Mechanical performance and oxidation resistance of SiC castables with lamellar Ti3SiC2 coatings on SiC aggregates prepared by SPS

被引:13
作者
Chen, Ding [1 ]
Gu, Huazhi [1 ]
Huang, Ao [1 ]
Ni, Hongwei [1 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Hubei, Peoples R China
基金
中国国家自然科学基金; 对外科技合作项目(国际科技项目);
关键词
SiC castable; Lamellar Ti3SiC2 coatings; Antioxidation; Spark plasma sintering; Principle of electrowetting; INCORPORATING ZR; CHROME-FREE; SILICA; ENHANCEMENT;
D O I
10.1016/j.jallcom.2019.03.358
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
SiC castables face serious degradation under a 1700 degrees C oxidation atmosphere in plasma gasifier. We used spark plasma sintering (SPS) and added Ti/Zr combined with Si and carbon black to improve the mechanical performance and antioxidation of the SiC castable. Metal Ti and Si formed liquid drops at high temperature and carbon black dissolved into the drops to form Ti-Si-C drops. Based on the principle of electrowetting, the wetting of the SiC aggregate by the Ti-Si-C drop was improved significantly under a high-frequency pulse electric field in the SPS system. The Ti-Si-C drop coated the SiC aggregate and formed Ti3SiC2, which resulted in the SiC aggregates being coated by in-situ lamellar Ti3SiC2. The new binder phase significantly improved the mechanical properties and the lamellar Ti3SiC2 coating was preferentially oxidized to TiO2 and SiO2. The TiO2 pinned SiO2 glass, which formed a protective layer on the SiC aggregate surface against further oxidation. (C) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页码:461 / 468
页数:8
相关论文
共 24 条
  • [1] An evaluation of vaporizing rates of SiO2 and TiO2 as protective coatings for ultrahigh temperature ceramic composites
    Bronson, Arturo
    Chessa, Jack
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2008, 91 (05) : 1448 - 1452
  • [2] Effect of Ti combined with Si and C on mechanical performance and oxidation resistance of SiC castables for plasma gasifier
    Chen, Ding
    Gu, Huazhi
    Huang, Ao
    Deng, Yanwen
    [J]. CERAMICS INTERNATIONAL, 2019, 45 (04) : 4147 - 4151
  • [3] Incorporating Zr to achieve self-protecting and enhancement of silica sol bonded SiC castables at active oxidation condition
    Chen, Ding
    Gu, Huazhi
    Huang, Ao
    Deng, Yanwen
    [J]. CERAMICS INTERNATIONAL, 2018, 44 (06) : 6089 - 6095
  • [4] Incorporating Zr combined Si and C to achieve self-repairing ability and enhancement of silica sol bonded SiC castables
    Chen, Ding
    Gu, Huazhi
    Huang, Ao
    Deng, Yanwen
    Shao, Zhijun
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 732 : 396 - 405
  • [5] Towards chrome-free of high-temperature solid waste gasifier through in-situ SiC whisker enhanced silica sol bonded SiC castable
    Chen, Ding
    Gu, Huazhi
    Huang, Ao
    Shao, Zhijun
    [J]. CERAMICS INTERNATIONAL, 2017, 43 (03) : 3330 - 3338
  • [6] Corrosion of Al2O3-Cr2O3 refractory lining for high-temperature solid waste incinerator
    Chen, Ding
    Huang, Ao
    Gu, Huazhi
    Zhang, Meijie
    Shao, Zhijun
    [J]. CERAMICS INTERNATIONAL, 2015, 41 (10) : 14748 - 14753
  • [7] Growth of SiC nanowires on wooden template surface using molten salt media
    Ding, Jun
    Zhu, Hongxi
    Li, Guangqiang
    Deng, Chengji
    Li, Jun
    [J]. APPLIED SURFACE SCIENCE, 2014, 320 : 620 - 626
  • [8] Optimization of the Ti3SiC2 MAX phase synthesis
    El Saeed, M. A.
    Deorsola, F. A.
    Rashad, R. M.
    [J]. INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2012, 35 : 127 - 131
  • [9] Investigations of SiC aggregates oxidation: Influence on SiC castables refractories life time at high temperature
    Gallet-Doncieux, A.
    Bahloul, O.
    Gault, C.
    Huger, M.
    Chotard, T.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (04) : 737 - 743
  • [10] Effects of Ti/Al addition on the microstructures and ablation properties of Cf/C-MoSi2-SiC composites
    Hao, Zhenhua
    Sun, Wei
    Xiong, Xiang
    Chen, Zhaoke
    Wang, Yalei
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (03) : 457 - 464