Effects of Porosity on Mechanical Properties and Corrosion Resistances of PM-Fabricated Porous Ti-10Mo Alloy

被引:49
|
作者
Xu, Wei [1 ]
Lu, Xin [1 ]
Zhang, Bing [2 ]
Liu, Chengcheng [1 ]
Lv, Shaomin [1 ,2 ]
Yang, Shidi [3 ]
Qu, Xuanhui [1 ]
机构
[1] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Beijing 100083, Peoples R China
[2] AECC Beijing Inst Areonaut Mat, Sci & Technol Adv High Temp Struct Mat Lab, Beijing 100095, Peoples R China
[3] Sanying Precis Instruments Co Ltd, Tianjin 300399, Peoples R China
基金
北京市自然科学基金;
关键词
porous Ti-10Mo alloy; corrosion resistances; mechanical property; powder metallurgy; TI-MO ALLOYS; DENTAL IMPLANT APPLICATIONS; BIOMEDICAL APPLICATIONS; TI-15MO ALLOY; TITANIUM; BEHAVIOR; MICROSTRUCTURE; COMPONENTS; CELLS;
D O I
10.3390/met8030188
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Porous binary Ti-10Mo alloys were prepared using non-spherical titanium, molybdenum powders by the powder metallurgy (PM) space holder technique. Based on the three-dimensional analysis of porosity characteristics, a detailed assessment of the effects of porosity on mechanical properties and corrosion resistances in phosphate-buffered saline (PBS) was carried out. For comparison, PM-fabricated CP-Ti with 50.5% porosity sintered at 1200 degrees C for 2 h and dense Ti-10Mo alloy sintered at 1450 degrees C for 2 h (relative density is 97.2% and porosity is 2.8%) were studied simultaneously. The results show that with the space-holder volume contents rising from 63 to 79%, the open porosity and average pore size (d(50)) increase remarkably, while the pore size distribution (d(10)-d(90)) tends to be stable at about 100 mu m. The average pore sizes (d(50)) of porous Ti-10Mo alloy can be controlled in the range of 70-380 mu m. The PM-fabricated porous Ti-10Mo alloy can achieve a wide range of mechanical properties, with yield compression strength of 248.2-76.9 MPa, and elastic modulus of 6.4-1.7 GPa. In addition, the yield compression strength and the elastic modulus meet the linear regression and exponential formula, respectively. With the porosity of Ti-10Mo alloy increasing from 2.8 to 66.9%, the corrosion rate rises exponentially from 1.6 g/m(2).day to 17.1 g/m(2).day. In comparison to CP-Ti with nearly the same porosity, Ti-10Mo alloy shows significantly higher corrosion resistance. As a result, the relationships between porosity and mechanical properties, corrosion resistances of Ti-10Mo alloys were established, which can be used as a design reference in material selection for orthopedic applications.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] The effects of copper on the mechanical properties of Ti-10Mo alloy prepared by powder metallurgy method
    Kharisma, Aji Abdillah
    Rudianto, Haris
    Mutiara, Achmad Benny
    Puspitodjati, Sulistyo
    Latief, Fahamsyah Hamdan
    Wismogroho, Agus Sukarto
    Widayatno, Wahyu Bambang
    Aryanto, Didik
    Firdharini, Cherly
    JOURNAL OF METALS MATERIALS AND MINERALS, 2024, 34 (01):
  • [2] Porous Ti-10Mo alloy fabricated by powder metallurgy for promoting bone regeneration
    Xu, Wei
    Liu, Zhuo
    Lu, Xin
    Tian, Jingjing
    Chen, Gang
    Liu, Bowen
    Li, Zhou
    Qu, Xuanhui
    Wen, Cuie
    SCIENCE CHINA-MATERIALS, 2019, 62 (07) : 1053 - 1064
  • [3] Mechanical modulation and bioactive surface modification of porous Ti-10Mo alloy for bone implants
    Gao, Zhifang
    Li, Qunyin
    He, Fang
    Huang, Yuan
    Wan, Yizao
    MATERIALS & DESIGN, 2012, 42 : 13 - 20
  • [4] The Mechanical Properties and In Vitro Biocompatibility of PM-Fabricated Ti-28Nb-35.4Zr Alloy for Orthopedic Implant Applications
    Xu, Wei
    Li, Ming
    Wen, Cuie
    Lv, Shaomin
    Liu, Chengcheng
    Lu, Xin
    Qu, Xuanhui
    MATERIALS, 2018, 11 (04):
  • [5] Preparation and properties of porous Ti-10Mo alloy by selective laser sintering
    Xie, Fangxia
    He, Xinbo
    Lu, Xin
    Cao, Shunli
    Qu, Xuanhui
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2013, 33 (03): : 1085 - 1090
  • [6] Structural characterization and electrochemical behavior of a laser-sintered porous Ti-10Mo alloy
    Xie, F. X.
    He, X. B.
    Cao, S. L.
    Lu, X.
    Qu, X. H.
    CORROSION SCIENCE, 2013, 67 : 217 - 224
  • [7] Ti-10Mo/Hydroxyapatite composites for orthopedic applications: Microstructure, mechanical properties and biological activity
    Xie, Fangxia
    Huang, Jiabing
    Yang, Hao
    He, Xueming
    MATERIALS TODAY COMMUNICATIONS, 2021, 29
  • [8] Effects of hydroxyapatite addition on corrosion behavior and in-vitro bioactivity of Ti-10Mo matrix biocomposite
    Xie, Fangxia
    Huang, Jiabing
    Cao, Shu
    He, Xueming
    MATERIALS TODAY COMMUNICATIONS, 2022, 31
  • [9] Effects of step-quenching on the αaEuro3 martensitic transformation, α precipitation, and mechanical properties of multiphase Ti-10Mo alloy
    Wang, C. H.
    Jiang, H.
    Cao, G. H.
    JOURNAL OF MATERIALS SCIENCE, 2018, 53 (16) : 11765 - 11778
  • [10] Physical, mechanical, and corrosion properties of Ti-12Mo and Ti-15Mo alloys fabricated by elemental blend and mechanical alloying techniques
    Awad, Ahmed H.
    Aly, Hayam A.
    Saood, Modar
    MATERIALS CHEMISTRY AND PHYSICS, 2024, 312