Damage detection versus heat dissipation in E-glass/Epoxy laminated composites under dynamic compression at high strain rate

被引:51
|
作者
Tarfaoui, M. [1 ]
El Moumen, A. [1 ]
Ben Yahia, H. [1 ]
机构
[1] CNRS, ENSTA Bretagne, FRE 3744, IRDL, F-29200 Brest, France
关键词
Hopkinson bars; Dynamic compression test; Composite materials; Damage; Heat dissipation; TEMPERATURE-MEASUREMENT; DEFORMATION; IMPACT; GENERATION; POLYMERS;
D O I
10.1016/j.compstruct.2017.11.083
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
In this investigation, a new experimental technique in which the deformation, damage mode, and the temperature are measured simultaneously during a high strain rate on laminated composites materials. The composites consist of unidirectional E-glass fibers reinforced epoxy polymer composites used in industrial applications. The experimental setup consists of a compression Split Hopkinson Pressure Bar (SHPB), a high-speed infrared camera and a high-speed Fastcam rapid camera. Specimens, with cubic like a shape, are impacted at different strain rates ranging from 200 to 2000 s(-1). During impact test, the specimen surface is controlled and monitored with the infrared camera which provides thermal images in time sequence and with high-speed camera which acquires the damage progressive in specimens. Experimental results show that the damage throughout specimens differs and the temperature change depending on the damage mode and their maximum exceed 219 degrees C.
引用
收藏
页码:50 / 61
页数:12
相关论文
共 50 条
  • [31] DAMAGE TOLERANCE AND STRAIN ENERGY ANALYSIS OF E-GLASS EPOXY COMPOSITES USING VIRTUAL CRACK CLOSURE TECHNIQUE AND COHESIVE ZONE MODELLING
    Joy, Eldho Jacob
    Menon, Arjun S.
    Sagar, Sarun
    Biju, N.
    M2D2015: PROCEEDINGS OF THE 6TH INTERNATIONAL CONFERENCE ON MECHANICS AND MATERIALS IN DESIGN, 2015, : 633 - 634
  • [32] Evaluation of solid particle erosion damage on E-glass/epoxy composites using acoustic emission activity
    Yang, N. H.
    Nayeb-Hashemi, H.
    PROCEEDINGS OF THE ASME NONDESTRUCTIVE EVALUATION ENGINEERING DIVISION, 2005, 26 : 37 - 46
  • [33] On the response of stitched woven S2-glass/epoxy composites to high strain rate compression loading
    Hosur, MV
    Karim, MR
    Jeelani, S
    POLYMERS & POLYMER COMPOSITES, 2004, 12 (03): : 183 - 196
  • [34] Dynamic fracture of carbon nanotube/epoxy composites under high strain-rate loading
    Bie, B. X.
    Han, J. H.
    Lu, L.
    Zhou, X. M.
    Qi, M. L.
    Zhang, Z.
    Luo, S. N.
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 68 : 282 - 288
  • [35] The effect of fiber orientation and stacking sequence on carbon/E-glass/epoxy intraply hybrid composites under dynamic loading conditions
    Samson, Ponnusamy Edwin
    Kumaran, Selvadurai Senthil
    Vigneshwaran, Shanmugam
    Oisik, Das
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2023, 34 (01) : 363 - 376
  • [36] Characterization of Interlaminar Shear Strength of Laminated Woven E-Glass/Epoxy Composites by Four Point Bend Shear Test
    Aslan, Zueleyha
    Alnak, Yeliz
    POLYMER COMPOSITES, 2010, 31 (02) : 359 - 368
  • [37] Experimental investigation of buckling behavior of E-glass/epoxy laminated composite materials with multi-walled carbon nanotube under uniaxial compression load
    Mutu, Halil Burak
    Aslan, Zuleyha
    JOURNAL OF COMPOSITE MATERIALS, 2022, 56 (16) : 2573 - 2584
  • [38] Determination of the material model and damage parameters of a carbon fiber reinforced laminated epoxy composite for high strain rate planar compression
    Shi, Chen
    Guo, Baoqiao
    Sarikaya, Mustafa
    Celik, Muhammet
    Chen, Pengwan
    Guden, Mustafa
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2021, 149
  • [39] Effects of fiber orientations on high strain rate behavior of glass/epoxy composites
    Haque, A
    Vaidya, UK
    Mahfuz, H
    Jeelani, S
    TECHNOLOGY TRANSFER IN A GLOBAL COMMUNITY, 1996, 28 : 586 - 595
  • [40] FAILURE STRENGTH AND DAMAGE MECHANISMS OF E-GLASS EPOXY LAMINATES UNDER INPLANE BIAXIAL COMPRESSIVE DEFORMATION
    WANG, JZ
    SOCIE, DF
    JOURNAL OF COMPOSITE MATERIALS, 1993, 27 (01) : 40 - 58