Experimental studies of Zn and Pb induced high temperature corrosion of two commercial boiler steels

被引:45
作者
Bankiewicz, Dorota [1 ]
Enestam, Sonja [1 ,2 ]
Yrjas, Patrik [1 ]
Hupa, Mikko [1 ]
机构
[1] Abo Akad Univ, Proc Chem Ctr, SF-20500 Turku, Finland
[2] Metso Power Oy, Tampere 33101, Finland
关键词
MSW; Demolition wood; High temperature corrosion; Zinc; Lead; MUNICIPAL SOLID-WASTE; ACCELERATED CORROSION; FULL-SCALE; INCINERATION; ZNCL2-KCL; GASIFICATION; CHLORINE; BEHAVIOR; VAPOR; ZINC;
D O I
10.1016/j.fuproc.2011.12.017
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Fuels such as demolition wood and MSW usually contain high levels of alkali chlorides and heavy metals especially Zn and Pb which may form low melting, highly aggressive deposits speeding up the corrosion reactions. In order to investigate the corrosion tendency of these specific heavy metals two common superheater materials were exposed to various Zn and Pb compounds in a laboratory tube furnace. Afterwards, the maximum and the mean oxide layer thicknesses were determined. Furthermore, the thickness distribution over the steel sample was also determined. Metallographic cross-sections of the specimens were characterized by means of SEM/EDX. The analysis of the specimens showed that the most severe corrosion attack occurred on both tested steels during the exposure to PbCl2 and already below the PbCl2 melting temperature. The poor resistance of the austenitic stainless steel (AISI 347) in this case was subscribed to PbCrO4 formation that decreased significantly the protectiveness of Cr2O3. The exposures to ZnCl2 showed no adverse effects on AISI 347 while 10CrMo9-10 suffered from an increased oxide layer growth at 350 degrees C. The laboratory experiments were supplemented with thermodynamic calculations in order to gain insight in the behavior of Zn and Pb in the corrosion mechanisms. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:89 / 97
页数:9
相关论文
共 31 条
[11]   High temperature interaction of pure Cr with KCl [J].
Li, YS ;
Sanchez-Pasten, M ;
Spiegel, M .
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 :1047-1053
[12]   Models describing the degradation of FeAl and NiAl alloys induced by ZnCl2-KCl melt at 400-450 °C [J].
Li, YS ;
Spiegel, M .
CORROSION SCIENCE, 2004, 46 (08) :2009-2023
[13]   Accelerated corrosion of pure Fe, Ni, Cr and several Fe-based alloys induced by ZnCl2-KCl at 450°C in oxidizing environment [J].
Li, YS ;
Niu, Y ;
Wu, WT .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 345 (1-2) :64-71
[14]   Accelerated corrosion of five commercial steels under a ZnCl2-KCl deposit in a reducing environment typical of waste gasification at 673-773 K [J].
Lu, W. M. ;
Pan, T. J. ;
Zhang, K. ;
Niu, Y. .
CORROSION SCIENCE, 2008, 50 (07) :1900-1906
[15]   Effect of ZnCl2 vapor on high temperature oxidation of pure chromium [J].
Ma, HT ;
Wang, L ;
Li, YS ;
Zhao, J .
JOURNAL OF MATERIALS SCIENCE LETTERS, 2003, 22 (10) :763-765
[16]   Effect of chlorine on volatilization of Na, K, Pb, and Zn compounds from municipal solid waste during gasification and melting in a shaft-type furnace [J].
Osada, Shohichi ;
Kuchar, Dalibor ;
Matsuda, Hitoki .
JOURNAL OF MATERIAL CYCLES AND WASTE MANAGEMENT, 2009, 11 (04) :367-375
[17]  
Otero E., 1999, OXIDATION METALS, V51
[18]  
Otero E., 1998, OXIDATION METALS, V49
[19]   A thermodynamic approach on vapor-condensation of corrosive salts from flue gas on boiler tubes in waste incinerators [J].
Otsuka, Nobuo .
CORROSION SCIENCE, 2008, 50 (06) :1627-1636
[20]  
Pan T.J., 2007, OXIDATION METALS, V67