Morphology characteristics and mode of CaO encapsulation during treatment of electrolytic manganese solid waste

被引:3
作者
Du, Bing [1 ,2 ,3 ]
Dan, Zhigang [1 ]
Zhou, Changbo [4 ,5 ]
Guo, Tingzheng [1 ]
Liu, Jianguo [2 ]
Zhang, Haiyan [1 ]
Shi, Feifei [1 ]
Duan, Ning [1 ]
机构
[1] Chinese Res Inst Environm Sci, Technol Ctr Heavy Met Cleaner Prod Engn, Beijing, Peoples R China
[2] Tsinghua Univ, Sch Environm, Key Lab Solid Waste Management & Environm Safety, Beijing, Peoples R China
[3] Shanxi Univ, Inst Resources & Environm Engn, Taiyuan, Peoples R China
[4] Chinese Res Inst Environm Sci, State Key Lab Environm Criteria & Risk Assessment, Beijing, Peoples R China
[5] Chinese Res Inst Environm Sci, Cleaner Prod Ctr, Beijing, Peoples R China
基金
美国国家科学基金会;
关键词
Electrolytic manganese solid waste; Calcium oxide; Encapsulation; Secondary hydration heat; Microstructure; HEAVY-METALS; LIME; HYDRATION; MICROSTRUCTURE; IMMOBILIZATION; SOILS;
D O I
10.1007/s11356-016-7347-0
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Electrolytic manganese solid waste (EMSW) is composed of manganese, calcium, and other sulfates. Common practice in China is to treat EMSW with quicklime (CaO); however, the per unit mass treatment efficiency of CaO is low. Studies of the interface between the CaO and EMSW particle and their microstructural characteristics are limited; these interactions may explain the low treatment efficiency. We conducted leaching experiments and measurements of the secondary heat generated by hydration of CaO to assess the extent of excess CaO in EMSW. The microstructure of CaO was also analyzed. It was determined that excess CaO particles in the EMSW were encapsulated, which influenced CaO hydration and morphology. The outer layer of the encapsulated CaO contained high levels of calcium and sulfur, which postulated to be caused by CaSO4 precipitates formed from the reaction of CaO hydration products with soluble sulfate. Three types of CaO encapsulation were identified: fully encapsulated CaO (55 % of the total CaO), partly encapsulated CaO (32 %), and self-encapsulated CaO (13 %). High concentrations of soluble sulfates in EMSW cause CaO encapsulation. These react to form CaSO4, which could negatively influence mass transfer and result in low treatment efficiency of EMSW by CaO.
引用
收藏
页码:21861 / 21871
页数:11
相关论文
共 24 条
[11]   REACTIVITY OF LIME AND RELATED OXIDES .15. CRYSTALLINE FORMS OF SULPHATED LIME [J].
GLASSON, DR .
JOURNAL OF APPLIED CHEMISTRY, 1965, 15 (09) :439-+
[12]   Quantifying particle aggregation in sediments [J].
Haberlah, David ;
Mctainsh, Grant H. .
SEDIMENTOLOGY, 2011, 58 (05) :1208-1216
[13]   Heavy metal concentrations in soils and plant accumulation in a restored manganese mineland in Guangxi, South China [J].
Li, M. S. ;
Luo, Y. P. ;
Su, Z. Y. .
ENVIRONMENTAL POLLUTION, 2007, 147 (01) :168-175
[14]   Simultaneous decontamination of cross-polluted soils with heavy metals and PCBs using a nano-metallic Ca/CaO dispersion mixture [J].
Mallampati, Srinivasa Reddy ;
Mitoma, Yoshiharu ;
Okuda, Tetsuji ;
Sakita, Shogo ;
Simion, Cristian .
ENVIRONMENTAL SCIENCE AND POLLUTION RESEARCH, 2014, 21 (15) :9270-9277
[15]   Enhanced heavy metal immobilization in soil by grinding with addition of nanometallic Ca/CaO dispersion mixture [J].
Mallampati, Srinivasa Reddy ;
Mitoma, Yoshiharu ;
Okuda, Tetsuji ;
Sakita, Shogo ;
Kakeda, Mitsunori .
CHEMOSPHERE, 2012, 89 (06) :717-723
[16]   Hydration of Calcium Oxide Surface Predicted by Reactive Force Field Molecular Dynamics [J].
Manzano, Hegoi ;
Pellenq, Roland J. M. ;
Ulm, Franz-Josef ;
Buehler, Markus J. ;
van Duin, Adri C. T. .
LANGMUIR, 2012, 28 (09) :4187-4197
[17]   Microstructure evolution of lime putty upon aging [J].
Mascolo, Giuseppe ;
Mascolo, Maria Cristina ;
Vitale, Alessandro ;
Marino, Ottavio .
JOURNAL OF CRYSTAL GROWTH, 2010, 312 (16-17) :2363-2368
[18]   Analysis of pollution materials generated from electrolytic manganese industries in China [J].
Ning Duan ;
Wang Fan ;
Zhou Changbo ;
Zhu Chunlei ;
Yu Hongbing .
RESOURCES CONSERVATION AND RECYCLING, 2010, 54 (08) :506-511
[19]   Experimental studies on ettringite-induced heaving in soils [J].
Puppala, AJ ;
Intharasombat, N ;
Vempati, RK .
JOURNAL OF GEOTECHNICAL AND GEOENVIRONMENTAL ENGINEERING, 2005, 131 (03) :325-337
[20]   Study of the hydration of CaO powder by gas-solid reaction [J].
Serris, E. ;
Favergeon, L. ;
Pijolat, M. ;
Soustelle, M. ;
Nortier, P. ;
Gaertner, R. S. ;
Chopin, T. ;
Habib, Z. .
CEMENT AND CONCRETE RESEARCH, 2011, 41 (10) :1078-1084