Structural and dielectrical characterization of low-k polyurethane composite films with silica aerogel

被引:24
作者
Bozoglu, Deniz [1 ]
Deligoz, Huseyin [2 ]
Ulutas, Kemal [1 ]
Yakut, Sahin [1 ]
Deger, Deniz [1 ]
机构
[1] Istanbul Univ, Fac Sci, Phys Dept, TR-34134 Istanbul, Turkey
[2] Istanbul Univ, Fac Engn, Chem Engn Dept, TR-34320 Avcilar, Turkey
关键词
Aerogel; Dielectric constant; Dielectric loss; Polymer composite; Relaxation time; AC CONDUCTIVITY; THERMAL-DEGRADATION; ELECTRIC MODULUS; CONSTANT; BEHAVIOR; POLYMER; RELAXATION;
D O I
10.1016/j.jpcs.2019.02.013
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
In this study, a hydrophobic silica aerogel was synthesized via one-step surface modification and polymer composite films based on a polyurethane (PU) matrix were prepared by doping with silica aerogel powder (at 2%, 3%, 5%, and 7% by weight = w/w%). The structural, thermal, morphological, and surface properties of the silica aerogel and PU composite films containing aerogel were investigated by Fourier transform infrared spectroscopy, thermogravimetric analysis, differential scanning calorimetry (DSC), scanning electron microscopy, and tensiometry. The dielectric properties of the silica aerogel and PU composite films containing the aerogel were determined over a temperature range of 293-423 K and a frequency range of 1-10(6) Hz. The contact angle of the silica aerogel was 10(6). Moreover, the PU composite film with 7% aerogel had the highest contact angle (theta = 105 degrees) among the composite samples, which was similar to contact angle of the silica aerogel. The dielectric constants and dielectric losses decreased with the frequency for all of the samples, whereas they increased with the temperature. The polarization regions and relaxation times were determined for all of the samples using the Cole Cole equation. The glass-transition temperatures (T-g) were determined for the silica aerogel and PU composite films containing aerogel by dielectric spectroscopy and compared with the DSC results. The dielectric constants were lower for the PU composite films than the PU film. The dielectric constant for the PU composite film doped with 2% silica aerogel was 2.9 at 10 MHz. Thus, the PU composite with a low dielectric constant and dielectric loss factor (tan delta) could be regarded as a potential dielectric constant candidate, with possible applications as a dielectric material in the microelectronics industry.
引用
收藏
页码:46 / 57
页数:12
相关论文
共 56 条
  • [1] Al-Saleh M. H., 2013, J PHYS D APPL PHYS, V46
  • [2] Anandraj J, 2017, INDIAN J PURE AP PHY, V55, P313
  • [3] Conductive composites of polyurethane resins and ionic liquids
    Berns, Belinda
    Deligoez, Hueseyin
    Tieke, Bernd
    Kremer, Friedrich
    [J]. MACROMOLECULAR MATERIALS AND ENGINEERING, 2008, 293 (05) : 409 - 418
  • [4] Synthesis of a Novel pH-Sensitive Polyurethane-Alginate Blend with Poly(ethylene terephthalate) Waste for the Oral Delivery of Protein
    Bhattacharyya, Aditi
    Mukhopadhyay, Piyasi
    Kundu, P. P.
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2014, 131 (16)
  • [5] Structure and properties of polyurethane/nanosilica composites
    Chen, YC
    Zhou, SX
    Yang, HH
    Wu, LM
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2005, 95 (05) : 1032 - 1039
  • [6] Dielectric behavior of some aromatic polyimide films
    Chisca, Stefan
    Musteata, Valentina Elena
    Sava, Ion
    Bruma, Maria
    [J]. EUROPEAN POLYMER JOURNAL, 2011, 47 (05) : 1186 - 1197
  • [7] Synthesis and characterization of high dielectric constant polyaniline/polyurethane blends
    Chwang, CP
    Liu, CD
    Huang, SW
    Chao, DY
    Lee, SN
    [J]. SYNTHETIC METALS, 2004, 142 (1-3) : 275 - 281
  • [8] Dependence of dielectric behavior on the physical property of fillers in the polymer-matrix composites
    Dang, ZM
    Zhang, YH
    Tjong, SC
    [J]. SYNTHETIC METALS, 2004, 146 (01) : 79 - 84
  • [9] A novel cross-linked polyimide film:: synthesis and dielectric properties
    Deligöz, H
    Özgümüs, S
    Yalçinyuva, T
    Yildirim, S
    Deger, D
    Ulutas, K
    [J]. POLYMER, 2005, 46 (11) : 3720 - 3729
  • [10] Characterization and dielectric properties of polyaniline-TiO2 nanocomposites
    Dey, A
    De, S
    De, A
    De, SK