Improvement in mechanical and oxidation properties of TiAl alloys with Sb additions

被引:33
作者
Huang, BY [1 ]
He, YH [1 ]
Wang, JN [1 ]
机构
[1] Cent S Univ Technol, Natl Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
titanium aluminides; based on TiAl;
D O I
10.1016/S0966-9795(98)00136-8
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The objective of this study is to improve the mechanical properties and oxidation resistance by control of both alloy addition and microstructure in two-phase TiAl alloys based on Ti-48Al (at%). It is found that with the addition of up to 0.15Sb, the room temperature bending deflection and fracture strength (sigma(b)) can be enhanced significantly. For example, sigma(b) reaches as high as 1345 MPa in the alloy of Ti-48Al-0.15Sb. These improved properties are attributed mainly to the refinements of the colony grain size and the interlamellar spacing with the addition of Sb. Additionally, the high-temperature oxidation resistance can also be substantially increased in the presence of 0.15Sb, being higher than those for Ti-48Al and Ti-48Al-2Cr-2Nb. The cause for this increase is suggested to be the formation of a protective layer of Al2O3 stabilized by Sb. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:881 / 888
页数:8
相关论文
共 26 条
[1]   MECHANISM OF ISOTHERMAL OXIDATION OF THE INTERMETALLIC TIAL AND OF TIAL ALLOYS [J].
BECKER, S ;
RAHMEL, A ;
SCHORR, M ;
SCHUTZE, M .
OXIDATION OF METALS, 1992, 38 (5-6) :425-464
[2]  
Courtney TH., 1990, MECH BEHAV MAT
[3]   DUCTILE REINFORCEMENT TOUGHENING OF GAMMA-TIAL - EFFECTS OF DEBONDING AND DUCTILITY [J].
DEVE, HE ;
EVANS, AG ;
ODETTE, GR ;
MEHRABIAN, R ;
EMILIANI, ML ;
HECHT, RJ .
ACTA METALLURGICA ET MATERIALIA, 1990, 38 (08) :1491-1502
[4]  
FFRLAND KS, 1996, ACTA CHIMICA SCANDIN, V20, P2573
[5]   EFFECTS OF ADDITIONAL ELEMENTS ON MECHANICAL-PROPERTIES OF TIAL-BASE ALLOYS [J].
HASHIMOTO, K ;
DOI, H ;
KASAHARA, K ;
NAKANO, O ;
TSUJIMOTO, T ;
SUZUKI, T .
JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1988, 52 (11) :1159-1166
[6]   MICROSTRUCTURES AND PROPERTY TRADEOFFS IN WROUGHT TIAL-BASE ALLOYS [J].
HUANG, SC .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1992, 23 (01) :375-377
[7]  
HUANG SC, 1993, STRUCTURAL INTERMETALLICS, P299
[8]   PLASTIC-DEFORMATION AND FRACTURE OF BINARY TIAL-BASE ALLOYS [J].
HUANG, SC ;
HALL, EL .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (02) :427-439
[9]   THE EFFECTS OF CR ADDITIONS TO BINARY TIAL-BASE ALLOYS [J].
HUANG, SC ;
HALL, EL .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11) :2619-2627
[10]   ORDERED DOMAINS IN TIAL COEXISTING WITH TI3AL IN THE LAMELLAR STRUCTURE OF TI-RICH TIAL COMPOUNDS [J].
INUI, H ;
OH, MH ;
NAKAMURA, A ;
YAMAGUCHI, M .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1992, 66 (04) :539-555