Study on the Microstructure, Mechanical Properties and Corrosion Behavior of Mg-Zn-Ca Alloy Wire for Biomaterial Application

被引:33
作者
Zheng, Maobo [1 ]
Xu, Guangquan [1 ]
Liu, Debao [1 ]
Zhao, Yue [1 ]
Ning, Baoqun [2 ]
Chen, Minfang [3 ]
机构
[1] Tianjin Univ Technol, Sch Mat Sci & Engn, Tianjin 300384, Peoples R China
[2] Tianjin Univ Technol, Natl Demonstrat Ctr Expt Funct Mat Educ, Tianjin 300384, Peoples R China
[3] Tianjin Univ Technol, Tianjin Key Lab Photoelect Mat & Devices, Tianjin 300384, Peoples R China
基金
中国国家自然科学基金;
关键词
cold drawing; corrosion resistance; mechanical properties; Mg-Zn-Ca alloy wire; microstructure; MAGNESIUM; DEGRADATION; TEXTURE; CALCIUM; PHASE;
D O I
10.1007/s11665-018-3278-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Due to their excellent biocompatibility and biodegradability, magnesium alloy wires have attracted much attention for biomaterial applications including orthopedic K-wires and sutures in wound closure. In this study, Mg-3Zn-0.2Ca alloy wires were prepared by cold drawing combined with proper intermediate annealing process. Microstructures, texture, mechanical properties and corrosion behavior of Mg-3Zn-0.2Ca alloy wire in a simulated body fluid were investigated. The results showed that the secondary phase and average grain size of the Mg-3Zn-0.2Ca alloy were refined in comparison with the as-extruded alloy and a strong (0002)< 10-10 >//DD basal fiber texture system was formed after multi-pass cold drawing. After the annealing, most of the basal planes were tilted to the drawing direction (DD) by about 35A degrees, presenting the characteristics of random texture, and the texture intensity decreased. The as-annealed wire shows good mechanical properties with the ultimate tensile strength (UTS), yield strength (YS) and elongation of 253 +/- 8.5 MPa, 212 +/- 11.3 MPa and 9.2 +/- 0.9%, respectively. Electrochemical and hydrogen evolution measurements showed that the corrosion resistance of the Mg-3Zn-0.2Ca alloy wire was improved after the annealing. The immersion test indicated that the Mg-3Zn-0.2Ca wire exhibited uniform corrosion behavior during the initial period of immersion, but then exhibited local corrosion behavior.
引用
收藏
页码:1837 / 1846
页数:10
相关论文
共 36 条
[1]   Neuropathology of aluminum toxicity in rats (glutamate and GABA impairment) [J].
Abd El-Rahman, SS .
PHARMACOLOGICAL RESEARCH, 2003, 47 (03) :189-194
[2]  
[Anonymous], JPN J APPL PHYS
[3]  
[Anonymous], 2004, Standard practice for laboratory immersion corrosion testing of metals
[4]  
[Anonymous], EUR CELLS MAT
[5]   Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy [J].
Aung, Naing Naing ;
Zhou, Wei .
CORROSION SCIENCE, 2010, 52 (02) :589-594
[6]   Preparation, microstructure and degradation performance of biomedical magnesium alloy fine wires [J].
Bai, Jing ;
Yin, Lingling ;
Lu, Ye ;
Gan, Yiwei ;
Xue, Feng ;
Chu, Chenglin ;
Yan, Jingli ;
Yan, Kai ;
Wan, Xiaofeng ;
Tang, Zhejun .
PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2014, 24 (05) :523-530
[7]   Relationship between the corrosion behavior and the thermal characteristics and microstructure of Mg-0.5Ca-xZn alloys [J].
Bakhsheshi-Rad, H. R. ;
Abdul-Kadir, M. R. ;
Idris, M. H. ;
Farahany, S. .
CORROSION SCIENCE, 2012, 64 :184-197
[8]   The relation between severe plastic deformation microstructure and corrosion behavior of AZ31 magnesium alloy [J].
Ben Hamu, G. ;
Eliezer, D. ;
Wagner, L. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 468 (1-2) :222-229
[9]   Static recrystallization kinetics of a heavily cold drawn AZ31 magnesium alloy under annealing treatment [J].
Chao, H. Y. ;
Sun, H. F. ;
Chen, W. Z. ;
Wang, E. D. .
MATERIALS CHARACTERIZATION, 2011, 62 (03) :312-320
[10]   Influence of large cold strain on the microstructural evolution for a magnesium alloy subjected to multi-pass cold drawing [J].
Chen, W. Z. ;
Zhang, W. C. ;
Chao, H. Y. ;
Zhang, L. X. ;
Wang, E. D. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 623 :92-96