Corrosion behaviour of Mg-Cu and Mg-Mo composites in 3.5% NaCl

被引:46
作者
Abhijeet, Budruk S. [1 ]
Balasubramaniam, R. [1 ]
Gupta, M. [2 ]
机构
[1] Indian Inst Technol, Dept Mat & Met Engn, Kanpur 208016, Uttar Pradesh, India
[2] Natl Univ Singapore, Dept Mech Engn, Singapore 119260, Singapore
关键词
Magnesium; Metal matrix composite; Cyclic voltammetry; Weight loss; Passivity; Pitting corrosion;
D O I
10.1016/j.corsci.2008.06.043
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The Corrosion behaviour of pure magnesium, Mg-Cu (0.3, 0.6, and 1 vol.%) and Mg-Mo (0.1, 0.3, and 0.6 vol.%) composites has been studied in 3.5% NaCl solution by weight loss and polarisation methods. Corrosion Fates determined by weight loss method were considerably higher than that determined by polarisation method. The corrosion rate increased with increasing volume fraction of reinforcement in Mg-Cu and Mg-Mo composites. At the same volume fraction of reinforcement, molybdenum reinforced composite corroded faster than copper reinforced composite. The galvanic current density between Mg-Cu and Mg-Mo couples has been experimentally measured using zero resistance ammeter technique. The experimentally observed galvanic current densities were in close agreement with those obtained using mixed potential theory analysis. SEM observation of corroded samples confirmed microgalvanic activity at the matrix/reinforcement interfaces. The poor corrosion resistance of composites has been attributed to microgalvanic effects between the matrix and reinforcements and inferior quality of surface films. (c) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2423 / 2428
页数:6
相关论文
共 17 条
[1]  
Foltz J.V., 1992, METAL MATRIX COMPOSI, V2, P2536
[2]   GALVANIC CORROSION BETWEEN SIC MONOFILAMENT AND MAGNESIUM IN NACL, NA2SO4 AND NANO3 SOLUTIONS FOR APPLICATION TO METAL-MATRIX COMPOSITES [J].
HIHARA, LH ;
KONDEPUDI, PK .
CORROSION SCIENCE, 1994, 36 (09) :1585-1595
[3]  
HIHARA LH, 1994, INT MATER REV, V39, P245, DOI 10.1179/095066094790151026
[4]   THE GALVANIC CORROSION OF SIC MONOFILAMENT/ZE41 MG METAL-MATRIX COMPOSITE IN 0.5 M NANO3 [J].
HIHARA, LH ;
KONDEPUDI, PK .
CORROSION SCIENCE, 1993, 34 (11) :1761-1772
[5]   Corrosion behaviour of high pressure die-cast and semi-solid cast AZ91D alloys [J].
Mathieu, S ;
Rapin, C ;
Hazan, J ;
Steinmetz, P .
CORROSION SCIENCE, 2002, 44 (12) :2737-2756
[6]   The electrochemical corrosion of pure magnesium in 1 N NaCl [J].
Song, G ;
Atrens, A ;
Stjohn, D ;
Nairn, J ;
Li, Y .
CORROSION SCIENCE, 1997, 39 (05) :855-875
[7]   The anodic dissolution of magnesium in chloride and sulphate solutions [J].
Song, G ;
Atrens, A ;
St John, D ;
Wu, X ;
Nairn, J .
CORROSION SCIENCE, 1997, 39 (10-11) :1981-2004
[8]  
Song GL, 1999, ADV ENG MATER, V1, P11, DOI 10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO
[9]  
2-N
[10]   Influence of processing parameters during disintegrated melt deposition processing on near net shape synthesis of aluminium based metal matrix composites [J].
Tham, LM ;
Gupta, M ;
Cheng, L .
MATERIALS SCIENCE AND TECHNOLOGY, 1999, 15 (10) :1139-1146