Effect of Heat Input on Cleavage Crack Initiation of Simulated Coarse Grain Heat-affected Zone in Microalloyed Offshore Platform Steel

被引:10
作者
Lu, Feng [1 ,2 ]
Cheng, Guang-ping [1 ]
Chai, Feng [2 ]
Pan, Tao [2 ]
Shi, Zhong-ran [2 ]
Su, Hang [2 ]
Yang, Cai-fu [2 ]
机构
[1] Anhui Univ Technol, Sch Mat Sci & Engn, Maanshan 243002, Anhui, Peoples R China
[2] Cent Iron & Steel Res Inst, Dept Struct Steel, Beijing 100081, Peoples R China
关键词
simulated coarse-grained heat-affected zone; martensite-austenite constituent; pearlite colony; cleavage fracture; V-N-Ti microalloying; MICROSTRUCTURE; MARTENSITE; TOUGHNESS; CONSTITUENT; FRACTURE; VANADIUM; BEHAVIOR; NIOBIUM; CGHAZ;
D O I
10.1016/S1006-706X(16)30161-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The combined effects of martensite-austenite (MA) constituent and pearlite colony on cleavage crack initiation in the simulated coarse-grained heat-affected zone (CGHAZ) of V-N-Ti microalloyed offshore platform steel under different heat inputs were investigated. The results of welding simulation, instrumented impact test, and quantitative analysis indicated that the size of the MA constituent decreased with the increase in cooling time, and by contrast, the size of the pearlite colony increased. According to Griffith theory, the critical sizes of cleavage microcracks were calculated. With the increase of cooling time, the calculated microcrack size could be characterized by the size of the MA constituent first, and then fitted with the size of the pearlite colony. Moreover, the calculated microcrack size variation was opposite to the microcrack initiation energy. This phenomenon is probably due to the combined effects of the MA constituent and pearlite colony with increasing the cooling time of the specimen's temperature from 800 to 500 degrees C.
引用
收藏
页码:1086 / 1095
页数:10
相关论文
共 20 条
[1]   MICRO-FRACTURE BEHAVIOR INDUCED BY M-A CONSTITUENT (ISLAND MARTENSITE) IN SIMULATED WELDING HEAT-AFFECTED ZONE OF HT80 HIGH-STRENGTH LOW ALLOYED STEEL [J].
CHEN, JH ;
KIKUTA, Y ;
ARAKI, T ;
YONEDA, M ;
MATSUDA, Y .
ACTA METALLURGICA, 1984, 32 (10) :1779-1788
[2]   FRACTURE-BEHAVIOR OF C-MN STEEL MULTIPASS MMA WELD METALS AT -60-DEGREES-C IN CHARPY-V TESTING [J].
CHEN, JH ;
YAN, C .
MATERIALS SCIENCE AND TECHNOLOGY, 1988, 4 (08) :732-739
[3]  
Curry D. A., 1978, Metal Science, V12, P511
[4]   Numerical simulation of welding temperature field, residual stress and deformation induced by electro slag welding [J].
Deng, Dean ;
Kiyoshima, Shoichi .
COMPUTATIONAL MATERIALS SCIENCE, 2012, 62 :23-34
[5]  
GLADMAN T, 1972, J IRON STEEL I, V210, P916
[6]   Effect of welding heat input on microstructures and toughness in simulated CGHAZ of V-N high strength steel [J].
Hu, Jun ;
Du, Lin-Xiu ;
Wang, Jian-Jun ;
Gao, Cai-Ru .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 577 :161-168
[7]   Correlation of martensite-austenite constituent and cleavage crack initiation in welding heat affected zone of low carbon bainitic steel [J].
Lan, Liangyun ;
Qiu, Chunlin ;
Song, Hongyu ;
Zhao, Dewen .
MATERIALS LETTERS, 2014, 125 :86-88
[8]   Effect of morphology of martensite-austenite phase on fracture of weld heat affected zone in vanadium and niobium microalloyed steels [J].
Li, Y. ;
Baker, T. N. .
MATERIALS SCIENCE AND TECHNOLOGY, 2010, 26 (09) :1029-1040
[9]   The effect of vanadium and niobium on the properties and microstructure of the intercritically reheated coarse grained heat affected zone in low carbon microalloyed steels [J].
Li, Y ;
Crowther, DN ;
Green, MJW ;
Mitchell, PS ;
Baker, TN .
ISIJ INTERNATIONAL, 2001, 41 (01) :46-55
[10]   Role of tandem submerged arc welding thermal cycles on properties of the heat affected zone in X80 microalloyed pipe line steel [J].
Moeinifar, S. ;
Kokabi, A. H. ;
Hosseini, H. R. Madaah .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2011, 211 (03) :368-375