
  • [2] The influence of bis-EMA vs bis GMA on the degree of conversion and water susceptibility of experimental composite materials
    Cornelio, Roberto Belloti
    Wikant, Aksel
    Mjosund, Hanne
    Kopperud, Hilde Molvig
    Haasum, Johan
    Gedde, Ulf Wiel
    Ortengren, Ulf Thore
    [J]. ACTA ODONTOLOGICA SCANDINAVICA, 2014, 72 (06) : 440 - 447
  • [3] Durability of Surface Treatments and Intermediate Agents Used for Repair of a Polished Composite
    Costa, T. R. F.
    Ferreira, S. Q.
    Klein-Junior, C. A.
    Loguercio, A. D.
    Reis, A.
    [J]. OPERATIVE DENTISTRY, 2010, 35 (02) : 231 - 237
  • [4] Water uptake and strength characteristics of a nanofilled resin-based composite
    Curtis, A. R.
    Shortall, A. C.
    Marquis, P. M.
    Palin, W. M.
    [J]. JOURNAL OF DENTISTRY, 2008, 36 (03) : 186 - 193
  • [5] ALTERNATIVE INTERPRETATIONS OF WATER SORPTION VALUES OF COMPOSITE RESINS
    FAN, PL
    EDAHL, A
    LEUNG, RL
    STANFORD, JW
    [J]. JOURNAL OF DENTAL RESEARCH, 1985, 64 (01) : 78 - 80
  • [6] Galvao Marilia Regalado, 2013, Eur J Dent, V7, P86
  • [7] Giannini Marcelo, 2003, J Esthet Restor Dent, V15, P43, DOI 10.1111/j.1708-8240.2003.tb00281.x
  • [8] Hickel R, 2001, J Adhes Dent, V3, P45
  • [9] Imbery T A, 2014, Oper Dent, V39, pE250, DOI 10.2341/13-299-L
  • [10] Irmak O, 2017, J ISTANB UNIV FAC DE, V51, P25, DOI 10.17096/jiufd.31921