Constitutive equations for hot deformation of an Al-6061/20%Al2O3 composite

被引:42
|
作者
Spigarelli, S
Evangelista, E
Cerri, E
Langdon, TG
机构
[1] Univ Ancona, INFM, Dept Mech, I-60131 Ancona, Italy
[2] Univ Lecce, INFM, Dept Ingn Innovaz, I-70131 Lecce, Italy
[3] Univ So Calif, Dept Mat Sci & Engn, Los Angeles, CA 90089 USA
关键词
hot deformation; composites; constitutive equations; torsion testing;
D O I
10.1016/S0921-5093(01)01071-1
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The hot deformation response of an Al-6061 + 20%Al2O3 particulate composite was investigated by means of torsion tests. An analysis of the flow stress dependence on strain rate and temperature gave a stress exponent of n approximate to 5.6 and an activation energy of Q approximate to 150 kJ mol(-1). This value of Q is reasonably close to the anticipated value for self-diffusion in Al. The results are in excellent agreement with other studies carried out on the hot deformation of composites but the phenomenological nature of the constitutive equation does not permit an unambiguous determination of the rate-controlling flow mechanism. Nevertheless, it is shown that an identical constitutive equation may be used to describe the creep of composites under both shear and hot torsion conditions. It is concluded that the mechanism controlling hot deformation and creep at high stresses is the climb of dislocations. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:721 / 725
页数:5
相关论文
共 50 条
  • [31] Hot deformation behavior and microstructure evolution of TiC–Al2O3/Al composites
    Rui-Ying Zhang
    Zhi-Ming Shi
    Xiu-Mei Zhang
    Rare Metals, 2015, 34 (10) : 725 - 730
  • [32] Hot deformation behavior and microstructure evolution of TiC–Al2O3/Al composites
    Rui-Ying Zhang
    Zhi-Ming Shi
    Xiu-Mei Zhang
    Rare Metals, 2015, 34 : 725 - 730
  • [33] Tribological Behavior of Plasma Sprayed Al2O3 and ZrO2 5CaO Coatings on Al-6061 Substrate
    Krishnamurthy, N.
    Murali, M. S.
    Mukunda, P. G.
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2010, 29 (03) : 111 - 126
  • [34] The effect of die shape on the hot extrudability and mechanical properties of 6061 Al/Al2O3 composites
    Kang, CG
    Kim, NH
    Kim, BM
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2000, 100 (1-3) : 53 - 62
  • [35] Influence of quenching agents on mechanical, wear, and fracture characteristics of Al2O3 / MoS2 reinforced Al-6061 hybrid Metal Matrix Composite (MMCs)
    Suchendra, K. R.
    Reddy, M. Sreenivasa
    Ravikumar, M.
    FRATTURA ED INTEGRITA STRUTTURALE-FRACTURE AND STRUCTURAL INTEGRITY, 2023, 17 (63): : 122 - 133
  • [36] Hot deformation behavior of Al2O3/Cu-10vol%WC composite
    Feng Jiang
    Tian Baohong
    Liu Yong
    MATERIALS AND COMPUTATIONAL MECHANICS, PTS 1-3, 2012, 117-119 : 921 - 924
  • [37] Hot deformation and recrystallization behaviour of a SiCp/6061 Al composite
    Xia, X.
    Sakaris, P.
    McQueen, H.J.
    1993, 1
  • [38] Achieving enhanced tensile ductility in an Al-6061 composite processed by severe plastic deformation
    Han, BQ
    Langdon, TG
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 410 : 430 - 434
  • [39] High temperature deformation of an Al6061-Al2O3 particulate metal matrix composite
    Spigarelli, S
    Gariboldi, E
    Langdon, TG
    CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 2001, : 291 - 298
  • [40] Fatigue and quantitative fractography of an AL-6061 matrix composite
    Crawford, BR
    Griffiths, JR
    ADVANCES IN FRACTURE RESEARCH, VOLS 1-6, 1997, : 2581 - 2586