Kinetics of thermal oxidative degradation of phosphorus-containing flame retardant copolyesters

被引:80
作者
Wu, B [1 ]
Wang, YZ [1 ]
Wang, XL [1 ]
Yang, KK [1 ]
Jin, YD [1 ]
Zhao, H [1 ]
机构
[1] Sichuan Univ, Sch Chem, Ctr Degradable & Flame Retardant Polymer Mat, Chengdu 610064, Peoples R China
关键词
flame retardant; phosphorus-containing copolyester; thermal oxidative degradation;
D O I
10.1016/S0141-3910(02)00041-1
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermal oxidative degradation of phosphorus-containing copolyester and poly(ethylene terephthalate) (PET) in air were studied by thermogravimetric analysis (TG) in order to obtain the activation energies of pyrolysis. The activation energies were determined using the Kissinger method and the Flynn-Wall-Ozawa method, which do not require knowledge of the reaction mechanism (RM). The results show that there is no large difference between the values of activation energy of phosphorus-containing copolyester and PET, which suggests that the flame retardants studied do not greatly influence the mechanisms of pyrolysis. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:401 / 409
页数:9
相关论文
共 14 条
[1]  
BEDNAS ME, 1981, J APPL POLYM SCI, V26, P288
[2]  
Budrugeac P, 2001, POLYM DEGRAD STABIL, V71, P185
[3]   KINETIC AND THERMOGRAVIMETRIC ANALYSIS OF THE THERMAL OXIDATIVE-DEGRADATION OF FLAME-RETARDANT POLYESTERS [J].
COONEY, JD ;
DAY, M ;
WILES, DM .
JOURNAL OF APPLIED POLYMER SCIENCE, 1984, 29 (03) :911-923
[4]   THERMAL-DEGRADATION OF POLY(ETHYLENE-TEREPHTHALATE) - A KINETIC-ANALYSIS OF THERMOGRAVIMETRIC DATA [J].
COONEY, JD ;
DAY, M ;
WILES, DM .
JOURNAL OF APPLIED POLYMER SCIENCE, 1983, 28 (09) :2887-2902
[5]  
CULLIS CF, 1987, J ANAL APPL PYROL, V11, P462
[6]  
DAY M, 1981, J APPL POLYM SCI, V26, P3097
[7]  
DAY M, 1988, J THERM ANAL, V34, P746
[8]  
GRANZOW A, 1977, J APPL POLYM SCI, V21, P1696
[9]  
GRANZOW A, 1976, J APPL POLYM SCI, V20, P700
[10]  
GULLONMARTIN, 2000, J ANAL APPL PYROLYSI, V58, P635