Closed-form structural stress and stress intensity factor solutions for spot welds in square plates under opening loading conditions

被引:7
作者
Sripichai, K. [1 ]
Pan, J. [1 ]
机构
[1] Univ Michigan, Ann Arbor, MI 48109 USA
关键词
Spot weld; Square specimen; Structural stress; Equivalent radius; Stress intensity factor; LAP-SHEAR SPECIMENS; GEOMETRIC FUNCTIONS;
D O I
10.1016/j.engfracmech.2012.06.016
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
Closed-form structural stress and stress intensity factor solutions for spot welds in square plates under opening loading conditions are investigated here. First, the existing analytical axisymmetric solutions for a rigid inclusion in a circular plate with simply supported and clamped outer edges are reviewed. Then the results of axisymmetrical finite element analyses for a rigid inclusion in a circular plate are presented. The results indicate that the finite element model with one element across the plate thickness is an appropriate model to investigate the structural stress solutions for a rigid inclusion in a square plate to avoid the local effect of the reaction force due to the constraint applied to the rigid inclusion. Next, the results of three-dimensional finite element analyses for a rigid inclusion in a square plate with simply supported and clamped outer edges are presented. The results indicate that, as the ratio of the plate width to the rigid inclusion diameter becomes large about 6, the structural stress solutions along the circumference of the rigid inclusion become almost uniform. Approximate equivalent radius solutions are then determined in order to use the analytical structural stress solutions for a rigid inclusion in a circular plate to calculate the structural stress solutions along the circumference of the rigid inclusion in a square plate. Then, the results of three-dimensional finite element analyses for spot welds between square plates of different thicknesses and materials are presented. The results indicate that the computational stress intensity factor solutions agree well with those based on the structural stress solutions with the equivalent radius. Based on the closed-form structural stress solutions, complete sets of the normalized stress intensity factor solutions for spot welds between square plates of different thicknesses and materials under opening loading conditions are presented for combinations of steel, aluminum and magnesium sheets and combinations of aluminum and copper sheets for convenient engineering applications. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:168 / 188
页数:21
相关论文
共 50 条
  • [41] Review and synthesis of stress intensity factor (SIF) solutions for annular outer cracks in round bars under tension loading
    Toribio, Jesus
    Gonzalez, Beatriz
    Matos, Juan-Carlos
    4TH INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY (ICSI 2021), 2022, 37 : 989 - 994
  • [42] Review and synthesis of stress intensity factor (SIF) solutions for circular inner cracks in round bars under tension loading
    Toribio, Jesus
    Gonzalez, Beatriz
    Matos, Juan-Carlos
    4TH INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY (ICSI 2021), 2022, 37 : 995 - 1000
  • [43] Stress intensity factor solutions for several crack problems using the proportional crack opening displacements
    Lan, Xin
    Ji, Shaobo
    Noda, Nao-Aki
    Cheng, Yong
    ENGINEERING FRACTURE MECHANICS, 2017, 171 : 35 - 49
  • [44] Stress intensity factors and T-stress in edge-cracked rectangular plates under mixed boundary conditions
    Fett, T
    ENGINEERING FRACTURE MECHANICS, 1998, 60 (5-6) : 625 - 630
  • [45] Effect of a graded interlayer on the stress intensity factor of cracks in a joint under thermal loading
    Bleeck, O
    Munz, D
    Schaller, W
    Yang, YY
    ENGINEERING FRACTURE MECHANICS, 1998, 60 (5-6) : 615 - 623
  • [46] Finite Element Analysis on the Stress Intensity Factor under Combined Bending and Torsion Loading
    Ismail, A. E.
    Ariffin, A. K.
    Abdullah, S.
    Ghazali, M. J.
    Abdulrazzaq, M.
    FRACTURE AND STRENGTH OF SOLIDS VII, PTS 1 AND 2, 2011, 462-463 : 1325 - +
  • [47] Dynamic stress intensity factor of a functionally graded material under antiplane shear loading
    C. Li
    G. J. Weng
    Z. Duan
    Z. Zou
    Acta Mechanica, 2001, 149 : 1 - 10
  • [48] Closed form stress intensity factors for a semi-elliptical crack in a thick-walled cylinder under thermal stress
    Shahani, AR
    Nabavi, SM
    INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (08) : 926 - 933
  • [49] Measurement of stress intensity factor under mixed-mode loading by the method of caustics
    Kawagishi, Y
    Hirose, Y
    Sasaki, T
    PROCEEDINGS OF THE SIXTH (1996) INTERNATIONAL OFFSHORE AND POLAR ENGINEERING CONFERENCE, VOL IV, 1996, 1996, : 280 - 286
  • [50] Computation of stress intensity factor in cracked plates under bending in static and fatigue by a hybrid method
    Hachi, B. K.
    Rechak, S.
    Haboussi, M.
    Taghite, M.
    Maurice, G.
    INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (9-11) : 1904 - 1912