Improvement of the performance properties of cutting tools using the multilayer composite wear-resistant coatings based on nitrides of Cr, Mo, Zr, Nb, and Al

被引:12
|
作者
Volosova, Marina [1 ]
Vereschaka, Alexey [2 ]
Andreev, Nikolay [3 ]
Sotova, Catherine [1 ]
Bublikov, Jury [2 ]
机构
[1] Moscow State Technol Univ STANKIN, Vadkovsky Per 1, Moscow 127994, Russia
[2] IDTI RAS, Vadkovsky Per 18-1A, Moscow 127055, Russia
[3] Natl Univ Sci & Technol MISIS, Leninsky Prospect 4, Moscow 119049, Russia
关键词
Multilayer composite wear-resistant coatings; Filtered cathodic vacuum arc deposition; Cutting tool; Turning; Tool life; HIGH-SPEED STEEL; MECHANICAL-PROPERTIES; NANOSTRUCTURED COATINGS; THERMAL-PROPERTIES; BEAM SOURCES; MICROSTRUCTURE; DEPOSITION; OXIDATION; MULTICOMPONENT; STABILITY;
D O I
10.1016/j.matpr.2020.08.118
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The article deals with the properties of the Cr,Mo-(Cr,Mo)N-(Cr,Mo,Al)N, Zr,Nb-(Zr,Nb)N-(Zr,Nb,Al)N, and Zr,Nb-(Zr,Nb)N-(Cr,Mo,Zr,Nb,Al)N multilayer composite wear-resistant coatings. The coatings were deposited using technology of Filtered Cathodic Vacuum Arc Deposition (FCVAD). The investigation of the coating structures, conducted using the transmission electron microscopy (TEM), showed the presence of the nanolayer structure with the nanolayer thicknesses within a range of 0.5-20 nm and the period lambda within a range of 92-136 nm. The microhardness of the Zr,Nb-(Zr,Nb)N-(Cr,Mo,Zr,Nb,Al)N coating turned out to be significantly higher than the microhardness of the other studied coatings, and that may be associated with the formation of a multicomponent fcc phase of (Cr,Mo,Zr,Nb,Al)N. According to the results of the cutting tests during the turning of American Iron and Steel Institute (AISI) 420 steel, the tool with the Zr,Nb-(Zr,Nb)N-(Cr,Mo,Zr,Nb,Al)N coating demonstrated the tool life which 2.5 times exceeds the tool life of the tool with the (Ti,Al)N commercial coating of similar thickness and by 50 and 30% exceeds the tool life of tools with two other studied coatings. The investigation of the fracture processes in coatings during the turning revealed a significant difference in the mechanisms of cracking and wear. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1421 / 1427
页数:7
相关论文
共 33 条
  • [31] Stability, elastic properties and fracture toughness of Al0.75X0.75B14(X = Sc, Ti, V, Cr, Y, Zr, Nb, Mo) investigated using ab initio calculations
    Emmerlich, Jens
    Thieme, Niklas
    to Baben, Moritz
    Music, Denis
    Schneider, Jochen M.
    JOURNAL OF PHYSICS-CONDENSED MATTER, 2013, 25 (33)
  • [32] Investigations into the Improvement of the Mechanical Properties of Ti-5Al-4Mo-4Cr-2Sn-2Zr Titanium Alloy by Using Low Energy Laser Peening without Coating
    Xue, Dingyuan
    Jiao, Yang
    He, Weifeng
    Shen, Xiaojun
    Gao, Yangjun
    Wang, Lili
    MATERIALS, 2020, 13 (06) : 1 - 14
  • [33] Effects of Y2O3 addition on the microstructure and wear-resistant performance of TiN/TiB-reinforced Ti-based laser-clad coatings on Ti-6Al-4V alloys
    Wang, Lixin
    Yang, Lijun
    Huang, Yiming
    Yuan, Yuxue
    Jia, Chenpeng
    MATERIALS TODAY COMMUNICATIONS, 2021, 29