A study on the susceptibility of high strength tempered martensite steels to hydrogen embrittlement (HE) based on incremental step load (ISL) testing methodology

被引:28
作者
Das, Tuhin [1 ]
Rajagopalan, Sriraman K. [1 ,2 ]
Brahimi, Salim V. [1 ,2 ]
Wang, Xiang [3 ]
Yue, Stephen [1 ]
机构
[1] McGill Univ, Dept Min & Mat Engn, Montreal, PQ H3A 0C5, Canada
[2] IBECA Technol Corp, Montreal, PQ H3H 1A8, Canada
[3] McMaster Univ, Dept Mat Sci & Engn, Hamilton, ON L8S 4L7, Canada
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2018年 / 716卷
基金
加拿大自然科学与工程研究理事会;
关键词
Hydrogen embrittlement; Material susceptibility; Incremental step load test; Transmission electron microscopy; Thermal desorption analysis; LOW-ALLOY STEELS; THERMAL-DESORPTION; DELAYED-FRACTURE; PIPELINE STEELS; DIFFUSION; INCLUSIONS; MECHANISM; PRESSURE; METALS; IRON;
D O I
10.1016/j.msea.2018.01.032
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Incremental step load (ISL) technique was used to determine the material susceptibility of three different grades of tempered martensite steels 35CrMo4, 41Cr4 and 36NiCrMo4 to hydrogen embrittlement (HE). In addition to testing the steel grades in air, the environmental hydrogen embrittlement susceptibilities (EHE) of each material were determined by in-situ charging of hydrogen at three different cathodic potentials -0.85 V-SCE, -1V(SCE) and -1.2V(SCE) to obtain the entire threshold curves for these materials. Overall investigation implies that 35CrMo4 is more susceptible than 41Cr4 and 36NiCrMo4. The fracture surface morphology in case of 35CrMo4 is entirely intergranular at -1V(SCE) and -1.2V(SCE) showing the severity of embrittlement. The higher matrix-cementite interfaces along with high cementite and low manganese sulphide (MnS) inclusion content of 36NiCrMo4 influencing the hydrogen transport kinetics within the material are responsible for the lower material susceptibility. The thermal desorption analyses (TDA) further corroborate the observations.
引用
收藏
页码:189 / 207
页数:19
相关论文
共 65 条
  • [41] Morris M.A., 1984, Comprehensive Chemical Kinetics, V19, P1, DOI [DOI 10.1016/S0069-8040(08)70099-2, DOI 10.1016/S0069-8040(08)70099]
  • [42] Hydrogen embrittlement mechanism in fatigue of austenitic stainless steels
    Murakami, Yukitaka
    Kanezaki, Toshihiko
    Mine, Yoji
    Matsuoka, Saburo
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2008, 39A (06): : 1327 - 1339
  • [43] The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel
    Nagao, Akihide
    Smith, Cynthia D.
    Dadfarnia, Mohsen
    Sofronis, Petros
    Robertson, Ian M.
    [J]. ACTA MATERIALIA, 2012, 60 (13-14) : 5182 - 5189
  • [44] Effect of Uniform Distribution of Fine Cementite on Hydrogen Embrittlement of Low Carbon Martensitic Steel Plates
    Nagao, Akihide
    Hayashi, Kenji
    Oi, Kenji
    Mitao, Shinji
    [J]. ISIJ INTERNATIONAL, 2012, 52 (02) : 213 - 221
  • [45] Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels
    Nagumo, M
    Nakamura, M
    Takai, K
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (02): : 339 - 347
  • [46] Hydrogen Embrittlement of a 1500-MPa Tensile Strength Level Steel with an Ultrafine Elongated Grain Structure
    Nie, Yihong
    Kimura, Yuuji
    Inoue, Tadanobu
    Yin, Fuxing
    Akiyama, Eiji
    Tsuzaki, Kaneaki
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2012, 43A (05): : 1670 - 1687
  • [47] HYDROGEN EMBRITTLEMENT OF STEELS
    ORIANI, RA
    [J]. ANNUAL REVIEW OF MATERIALS SCIENCE, 1978, 8 : 327 - 357
  • [48] Consequence of the diffusive hydrogen contents on tensile properties of martensitic steel during the desorption at room temperature
    Oudriss, A.
    Fleurentin, A.
    Courlit, G.
    Conforto, E.
    Berziou, C.
    Rebere, C.
    Cohendoz, S.
    Sobrino, J. M.
    Creus, J.
    Feaugas, X.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 598 : 420 - 428
  • [49] QUANTITATIVE-ANALYSIS OF HYDROGEN TRAPPING
    PRESSOUYRE, GM
    BERNSTEIN, IM
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (11): : 1571 - 1580
  • [50] CLASSIFICATION OF HYDROGEN TRAPS IN STEEL
    PRESSOUYRE, GM
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (10): : 1571 - 1573