Severe plastic deformation of rheoforged aluminum alloy A356

被引:25
作者
Dodangeh, A. [1 ]
Kazeminezhad, M. [1 ]
Aashuri, H. [1 ]
机构
[1] Sharif Univ Technol, Dept Mat Sci & Engn, Tehran, Iran
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2012年 / 558卷
关键词
Globular structure; Severe plastic deformation; Mechanical properties; Microstructure; A356; MECHANICAL-PROPERTIES; MICROSTRUCTURAL EVOLUTION; HEAT-TREATMENT; BEHAVIOR; RECRYSTALLIZATION;
D O I
10.1016/j.msea.2012.08.014
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this research, the electromagnetic stirring (EMS) process was used to produce semi-solid slurry with globular structure from cast A356 aluminum alloy. Then the slurry was forged in a die, which named rheoforging process. Utilizing multidirectional forging (MDF), the effect of severe plastic deformation on microstructure and mechanical properties of this alloy in dendritic and globular states was investigated. Shear punch, micro- and macro-hardness tests were used to study the mechanical properties of these samples. For metallographic examinations, the optical microscope equipped with the Clemex(R) image analyzer software was used. Optimum globular structure of rheoforged specimens was achieved to deform those in three successful passes of MDF. The results show that more severe strain can be imposed on globular structure with respect to dendritic one. Also, MDF process can effectively improve the strength of the samples with no noticeable change in globules morphology of the rheoforged samples. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:371 / 376
页数:6
相关论文
共 38 条
[1]   Semi-solid microstructure evolution during reheating of aluminum A356 alloy deformed severely by ECAP [J].
Ashouri, S. ;
Nili-Ahmadabadi, M. ;
Moradi, M. ;
Iranpour, M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 466 (1-2) :67-72
[2]   Severe plastic deformation (SPD) processes for metals [J].
Azushima, A. ;
Kopp, R. ;
Korhonen, A. ;
Yang, D. Y. ;
Micari, F. ;
Lahoti, G. D. ;
Groche, P. ;
Yanagimoto, J. ;
Tsuji, N. ;
Rosochowski, A. ;
Yanagida, A. .
CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2008, 57 (02) :716-735
[3]   Characterization of the microstructure evolution of a semi-solid metal slurry during the early stages [J].
Canyook, R. ;
Wannasin, J. ;
Wisuthmethangkul, S. ;
Flemings, M. C. .
ACTA MATERIALIA, 2012, 60 (08) :3501-3510
[4]   Evolution of microstructure in semi-solid slurries of rheocast aluminum alloy [J].
Canyook, R. ;
Petsut, S. ;
Wisutmethangoon, S. ;
Flemings, M. C. ;
Wannasin, J. .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (09) :1649-1655
[5]   Effect of heat treatments on mechanical properties and damage evolution of thixoformed aluminium alloys [J].
Cavaliere, P ;
Cerri, E ;
Leo, P .
MATERIALS CHARACTERIZATION, 2005, 55 (01) :35-42
[6]   Microstructural evolution of previously deformed ZA27 alloy during partial remelting [J].
Chen, TJ ;
Hao, Y ;
Sun, J .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 337 (1-2) :73-81
[7]   Mechanical properties and their microstructure evaluation in the thixoforming process of semi-solid aluminum alloys [J].
Cho, WG ;
Kang, CG .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2000, 105 (03) :269-277
[8]   The effects of mischmetal, cooling rate and heat treatment on the eutectic Si particle characteristics of A319.1, A356.2 and A413.1 Al-Si casting alloys [J].
El Sebaie, O. ;
Samuel, A. M. ;
Samuel, F. H. ;
Doty, H. W. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 480 (1-2) :342-355
[9]   Microstructure and mechanical properties of rheo-diecast (RDC) aluminium alloys [J].
Fan, Z ;
Fang, X ;
Ji, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 412 (1-2) :298-306
[10]   The use of severe plastic deformation for microstructural control [J].
Furukawa, M ;
Horita, Z ;
Nemoto, M ;
Langdon, TG .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 324 (1-2) :82-89