Tribological behavior of PACVD TiN coatings in the temperature range up to 500°C

被引:33
作者
Badisch, E
Fontalvo, GA
Stoiber, M
Mitterer, C
机构
[1] Mat Ctr Leoben, A-8700 Leoben, Austria
[2] Univ Leoben, Dept Phys Met & Mat Testing, A-8700 Leoben, Austria
关键词
TiN coating; PACVD; ball-on-disc tests; dry sliding; low-friction;
D O I
10.1016/S0257-8972(02)00626-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Titanium nitride (TiN), is still the standard coating for cutting as well as forming applications. The aim of this study is to investigate the tribological behavior of low-friction plasma-assisted chemical vapor deposition (PACVD) TiN coatings with low chlorine content as well as the thermal stability of the low-friction effect. Dry sliding experiments at temperatures ranging from room temperature to 500 degreesC were conducted on PACVD TiN coatings, deposited onto high speed steel substrates. The coatings were worn against ball-bearing steel and Al2O3 balls using a ball-on-disc configuration. Characterization of the wear tracks was done by scanning electron microscopy, electron-probe microanalysis and an optical 3d profiling system. Extremely low-friction coefficients against ball-bearing steel and Al2O3 balls of 0.14-0.17 have been obtained at room temperature for coatings with chlorine contents between 3.2 and 3.7 at.%. The friction coefficient against Al2O3 increases to values of approximately 0.6-0.8 for temperatures above 70 degreesC. The lowest coating wear coefficient with 1.93 X 10(-16) m(2)/N was obtained for Al2O3 balls at room temperature, whereas for temperatures exceeding 200 degreesC increased abrasion of the coating takes place, resulting in higher wear rates. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:585 / 590
页数:6
相关论文
共 19 条
  • [1] Tribological behaviour at elevated temperatures of thin physical vapour deposited coatings
    Abourayak, K
    Fayeulle, S
    Vincent, L
    Ribeiro, C
    Cavaleiro, A
    Vieira, MT
    [J]. SURFACE & COATINGS TECHNOLOGY, 1996, 80 (1-2) : 171 - 175
  • [2] The crystallization of amorphous debris on titanium nitride coatings influenced by sliding wear conditions
    de Wit, E
    Froyen, L
    Celis, JP
    [J]. WEAR, 1998, 221 (02) : 124 - 133
  • [3] FONTALVO G, 2001, THESIS U LEOBEN
  • [4] Franklin S. E., 1992, Surface and Coatings Technology, V54-55, P459, DOI 10.1016/S0257-8972(07)80066-1
  • [5] Hard coatings produced by PACVD applied to aluminium die casting
    Heim, D
    Holler, F
    Mitterer, C
    [J]. SURFACE & COATINGS TECHNOLOGY, 1999, 116 : 530 - 536
  • [6] TiAlN and TiAlCN deposition in an industrial PaCVD-plant
    Heim, D
    Hochreiter, R
    [J]. SURFACE & COATINGS TECHNOLOGY, 1998, 98 (1-3) : 1553 - 1556
  • [7] HOLMBERG K, 1994, COATING TRIBOLOGY PR, P173
  • [8] HOLMBERG K, 1994, COATINGS TRIBOLOGY P, P37
  • [9] HUQ MZ, IN PRESS WEAR
  • [10] Jehn H., 1993, DIN Fachbericht 39. Characterisierung dunner Schichren