摘要
Currently, direct laser deposition technology is used to create products with complex geometry in various industries, such as: aircraft engine building, shipbuilding, and the energy industry. This technology allows made workpieces with minimal subsequent machining. Parts manufactured for these areas should have the required performance characteristics. The mechanical properties of products obtained using direct laser deposition technology are affected by internal and surface defects: pores, non-fusion, cracks, and roughness, since they are the main stress concentrators. This article describes such internal defects as pores and non-fusion in different situations, identifies the causes of their occurrence and considers their elimination methods. (C) 2019 Elsevier Ltd. All rights reserved.
引用
收藏
页码:523 / 527
页数:5
相关论文
共 50 条
[31]   Effect of post-heat treatment on mechanical, microstructure, and thermal properties of Nitinol (NiTiNb) manufactured using laser direct metal deposition (LDMD) process [J].
Skhosane, Samuel ;
Maledi, Nthabiseng ;
Pityana, Sisa ;
Lekoadi, Paul ;
Tlotleng, Monnamme .
MRS ADVANCES, 2025, 10 (09) :1103-1108
[32]   Effect of the Cooling Liquid on the Milled Interface in the Combined Process of Milling and Direct Metal Deposition [J].
Egorov, Sergei ;
Schudeleit, Timo ;
Wegener, Konrad .
MATERIALS, 2024, 17 (13)
[33]   Study on a multifield coupling mechanism and a numerical simulation method of a pulsed laser deposition process from a disk laser [J].
Han, Xing ;
Da Zhang, Cheng ;
Li, Chang ;
Yu, Zhi Bin ;
Zhang, BaoGui .
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2021, 127 (01)
[34]   Microstructure and mechanical properties of thin-wall structure by hybrid laser metal deposition and laser remelting process [J].
Xin, Bo ;
Zhou, Xianxin ;
Cheng, Guang ;
Yao, Jun ;
Gong, Yadong .
OPTICS AND LASER TECHNOLOGY, 2020, 127
[35]   Contact-Free Support Structures for the Direct Metal Laser Melting Process [J].
Celik, Alican ;
Tekoglu, Emre ;
Yasa, Evren ;
Sonmez, Mehmet Seref .
MATERIALS, 2022, 15 (11)
[36]   Metal solidification micro-structure simulation of direct laser deposition based on cellular automation [J].
Guan, Tingting ;
Chen, Suiyuan ;
Zhou, Yue ;
Cui, Tong ;
Liang, Jing ;
Liu, Changsheng .
2017 2ND INTERNATIONAL CONFERENCE ON MECHATRONICS AND INFORMATION TECHNOLOGY (ICMIT 2017), 2017, :156-160
[37]   Microstructure Evolution and Mechanical Behavior of Inconel 625 Produced Using Direct Laser Metal Deposition [J].
Wang, Xingcheng ;
Chen, Changjun ;
Qin, Lanlan ;
Zhang, Min .
PHYSICS OF METALS AND METALLOGRAPHY, 2021, 122 (09) :896-907
[38]   Prediction of deposit characteristics based on the discrete coaxial nozzle during laser direct metal deposition [J].
Han, Bin ;
Li, Rui ;
Pi, Qingyang ;
Shi, Yan ;
Qi, Huan ;
Bi, Kedong ;
Sun, Guifang .
OPTICS AND LASER TECHNOLOGY, 2023, 163
[39]   Synthesis of (Ti, Cr)xCy Carbides in VT6 Alloy by Direct Laser Deposition [J].
Gorunov, A. I. .
INORGANIC MATERIALS-APPLIED RESEARCH, 2024, 15 (05) :1437-1443
[40]   Laser Preheating for Hot Crack Reduction in Direct Metal Deposition of Inconel 738LC [J].
Soffel, Fabian ;
Papis, Konrad ;
Bambach, Markus ;
Wegener, Konrad .
METALS, 2022, 12 (04)