Self-healing characteristics of cement concrete containing expansive agent

被引:15
作者
Jeon, Sungil [1 ]
Hossain, Mohammad Shakhawat [2 ]
Han, Seungyeon [1 ,3 ]
Choi, Pangil [4 ]
Yun, Kyong-Ku [2 ]
机构
[1] Korea Inst Civil Engn & Bldg Technol KICT, Goyang 10223, South Korea
[2] Kangwon Natl Univ, Dept Civil Engn, 1 Gangwondaegil, Chunchon 24341, South Korea
[3] Kangwon Natl Univ, KIITKangwon Inst Inclus Technol, 1 Gangwondaegil, Chunchon 24341, South Korea
[4] Texas Dept Transportat, Maintenance Div, Austin, TX USA
关键词
Self-healing; Shrinkage; Ternary blended concrete; Expansion agent; Microscopic image analysis; Concrete overlay for bridge deck; CRACKS; BEHAVIOR; MORTAR; PERMEABILITY; MINERALS; SYSTEM;
D O I
10.1016/j.cscm.2022.e01609
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Many studies have been conducted to identify the self-healing effect in cementitious materials. However, the knowledge regarding the self-healing effect is insufficient to utilize this effect for design purposes. This study examined the influence of numerous admixtures such as expansive agents (EA), ultra-fine fly ash (UFFA), finely ground granulated blast furnace slag (FGGBS), and silica fume (SF) on the self-healing capacity of Portland cement concrete. Here, focused on investigating the effect of the expansive agent (EA) used in concrete mixtures to identify whether the EA could act as a self-healing trigger in concrete materials that are frequently used in a bridge deck overlay. Ordinary Portland cement concrete (OPC), latex-modified concrete (LMC), and silica fume concrete (SFC) was used to compare the effect of the EA (0,4,8%, and 12%) in the ternary blended cement concrete on each material for bridge deck overlay concrete. In this study, the crack width was examined at 0,7,14 and 28 days respectively which were inducement at 3 and 7 days age of concrete specimens by the microscopic image analysis system. Samples with healed cracks with a width range of 100-200 mu m and EA >= 8% on day 28 exhibited faster self-healing performance. Additionally, we calculated the self-cracking closing ratio and performed a microstructure analysis by SEM/EDS. Moreover, the compressive strength was examined at 7, 28,56, and 90 days for understanding the improved performance of all concrete mixtures.
引用
收藏
页数:20
相关论文
共 54 条
[1]  
Ahn T.H., 2008, THESIS U TOKYO JAPAN
[2]   Crack Self-healing Behavior of Cementitious Composites Incorporating Various Mineral Admixtures [J].
Ahn, Tae-Ho ;
Kishi, Toshiharu .
JOURNAL OF ADVANCED CONCRETE TECHNOLOGY, 2010, 8 (02) :171-186
[3]   Feasibility assessment on self-healing ability of cementitious composites with MgO [J].
Beshr, Saleh Salem B. ;
Mohaimen, I. M. Abdul ;
Azline, M. N. Noor ;
Azizi, S. Nor ;
Nabilah, A. B. ;
Aznieta, A. A. Farah Nora .
JOURNAL OF BUILDING ENGINEERING, 2021, 34
[4]  
Breugel K.V., 2007, P 1 INT C SELF HEAL, P18
[5]   Effect of age and level of damage on the autogenous healing of lime mortars [J].
De Nardi, C. ;
Cecchi, A. ;
Ferrara, L. ;
Benedetti, A. ;
Cristofori, D. .
COMPOSITES PART B-ENGINEERING, 2017, 124 :144-157
[6]  
Dhir R.K., 1973, ACI J. Proc, V70, P231, DOI [10.14359/11202, DOI 10.14359/11202]
[7]  
Edvardsen C, 1999, ACI MATER J, V96, P448
[8]   Progress and challenges in self-healing cementitious materials [J].
Fernandez, Carlos A. ;
Correa, Miguel ;
Nguyen, Manh-Thuong ;
Rod, Kenton A. ;
Dai, Gao L. ;
Cosimbescu, Lelia ;
Rousseau, Roger ;
Glezakou, Vassiliki-Alexandra .
JOURNAL OF MATERIALS SCIENCE, 2021, 56 (01) :201-230
[9]   On the use of crystalline admixtures in cement based construction materials: from porosity reducers to promoters of self healing [J].
Ferrara, Liberato ;
Krelani, Visar ;
Moretti, Fabio .
SMART MATERIALS AND STRUCTURES, 2016, 25 (08)
[10]   A "fracture testing" based approach to assess crack healing of concrete with and without crystalline admixtures [J].
Ferrara, Liberato ;
Krelani, Visar ;
Carsana, Maddalena .
CONSTRUCTION AND BUILDING MATERIALS, 2014, 68 :535-551