Synthesis of WC and dense WC-5 vol.% Co hard materials by high-frequency induction heated combustion

被引:47
作者
Kim, HC [1 ]
Oh, DY [1 ]
Guojian, J [1 ]
Shon, IJ [1 ]
机构
[1] Chonbuk Natl Univ, Engn Res Inst, Dept Mat Engn, Jeonju 560756, South Korea
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2004年 / 368卷 / 1-2期
关键词
high-frequency induction heated combustion; WC-Co composites; hard materials; combustion synthesis; hardness; fracture toughness;
D O I
10.1016/j.msea.2003.08.105
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Tungsten carbide (WC) and dense WC-5 vol.% Co materials, with grain size of similar to1 mum, were synthesized by high-frequency induction heated combustion synthesis (HFIHCS) method in one step from elemental powders of W, C, and cobalt (Co) within several minutes. Simultaneous combustion synthesis and densification were accomplished under the combined effects of an induced current and mechanical pressure. In the absence of cobalt additive, WC can be formed, but its relative density was low (about 70%) under simultaneous application of a 60MPa pressure and the induced current. However, in the presence of 5 vol. % cobalt, the density increased to 98.5% under the same experimental conditions. The percentages of the total volume shrinkage occurring before and during the synthesis reaction of WC-5 vol.% Co were 7 and 57%, respectively. The fracture toughness and hardness values obtained of WC-5 vol.% Co were 7 MPa m(1/2) and 2100 kg/mm(2), respectively. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:10 / 17
页数:8
相关论文
共 30 条
[1]   Strength degradation of a tungsten carbide-cobalt composite at elevated temperatures [J].
Acchar, W ;
Gomes, UU ;
Kaysser, WA ;
Goring, J .
MATERIALS CHARACTERIZATION, 1999, 43 (01) :27-32
[2]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[3]   Quantitative evaluation of normal and abnormal grain growth of cemented carbides during liquid phase sintering [J].
Chabretou, V ;
Lavergne, O ;
Missiaen, JM ;
Allibert, CH .
METALS AND MATERIALS-KOREA, 1999, 5 (02) :205-210
[4]   Two-step synthesis of nanostructured tungsten carbide-cobalt powders [J].
Fu, L ;
Cao, LH ;
Fan, YS .
SCRIPTA MATERIALIA, 2001, 44 (07) :1061-1068
[5]   LOW-TEMPERATURE CARBURIZATION OF HIGH-SURFACE-AREA TUNGSTEN POWDERS [J].
GAO, L ;
KEAR, BH .
NANOSTRUCTURED MATERIALS, 1995, 5 (05) :555-569
[6]   Synthesis of nanophase WC powder by a displacement reaction process [J].
Goa, L ;
Kear, BH .
NANOSTRUCTURED MATERIALS, 1997, 9 (1-8) :205-208
[7]   Determination of three-dimensional grain size distribution by linear intercept measurement [J].
Han, JW ;
Kim, DY .
ACTA MATERIALIA, 1998, 46 (06) :2021-2028
[8]  
HAN SH, 1999, J KOR POWDER METALL, V6, P307
[9]   Adhesion properties of CVD diamond film on binder-less sintered tungsten carbide prepared by the spark sintering process [J].
Hirata, A ;
Zheng, H ;
Yoshikawa, M .
DIAMOND AND RELATED MATERIALS, 1998, 7 (11-12) :1669-1674
[10]   Microstructure, hardness and toughness of nanostructured and conventional WC-Co composites [J].
Jia, K ;
Fischer, TE ;
Gallois, B .
NANOSTRUCTURED MATERIALS, 1998, 10 (05) :875-891