Degradation Behavior of TiN Coatings with Different Thicknesses after a Pulsed Laser Thermal Shock Test

被引:0
作者
Jeon, Seol [1 ]
Choi, Youngkue [1 ,2 ]
Shin, Hyun-Gyoo [1 ,2 ]
Park, Hyun [3 ]
Lee, Heesoo [1 ]
Seo, Nokun [1 ,2 ]
机构
[1] Pusan Natl Univ, Sch Mat Sci & Engn, Pusan 609735, South Korea
[2] Korea Testing Lab, Mat Testing Ctr, Seoul 152848, South Korea
[3] Pusan Natl Univ, GCRC SOP, Pusan 609735, South Korea
来源
KOREAN JOURNAL OF METALS AND MATERIALS | 2013年 / 51卷 / 10期
基金
新加坡国家研究基金会;
关键词
thin films; sputtering; fracture; focused ion beam (FIB); laser thermal shock; HARD COATINGS; DEFORMATION MECHANISMS; FILMS; SURFACE; STEEL; DIE;
D O I
10.3365/KJMM.2013.51.10.729
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The degradation behavior of TiN coatings with different thicknesses deposited on Inconel 617 substrates was investigated in terms of surface and interface microstructures after pulsed laser thermal shock. The specimens with coating thicknesses of 1.0 and 4.5 mu m were exposed to repetitive laser shock using a pulsed laser ablation system (LSX-213). The TiN coating with a 1.0 mu m thickness contained cracks along the columnar grains in the coating layer, and spalling and delamination with interface cracks appeared with an increase in the number of ablations. In contrast, the 4.5 mu m thick TiN coating still maintained adhesion to the substrate until the substrate elements dissolved out to the surface. Surface and cross-sectional observation showed that the pulsed laser seems to simultaneously induce normal and shear stress to the surface at the ablated spots with high thermal stress.
引用
收藏
页码:729 / 734
页数:6
相关论文
共 25 条
  • [1] Effect of heat treatment of TiN films deposited by CFUBMS
    Arslan, E
    Efeoglu, I
    [J]. MATERIALS CHARACTERIZATION, 2004, 53 (01) : 29 - 34
  • [2] Nature of contact deformation of TiN films on steel
    Bhowmick, S
    Xie, ZH
    Hoffman, M
    Jayaram, V
    Biswas, SK
    [J]. JOURNAL OF MATERIALS RESEARCH, 2004, 19 (09) : 2616 - 2624
  • [3] HARD COATINGS OF TIN, (TIHF)N AND (TINB)N DEPOSITED BY RANDOM AND STEERED ARC EVAPORATION
    BOELENS, S
    VELTROP, H
    [J]. SURFACE & COATINGS TECHNOLOGY, 1987, 33 (1-4) : 63 - 71
  • [4] Degradation of TiN coatings under cyclic loading
    Cairney, JM
    Tsukano, R
    Hoffman, MJ
    Yang, M
    [J]. ACTA MATERIALIA, 2004, 52 (11) : 3229 - 3237
  • [5] The interface crack problem for a nonhomogeneous coating bonded to a homogeneous substrate
    Chen, YF
    Erdogan, F
    [J]. JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1996, 44 (05) : 771 - 787
  • [6] Crack propagation behavior of TiN coatings by laser thermal shock experiments
    Choi, Youngkue
    Jeon, Seol
    Jeon, Min-seok
    Shin, Hyun-Gyoo
    Chun, Ho Hwan
    Lee, Youn-seoung
    Lee, Heesoo
    [J]. APPLIED SURFACE SCIENCE, 2012, 258 (22) : 8752 - 8757
  • [7] Mechanical properties of TiN thin film coatings on 304 stainless steel substrates
    Chou, WJ
    Yu, GP
    Huang, JH
    [J]. SURFACE & COATINGS TECHNOLOGY, 2002, 149 (01) : 7 - 13
  • [8] ON THE MECHANICS OF DELAMINATION AND SPALLING IN COMPRESSED FILMS
    EVANS, AG
    HUTCHINSON, JW
    [J]. INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1984, 20 (05) : 455 - 466
  • [9] The tribological characteristics of titanium nitride coatings .1. Coating thickness effects
    Guu, YY
    Lin, JF
    Ai, CF
    [J]. WEAR, 1996, 194 (1-2) : 12 - 21
  • [10] Simulation of thermal stress in magnetron sputtered thin coating by finite element analysis
    Haider, J
    Rahman, M
    Corcoran, B
    Hashmi, MSJ
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 168 (01) : 36 - 41