Effect of autoclave postpolymerization treatments on the fracture toughness of autopolymerizing dental acrylic resins

被引:0
|
作者
Durkan, Rukiye [2 ]
Gurbuz, Ayhan [3 ]
Yilmaz, Burak [1 ]
Ozel, M. Birol [4 ]
Bagis, Bora [2 ]
机构
[1] Ohio State Univ, Coll Dent, Div Restorat & Prosthet Dent, Columbus, OH 43210 USA
[2] Karadeniz Tech Univ, Dept Prosthodont, Fac Dent, Trabzon, Turkey
[3] Ankara Univ, Dept Prosthodont, Fac Dent, TR-06100 Ankara, Turkey
[4] Karadeniz Tech Univ, Dept Orthodont, Fac Dent, Trabzon, Turkey
关键词
Acrylic resin; Autoclave; Fracture toughness; RESIDUAL MONOMER CONTENT; DENTURE BASE MATERIALS; MECHANICAL-PROPERTIES; MICROWAVE IRRADIATION; FLEXURAL STRENGTH; WATER; POLYMERIZATION; RELINE; MICROHARDNESS; SOLUBILITY;
D O I
10.5301/JABB.2012.9026
中图分类号
Q6 [生物物理学];
学科分类号
071011 ;
摘要
Introduction: Microwave and water bath postpolymerization have been suggested as methods to improve the mechanical properties of heat and autopolymerizing acrylic resins. However, the effects of autoclave heating on the fracture properties of autopolymerizing acrylic resins have not been investigated. Purpose: The aim of this study was to assess the effectiveness of various autoclave postpolymerization methods on the fracture properties of 3 different autopolymerizing acrylic resins. Methods: Forty-two specimens of 3 different autopolymerizing acrylic resins (Orthocryl, Paladent RR and Futurajet) were fabricated (40x8x4mm), and each group was further divided into 6 subgroups (n=7). Control group specimens remained as processed (Group 1). The first test group was postpolymerized in a cassette autoclave at 135 degrees C for 6 minutes and the other groups were postpolymerized in a conventional autoclave at 130 degrees C using different time settings (5, 10, 20 or 30 minutes). Fracture toughness was then measured with a three-point bending test. Data were analyzed by ANOVA followed by the Duncan test (alpha=0.05). Results: The fracture toughness of Orthocryl and Paladent-RR acrylic resins significantly increased following conventional autoclave postpolymerization at 130 degrees C for 10 minutes (P<.05). However, the fracture toughness of autoclave postpolymerized Futurajet was not significantly different than its control specimens (P<.05). The fracture toughness of Futurajet was significantly less than Paladent RR and Orthocryl specimens when autoclaved at 130 degrees C for 10 minutes. Conclusions: Within the limitations of this study, it can be suggested that autoclave postpolymerization is an effective method for increasing the fracture toughness of tested autoploymerized acrylic resins.
引用
收藏
页码:37 / 42
页数:6
相关论文
共 40 条
  • [21] Effect of Ambient Plasma Treatments on Thermal Conductivity and Fracture Toughness of Boron Nitride Nanosheets/Epoxy Nanocomposites
    Choi, Won-Jong
    Lee, Seul-Yi
    Park, Soo-Jin
    NANOMATERIALS, 2023, 13 (01)
  • [22] Effect of Atmospheric-Pressure Plasma Treatments on Fracture Toughness of Carbon Fibers-Reinforced Composites
    Kim, Won-Jong
    Heo, Young-Jung
    Lee, Jong-Hoon
    Rhee, Kyong Yop
    Park, Soo-Jin
    MOLECULES, 2021, 26 (12):
  • [23] Effect of rapid cooling on residual stress and surface fracture toughness of dental zirconia
    Nonaka, Kazumichi
    Teramae, Mitsuji
    Pezzotti, Giuseppe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2024, 157
  • [24] Effect of cyclic loading and environmental aging on the fracture toughness of dental resin composite
    Ravindranath, Viswanath
    Gosz, Michael
    De Santiago, Eduardo
    Drummond, James L.
    Mostovoy, Sheldon
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2007, 80B (01) : 226 - 235
  • [25] Apparent fracture toughness of acrylic bone cement: effect of test specimen configuration and sterilization method
    Lewis, G
    BIOMATERIALS, 1999, 20 (01) : 69 - 78
  • [26] Effect of silane coupling agent and concentration on fracture toughness and water sorption behaviour of fibre-reinforced dental composites
    Varghese, Jerrin Thadathil
    Cho, Kiho
    Raju
    Farrar, Paul
    Prentice, Leon
    Prusty, B. Gangadhara
    DENTAL MATERIALS, 2023, 39 (04) : 362 - 371
  • [27] Effect of Cryogenic Treatments on Hardness, Fracture Toughness, and Wear Properties of Vanadis 6 Tool Steel
    Yarasu, Venu
    Jurci, Peter
    Ptacinova, Jana
    Dlouhy, Ivo
    Hornik, Jakub
    MATERIALS, 2024, 17 (07)
  • [28] Residual monomer of reline acrylic resins - Effect of water-bath and microwave post-polymerization treatments
    Urban, Vanessa M.
    Machado, Ana L.
    Oliveira, Regina V.
    Vergani, Carlos E.
    Pavarina, Ana C.
    Cass, Quezia B.
    DENTAL MATERIALS, 2007, 23 (03) : 363 - 368
  • [29] Tunable effect of polyvinyl butyral nanofiber veil on fracture toughness of glass reinforced phenolic composites manufactured with out of autoclave method
    Barzoki, P. Kheirkhah
    Rezadoust, A. M.
    Latifi, M.
    POLYMER TESTING, 2018, 71 : 255 - 261
  • [30] Effect of heat treatments and loading orientation on the tensile properties and fracture toughness of AlSi7Mg alloy produced by Laser Powder Bed Fusion
    de Menezes, Joao Teixeira Oliveira
    Castrodeza, Enrique Mariano
    Patriarca, Luca
    Casati, Riccardo
    INTERNATIONAL JOURNAL OF FRACTURE, 2022, 235 (01) : 145 - 157