摘要
The Vickers indentation fracture toughness test, or VIF, is addressed by considering its origins and the numerous equations that have been applied along with the technique to estimate the fracture resistance, or the K-Ic of ceramics. Initiation and propagation of cracks during the VIF test are described and contrasted with the pre-cracking and crack growth for internationally standardized fracture toughness tests. It is concluded that the VIF test technique is fundamentally different than standard fracture toughness tests. The VIF test has a complex three-dimensional crack system with substantial deformation residual stresses and damage around the cracks. The VIF test relates to an ill-defined crack arrest condition as opposed to the rapid crack propagation of the standardized fracture toughness tests. Previously published fracture toughness results employing the VIF technique are reviewed. These reveal serious discrepancies in reported VIF fracture toughness values. Finally, recent fracture resistance measurements by the VIF technique for the Standard Reference Material SRM 2100 are presented. These are compared with standardized test results for the same material. It is concluded that the VIF technique is not reliable as a fracture toughness test for ceramics or for other brittle materials. What the VIF actually measures in terms of fracture resistance cannot be readily defined. It is recommended that the VIF technique no longer be acceptable for the fracture toughness testing of ceramic materials.
引用
收藏
页码:673 / 680
页数:8
相关论文
共 45 条
[1]  
[Anonymous], 2003, 15732 ISO
[2]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[3]  
*ASTM INT, 1999, ANN BOOK STAND
[4]  
*ASTM INT, 2003, ANN BOOK STAND
[5]   FLAT R-CURVE FROM STABLE PROPAGATION OF INDENTATION CRACKS IN COARSE-GRAINED ALUMINA [J].
BLEISE, D ;
STEINBRECH, RW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (02) :315-322
[6]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .2. STRENGTH METHOD [J].
CHANTIKUL, P ;
ANSTIS, GR ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :539-543
[7]   DIRECT OBSERVATION AND ANALYSIS OF INDENTATION CRACKING IN GLASSES AND CERAMICS [J].
COOK, RF ;
PHARR, GM .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (04) :787-817
[8]  
*EUR COMM STAND, 2003, 14425 CEN TS EUR COM
[9]   QUASI-STATIC SOLID PARTICLE DAMAGE IN BRITTLE SOLIDS .1. OBSERVATIONS, ANALYSIS AND IMPLICATIONS [J].
EVANS, AG ;
WILSHAW, TR .
ACTA METALLURGICA, 1976, 24 (10) :939-956
[10]   FRACTURE TOUGHNESS DETERMINATIONS BY INDENTATION [J].
EVANS, AG ;
CHARLES, EA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (7-8) :371-372